The passivation behaviour of copper-containing high-performance ferritic stainless steels in the cathode environment of polymer electrolyte membrane fuel cells
Source abstract
Abstract
Abstract The passivation behaviour of copper-containing high-performance ferritic stainless steels in the cathode environment of polymer electrolyte membrane fuel cells was investigated using electrochemical tests and XPS surface analyses. The addition of copper to the alloy deteriorated the corrosion resistance at a passive region of 0.6 VSCE. With an increase of the copper content, the passivity of the alloy degraded due to an increase of the formation of Cr-containing inclusions, and a decrease of the Cr oxide and hydroxide in the passive film.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Fuel Cells and Related Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Acres · J. Power Sources · 2001 · 100 · 6010.1016/S0378-7753(01)00883-7 ↗
2. Hentall · J. Power Sources · 1999 · 80 · 23510.1016/S0378-7753(98)00264-X ↗
3. Cleghorn · Int. J. Hydrogen Energy · 1997 · 22 · 113710.1016/S0360-3199(97)00016-5 ↗
4. Ihonen · Electrochim. Acta · 2001 · 46 · 289910.1016/S0013-4686(01)00510-2 ↗
5. Wang · Electrochim. Acta · 2007 · 52 · 679310.1016/j.electacta.2007.05.001 ↗
6. Lafront · Electrochim. Acta · 2007 · 52 · 507610.1016/j.electacta.2007.01.080 ↗
7. Burstein · Corros. Sci. · 2009 · 51 · 224910.1016/j.corsci.2009.07.010 ↗
8. Wang · J. Power Sources · 2003 · 115 · 24310.1016/S0378-7753(03)00023-5 ↗
9. Agneaux · Fuel Cells · 2006 · 6 · 4710.1002/fuce.200500100 ↗
10. Davies · J. Appl. Electrochem. · 2000 · 30 · 10110.1023/A:1003831406406 ↗
11. Wang · J. Power Sources · 2004 · 128 · 19310.1016/j.jpowsour.2003.09.075 ↗
12. Ma · Electrochem. Syst. · 2000 · 3 · 221
13. LaConti · 2004 · vol. 3 · 647
14. Seo · Corros. Sci. · 1986 · 26 · 94910.1016/0010-938X(86)90085-5 ↗
15. Jiangnan · Corros. Sci. · 1992 · 33 · 85110.1016/0010-938X(92)90049-9 ↗
16. Hultquist · Corros. Sci. · 1987 · 27 · 93710.1016/0010-938X(87)90060-6 ↗
17. Postrach · Werkst. Korros. · 1994 · 45 · 50810.1002/maco.19940450904 ↗
18. Fedrizzi · Br. Corros. J. · 1991 · 26 · 4610.1179/000705991798269378 ↗
19. Yamamoto · Boshoku Gijutsu · 1986 · 35 · 448
20. Kim · Corrosion · 2007 · 63 · 11410.5006/1.3278336 ↗
21. Ishii · Tetsu-to-Hagané (J. Iron Steel Inst. Jpn.) · 2011 · 97 · 44110.2355/tetsutohagane.97.441 ↗
22. Wilde · Corrosion · 1969 · 25 · 30010.5006/0010-9312-25.7.300 ↗
23. Lizovs · Corrosion · 1966 · 22 · 279
24. Postrach · Mater. Corros. · 1994 · 45 · 50810.1002/maco.19940450904 ↗
25. Guedes · Thin Solid Films · 2006 · 515 · 216710.1016/j.tsf.2006.05.011 ↗
26. Banas · Mater. Sci. Eng. A · 2000 · 277 · 18310.1016/S0921-5093(99)00530-4 ↗
27. Oguzie · Electrochim. Acta · 2010 · 55 · 502810.1016/j.electacta.2010.04.015 ↗
28. ASTM A 763-93 Standard, Standard Practices for Detecting Susceptibility to Intergranular Attack in Ferritic Stainless Steels, ASTM International, 01-May-2009, West Conshohocken, PA, USA.
29. ASTM A 262-02 Standard, Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels, ASTM International, 01-May-2009, West Conshohocken, PA, USA.
30. Chu · J. Power Sources · 1999 · 80 · 22610.1016/S0378-7753(98)00263-8 ↗
31. Makkus · Fuel Cells Bull. · 2000 · 3 · 510.1016/S1464-2859(00)87319-8 ↗
32. Scholta · 1997 · 300
33. Borup · 1995 · vol. 393
34. ASTM G5-94 Standard, Standard Reference Test Method for Mak ing Potentiostatic and Potentiodynamic Anodic Polarization Measurements, ASTM International, 01-May-2009, West Conshohocken, PA, USA.
35. Jeon · Corros. Sci. · 2011 · 53 · 140810.1016/j.corsci.2011.01.005 ↗
36. Lee · 1999
37. Steelmaking Data Source Book, Revised Edition, Japan Society for the Promotion of Science (JSPS), 19th Committee on Steelmaking, Gordon and Breach Science Publishers, New York, NY, 1988, pp. 273–325
38. Sigworth · Met. Sci. · 1974 · 8 · 29810.1179/msc.1974.8.1.298 ↗
39. Pistorius · Corros. Sci. · 1994 · 36 · 52510.1016/0010-938X(94)90041-8 ↗
40. Pistorius · Corros. Sci. · 1992 · 33 · 188510.1016/0010-938X(92)90191-5 ↗
41. Stewart · Corros. Sci. · 1992 · 33 · 45710.1016/0010-938X(92)90074-D ↗
42. Kim · Corros. Sci. · 2010 · 52 · 189710.1016/j.corsci.2010.02.043 ↗
43. Jeon · Corros. Sci. · 2010 · 52 · 353710.1016/j.corsci.2010.07.002 ↗
44. Machuca · Corros. Sci. · 2013 · 67 · 24210.1016/j.corsci.2012.10.023 ↗
45. T. Charng, F. Lansing, TDA Progress Report 42–69, March and April 1982, pp. 145–156.
46. Yang · J. Electrochem. Soc. · 1999 · 146 · 210710.1149/1.1391899 ↗