Abstract

Abstract Surface abrasion has been shown to create altered surface layers (ASLs) that are hundreds of nm thick on all types of Al alloys. Such ASLs have lower corrosion resistance than the underlying substrate of Al-Zn-Mg-Cu alloys. Here, we demonstrate how heat treatments affect the ASL microstructure on abraded Al-Zn-Mg-Cu alloys using transmission electron microscopy and atom probe tomography, and also how the corrosion properties change using electrochemical polarization. High temperature treatments on the abraded bulk samples enhance η phase precipitation in the ASL, leading to a decreased Zn content in the ASL solid solution, which ennobles the ASL breakdown potential.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Materials Characterization Techniques · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Influence of heat treatment and surface conditioning on filiform corrosion of aluminium alloys AA3005 and AA575410.1016/S0010-938X(01)00019-1 ↗
2. Precipitation in an AA6111 aluminium alloy and cosmetic corrosion10.1016/j.actamat.2006.08.025 ↗
3. Near-surface deformed layers on rolled aluminum alloys10.1007/s11661-010-0538-2 ↗
4. The ubiquitous beilby layer on aluminium surfaces10.1002/sia.3204 ↗
5. Effect of heat treatment on filiform corrosion of aluminium alloy AA300510.1016/S0010-938X(01)00014-2 ↗
6. Filiform corrosion of aluminium sheet. III. Microstructure of reactive surfaces10.1016/S0010-938X(98)00094-8 ↗
7. Microstructure evolution in the near-surface region during homogenization of a twin-roll cast AlFeMnSi alloy10.1007/s11661-016-3568-6 ↗
8. The corrosion behaviour of machined AA7150-T651 aluminium alloy10.1016/j.corsci.2017.07.008 ↗
9. Chemistry and formation of the beilby layer during polishing of fused silica glass10.1111/jace.13659 ↗
10. The nature of mechanically polished surfaces of copper10.1016/0026-0800(85)90059-X ↗
11. A surface deformation region on mechanically polished surfaces of 316 stainless steels: its effects on the sensitization of the alloy10.1016/0956-716X(92)90635-R ↗
12. The effect of temper on the first breakdown in AA707510.1016/j.corsci.2007.02.004 ↗
13. On the first breakdown in AA7075-T610.1016/j.corsci.2007.02.001 ↗
14. Effect of altered surface layer on localized corrosion of aluminum alloy 202410.1149/2.1541706jes ↗
15. Mechanism of localized breakdown of 7000 series aluminum alloys10.1149/2.080310jes ↗
16. Influence of the altered surface layer on the corrosion of AA508310.1149/2.0321506jes ↗
17. Accelerated precipitation and growth of phases in an Al-Zn-Mg-Cu alloy processed by surface abrasion10.1016/j.actamat.2017.03.074 ↗
18. The subsurface structure of abraded Al-Zn-Mg-Cu alloy
19. Effects of long-term natural aging on the altered surface layer on an Al-Zn-Mg-Cu alloy and on corrosion properties10.1016/j.electacta.2018.02.001 ↗
20. In situ site-specific specimen preparation for atom probe tomography10.1016/j.ultramic.2006.06.008 ↗
21. Microstructure of two-phase Al–1.7 at% Cu alloy deformed by equal-channel angular pressing10.1016/S1359-6454(00)00308-6 ↗
22. Strain-induced dissolution of Cu-Mg co-clusters and dynamic recrystallization near a fatigue crack tip of an underaged Al-Cu-Mg alloy during cyclic loading at ambient temperature10.1016/j.scriptamat.2011.03.012 ↗
23. Cementite dissolution in heavily cold drawn pearlitic steel wires10.1016/S1359-6454(96)00216-9 ↗
24. Vurpillot · 2000
25. Pitting potential of high purity binary aluminium alloys-I. Al‒Cu alloys. Pitting and intergranular corrosion10.1016/0010-938X(77)90044-0 ↗
26. Pitting potential of high purity binary aluminium alloys-II. Al‒Mg and Al‒Zn alloys10.1016/S0010-938X(77)80014-0 ↗