journal article·2021-09

Application of Scratch Testing for the Assessment of the Adherent Properties of Scales and CO2 Corrosion Product Layers and their Relation to Corrosion

Claudia Prieto, Hamed Mansoori, Bruce Brown, Marc Singer, David Young

Corrosion Science· Volume 190
Publisher page

Abstract

Abstract Protective corrosion product layers, such as iron carbonate, can govern pipeline corrosion; their formation being associated with operational conditions (high [Fe2+], pH > 6.0, T > 70 °C). Brines contain Ca2+ that can incorporate as a substitutional cation in the iron carbonate lattice, potentially compromising the mechanical integrity of the protective layer. This work utilized scratch testing as an analytical technique that provides more information on layer adherence than indentation methods. It was demonstrated that the presence of iron calcium carbonate layers contributes to the formation of a protective and mechanically stable iron carbonate layer adjacent to the steel surface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (57)

Show source-provided references
1. A Mechanistic Model for Carbon Dioxide Corrosion of Mild Steel in the Presence of Protective Iron Carbonate Films — Part 2 : A Numerical Experiment10.5006/1.3277579 ↗
2. The effect of temperature and ionic strength on iron carbonate (FeCO3) solubility limit10.1016/j.corsci.2009.03.009 ↗
3. A mechanistic model for carbon dioxide corrosion of mild steel in the presence of protective iron carbonate films-Part 3: Film growth model10.5006/1.3277592 ↗
4. Sun · 2006
5. Influence of calcium and magnesium ions on CO2 corrosion of carbon steel in oil and gas production systems - A review10.1016/j.jngse.2018.08.025 ↗
6. A mechanistic model for carbon dioxide corrosion of mild steel in the presence of protective iron carbonate films - Part 3: Film growth model10.5006/1.3277592 ↗
7. Effect of CaCO3-saturated solution on CO2 corrosion of mild steel explored in a system with controlled water chemistry and well-defined mass transfer conditions10.1016/j.corsci.2019.07.004 ↗
8. Corrosion of carbon steel under CO2 conditions: Effect of CaCO3 precipitation on the stability of the FeCO3 protective layer10.1016/j.corsci.2019.108214 ↗
9. Mechanical Strength and Removal of a Protective Iron Carbonate Layer Formed on Mild Steel in CO2 Corrosion
10. Fracture mechanical properties of CO2 corrosion product scales and their relation to localized corrosion
11. Mechanical properties of CO2 corrosion product scales and their relationship to corrosion rates10.1016/j.corsci.2008.07.016 ↗
12. Understanding localized CO2 corrosion of carbon steel from physical properties of iron carbonate scales
13. Iron Calcium Carbonate Instability: Structural Modification of Siderite Corrosion Films10.1021/acsami.0c14513 ↗
14. Protective iron carbonate films - Part 1: Mechanical removal in single-phase aqueous flow
15. Protective iron carbonate films -Part 2: Chemical removal by dissolution in single-phase aqueous flow
16. Protective iron carbonate films - Part 3: Simultaneous chemo-mechanical removal in single-phase aqueous flow10.5006/1.3278425 ↗
17. Mechanical integrity of corrosion product films on rotating cylinder specimens10.1016/j.corsci.2014.11.042 ↗
18. Reliability of the pull-off test for in situ evaluation of adhesion strength10.1016/j.conbuildmat.2011.12.097 ↗
19. Reliability of pull-off test for steel fiber reinforced self-compacting concrete10.1016/j.measurement.2015.06.013 ↗
20. Reliability on coating pull-off adhesion strength test
21. Mechanical Properties of CO2 Corrosion Scale Formed at Different Temperatures and their Relationship to Corrosion Rate10.1179/1743278211Y.0000000023 ↗
22. Fracture Toughness Determinations by Means of Indentation Fracture
23. Fundamentals of fracture mechanics
24. Hardness, toughness, and brittleness: an indentation analysis10.1111/j.1151-2916.1979.tb19075.x ↗
25. On the vickers indentation fracture toughness Test10.1111/j.1551-2916.2006.01482.x ↗
26. Vickers Indentation Fracture (VIF) modeling to analyze multi-cracking toughness of titania, alumina and zirconia plasma sprayed coatings10.1016/j.msea.2009.08.058 ↗
27. Adhesion of thin films10.1116/1.568754 ↗
28. The use of scratch adhesion testing for the determination of interfacial adhesion: The importance of frictional drag10.1016/0257-8972(88)90178-8 ↗
29. An overview of the potential of quantitativa coating adhesion measurements by scratch testing10.1016/j.triboint.2005.04.013 ↗
30. New developments in the modelling of the hardness and scratch adhesion of thin films10.1016/0257-8972(90)90121-R ↗
31. The adhesion of chemically vapour-deposited hard coatings to steel-the scratch test10.1016/0040-6090(81)90419-3 ↗
32. Measurement of adhesion of thin films
33. Adhesion of TiC and TiN coatings prepared by chemical vapour deposition on WC-Co-based cemented carbides10.1007/BF01114266 ↗
34. Adhesion of diamond-like carbon films on polymers: an assessment of the validity of the scratch test technique applied to flexible substrates10.1163/156856194X00401 ↗
35. Effect of FexCayCO3 and CaCO3 scales on the CO2 corrosion of mild steel
36. Key issues related to modelling of internal corrosion of oil and gas pipelines – A review10.1016/j.corsci.2007.06.006 ↗
37. Carbonates
38. Kinetics of precipitation of calcium carbonate in alkaline pH at constant supersaturation. Spontaneous and seeded growth10.1021/jp981171h ↗
39. ASTM G102 - 89(2010) Standard Practice for Calculation of Corrosion Rates and Related Information from Electrochemical Measurements
40. McCafferty · 2010
41. The effect of acetic acid on the integity of protective iron carbonate layers in CO2 corrosion of mild steel
42. Acetic acid and carbon dioxide corrosion of carbon steel covered with iron carbonate
43. Failure mode maps in the thin film scratch adhesion test10.1016/S0301-679X(97)00012-1 ↗
44. Dowson · 1993
45. Lafuente · 2015
46. Protectiveness, morphology and composition of corrosion products formedon carbon steel in the presence of Cl-, Ca2+ and Mg2+ in high pressure CO2 environments10.1016/j.apsusc.2018.05.140 ↗
47. Brandon · 2008
48. ASTM · 2010 · 1
49. Mechanical Characterization and Adherence of Iron Carbonate on an X65 Steel
50. Wedding Cake Growth Mechanism in One-Dimensional and Two-Dimensional Nanostructure Evolution10.1021/acs.nanolett.5b04072 ↗
51. The AlN layer thickness dependent coherent epitaxial growth, stress and hardness in NbN/AlN nanostructured multilayer films10.1016/j.surfcoat.2013.08.004 ↗
52. Physical origins of intrinsic stresses in Volmer-Weber thin films10.1557/mrs2002.15 ↗
53. Strain-induced growth instability and nanoscale surface patterning in perovskite thin films10.1038/srep26075 ↗
54. Cracking of thin bonded films in residual tension10.1016/0020-7683(92)90015-L ↗
55. Bushan · 1999
56. A direct measurement of wall shear stress in multiphase flow-Is it an important parameter in CO2 corrosion of carbon steel pipelines?10.1016/j.corsci.2016.04.008 ↗
57. Role of Conductive Corrosion Products in the Protectiveness of Corrosion Layers10.5006/1.3284844 ↗