Corrosion resistance and mechanism of X100 pipeline steel laser-metal active gas hybrid welds with Cr containing welding wire in NS4 solution
Source abstract
Abstract
The corrosion mechanism of pipeline steel laser-metal active gas (MAG) hybrid welds have been widely concerned with its applied in pipeline welding. The corrosion mechanism of X100 pipeline steel laser-MAG hybrid welds with Cr containing welding wire in NS 4 solution was investigated. The corrosion products of weld metal (WM) had a double-layer structure, of which the outer and the inner layer were composed of FeOOH and Cr(OH) 3 , respectively. Compared with the base metal (BM), WM had higher Cr content and more homogeneous microstructure, so it can form dense corrosion layer, making its corrosion resistance reach the level of the BM.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Effect of root welding heat input on microstructure evolution and fracture mechanism in intercritically reheat-coarse grained heat-affected zone of X80 pipeline steel
2. Acicular ferrite nucleation mechanism in laser-MAG hybrid welds of X100 pipeline steel10.1016/j.matlet.2021.130603 ↗
3. Effect of secondary peak temperature on microstructure and toughness in ICCGHAZ of laser-arc hybrid welded X100 pipeline steel joints10.1016/j.jmrt.2020.05.016 ↗
4. Hybrid laser arc welding of thick high-strength pipeline steels of grade X120 with adapted heat input
5. Influence of heat input and preheating on the cooling rate, microstructure and mechanical properties at the hybrid laser-arc welding of API 5L X80 steel10.1016/j.procir.2018.08.018 ↗
6. Deep penetration fiber laser-arc hybrid welding of thick HSLA steel10.1016/j.jmatprotec.2018.02.026 ↗
7. Laser-arc hybrid welding of thick HSLA steel10.1016/j.jmatprotec.2018.04.019 ↗
8. Effect of microstructure homogeneity on the impact fracture mechanism of X100 pipeline steel laser-MAG hybrid welds with an alternating magnetic field
9. Residual stress- microstructure- mechanical property interrelationships in multipass HSLA steel welds10.1016/j.jmatprotec.2016.01.020 ↗
10. Characterization of mechanical properties, fatigue-crack propagation, and residual stresses in a microalloyed pipeline-steel friction-stir weld10.1016/j.matdes.2015.09.049 ↗
11. Pitting corrosion in pipeline steel weld zones10.1016/j.corsci.2011.08.005 ↗
12. Early corrosion of mild steel in seawater10.1016/j.corsci.2004.08.006 ↗
13. Effects of Cr and Ni on the microstructure and corrosion resistance of high-strength low alloy steel10.1016/j.jmrt.2022.12.191 ↗
14. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
15. Microstructure characteristics of Q345R-steel welded joints and their corrosion behavior in a hydrofluoric acid environment10.1016/j.jnucmat.2022.154214 ↗
16. Effects of temperature on the corrosion behaviour of X70 steel in CO2-Containing formation water10.1016/j.jngse.2021.103815 ↗
17. The relationship between fracture toughness of CO2 corrosion scale and corrosion rate of X65 pipeline steel under supercritical CO2 condition10.1016/j.ijggc.2011.09.011 ↗
18. The role of Cr content on the corrosion resistance of carbon steel and low-Cr steels in the CO2-saturated brine10.1016/j.petsci.2022.11.016 ↗
19. Weathering steels: From empirical development to scientific design. A review10.1016/j.corsci.2014.03.006 ↗
20. Corrosion behaviors according to the welding process of superduplex stainless steel welded tubes: Gas tungsten arc welding vs. laser beam welding10.1016/j.corsci.2023.111108 ↗
21. Insight into sulfate-reducing bacteria corrosion behavior of X80 pipeline steel welded joint in a soil solution10.1016/j.jmrt.2023.04.163 ↗
22. Effect of secondary peak temperature on microstructure and toughness in ICCGHAZ of laser-arc hybrid welded X100 pipeline steel joints10.1016/j.jmrt.2020.05.016 ↗
23. Influence of heat input on the changes in the microstructure and fracture behavior of laser welded 800MPa grade high-strength low-alloy steel10.1016/j.jmapro.2019.12.007 ↗
24. Stress corrosion cracking behavior of X90 pipeline steel and its weld joint at different applied potentials in near-neutral solutions10.1016/j.ngib.2018.08.002 ↗
25. Study of electrochemical behavior, hydrogen permeation and diffusion in pipeline steel10.4028/www.scientific.net/MSF.1019.145 ↗
26. Hydrogen assisted cracking and CO2 corrosion behaviors of low-alloy steel with high strength used for armor layer of flexible pipe10.1016/j.apsusc.2018.01.223 ↗
27. Influence of alloyed chromium on the atmospheric corrosion resistance of weathering steels10.1016/j.corsci.2013.05.008 ↗
28. ASTM G1–03, Standard practice for preparing, cleaning, and evaluating corrosion test specimens, ASTM, West Conshohocken, Pennsylvania, United States.
29. Misorientation mapping for visualization of plastic deformation via electron back-scattered diffraction10.1017/S1431927606060120 ↗
30. Toughening of martensite matrix in high strength low alloy steel: Regulation of variant pairs10.1016/j.msea.2019.05.030 ↗
31. Thermodynamic basis of twin-related variant pair in high strength low alloy steel
32. Corrosion of low carbon steel in atmospheric environments of different chloride content10.1016/j.corsci.2009.02.009 ↗
33. Atmospheric corrosion of Ni-advanced weathering steels in marine atmospheres of moderate salinity10.1016/j.corsci.2013.06.053 ↗
34. Corrosion of Cr bearing low alloy pipeline steel in CO2 environment at static and flowing conditions10.1016/j.apsusc.2013.01.036 ↗
35. In situ synchrotron X-ray diffraction study of the effect of chromium additions to the steel and solution on CO2 corrosion of pipeline steels10.1016/j.corsci.2013.11.035 ↗
36. Determining the corrosive potential of CO2 transport pipeline in high CO2–water environments10.1016/j.ijggc.2010.11.008 ↗
37. The growth mechanism of CO2 corrosion product films10.1016/j.corsci.2010.09.060 ↗
38. Corrosion behavior of the 3 wt% Ni weathering steel with replacing 1 wt% Cr in the simulated tropical marine atmospheric environment10.1016/j.jpcs.2023.111221 ↗
39. The AC corrosion and SCC mechanism of X80 pipeline steel in near-neutral pH solution10.1016/j.engfailanal.2020.104904 ↗
40. Corrosion behavior of weathering steel in marine atmosphere10.1016/S0254-0584(02)00110-4 ↗
41. Atmospheric corrosion of carbon steel in Colombia10.1016/j.corsci.2009.09.006 ↗
42. The passivity of iron-chromium alloys10.1016/0010-938X(89)90060-7 ↗
43. Electrochemical behaviour and structure of rust formed on Si- and Al-bearing steel after atmospheric exposure10.1016/j.corsci.2010.07.006 ↗
44. The influence of carbon steel microstructure on corrosion layers: An XPS and SEM characterization10.1016/S0169-4332(02)01218-7 ↗
45. A comparative analysis on microstructure and fracture mechanism of X100 pipeline steel CGHAZ between laser welding and arc welding10.1007/s11665-019-04412-5 ↗
46. Effect of martensite-austenite (MA) distribution on mechanical properties of inter-critical Reheated Coarse Grain heat affected zone in X80 linepipe steel10.1016/j.msea.2019.138301 ↗
47. Corrosion behaviour of low-alloy martensite steel exposed to vapour-saturated CO2 and CO2-saturated brine conditions10.1016/j.electacta.2016.08.024 ↗
48. Influence of rare earth metals on mechanisms of localised corrosion induced by inclusions in Zr-Ti deoxidised low alloy steel10.1016/j.corsci.2020.108463 ↗
49. Mechanism of the dual effect of Te addition on the localised corrosion resistance of 15–5PH stainless steel10.1016/j.corsci.2023.110970 ↗
50. Effects of nanoscale Sn segregation on corrosion behavior of laser powder bed fusion Cu-15Ni-8Sn alloy10.1016/j.jmst.2023.01.056 ↗