New Rapid prototyping technology for the prevention of hydrogen embrittlement of metal strips
Source abstract
Abstract
Abstract Hydrogen embrittlement is a serious concern for advanced steels. In this research, twin-roll strip vibration cast-rolling was developed independently as a novel method for steel strip industrial production that inhibits hydrogen embrittlement. It reduces the hydrogen embrittlement sensitivity by optimizing the microstructure of strip steel products during the manufacturing process. Control experiments and cross-scale simulations were performed to reveal the phenomena and mechanisms that inhibit hydrogen embrittlement. The results show that the twin-roll strip vibration cast-rolling process can effectively reduce the hydrogen embrittlement sensitivity of steel strips.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Hydrogen enhances strength and ductility of an equiatomic highentropy alloy10.1038/s41598-017-10774-4 ↗
2. Understanding and mitigating hydrogen embrittlement of steels: a review of experimental, modelling and design progress from atomistic to continuum10.1007/s10853-017-1978-5 ↗
3. The influence of chemical composition and microstructure of API linepipe steels on hydrogen induced cracking and sulfide stress corrosion cracking10.1016/S0921-5093(03)00217-X ↗
4. Hardness assurance for proton direct ionization-induced SEEs using a high-energy proton beam10.1109/TNS.2014.2364953 ↗
5. Hydrogen embrittlement in bearing steels10.1080/02670836.2016.1156810 ↗
6. Influence of microstructure on the mechanical properties and hydrogen embrittlement characteristics of 1800 MPa grade hot-stamped 22MnB5 steel10.1007/s10853-018-3175-6 ↗
7. Role of in-service stress and strain fields on the hydrogen embrittlement of the pressure vessel constituent materials in a pressurized water reactor10.1016/j.engfailanal.2017.08.004 ↗
8. Enhanced hydrogen concentrations ahead of rounded notches and cracks—Competition between plastic strain and hydrostatic stress10.1016/S1359-6454(97)00364-9 ↗
9. Hydrogen embrittlement of high strength pipeline steels10.1016/j.corsci.2006.02.011 ↗
10. Hydrogen degradation of a boron-bearing steel with 1050 and 1300MPa strength levels10.1016/j.scriptamat.2004.10.023 ↗
11. Development of microalloyed steels through thin slab casting and rolling (TSCR) route10.1007/s12666-016-0963-z ↗
12. Characterization of microstructure, texture and magnetic properties in twin-roll casting high silicon non-oriented electrical steel
13. Microstructure,texture and precipitates of grain-oriented silicon steel produced by thin slab casting and rolling process10.1016/S1006-706X(17)30013-4 ↗
14. Recent progress on commercialization of CASTRIP direct strip casting technology at Nucor Crawfordsville10.1007/s11015-005-0016-z ↗
15. A comprehensive analysis of macrosegregation formation during twin-roll casting10.1007/s11663-019-01527-x ↗
16. A statistical-mechanical method to evaluate hydrogen solubility in metal10.1021/jp906506z ↗
17. Hydrogen trapping sites and hydrogen-induced cracking in high strength quenching & partitioning (Q&P) treated steel10.1016/j.ijhydene.2014.06.079 ↗
18. Improved resistance to hydrogen embrittlement in a high-strength steel by quenching–partitioning–tempering treatment10.1016/j.scriptamat.2014.10.030 ↗
19. Impact of heat treatment on the mechanical properties of AISI304L austenitic stainless steel in high-pressure hydrogen gas10.1007/s10853-012-6526-8 ↗
20. Hydrogen embrittlement property of a 1700-MPa-class ultrahigh-strength tempered martensitic steel10.1088/1468-6996/11/2/025005 ↗
21. Study of the effect of hydrogen charging on the tensile properties and microstructure of four variant heat treatments of nickel alloy 71810.1016/j.ijhydene.2017.02.149 ↗
22. Role of heat treatment and cathodic charging conditions on the hydrogen embrittlement of HP 7075 aluminum alloy10.1007/BF02782426 ↗
23. Accelerated corrosion exposure in ultra thin sheets of 2024 aircraft aluminium alloy for GLARE applications10.1016/j.corsci.2011.10.032 ↗
24. Novel methods for prevention of hydrogen embrittlement in Iron10.1038/s41598-017-17263-8 ↗
25. Inhibiting hydrogen embrittlement in ultra-strong steels for automotive applications by Ni-alloying
26. Comparative study on the efects of Cr, V, and Mo carbides for hydrogen-embrittlement resistance of tempered martensitic steel10.1038/s41598-019-41436-2 ↗
27. Role of Cu on hydrogen embrittlement behavior in Fe-Mn-C-Cu TWIP steel10.1016/j.ijhydene.2015.04.022 ↗
28. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
29. Effect of hydrogen charging on the mechanical properties of advanced high strength steels10.1016/j.ijhydene.2013.12.190 ↗
30. Phase stability effects on hydrogen embrittlement resistance in martensite-reverted austenite steels10.1007/s11661-018-4948-x ↗
31. Ab initio simulation of hydrogen-induced decohesion in cementite-containing microstructures10.1016/j.actamat.2018.03.005 ↗
32. Comparison of constant load, SSRT and CSRT methods for hydrogen embrittlement evaluation using round bar specimens of high strength steels10.2355/isijinternational.ISIJINT-2015-565 ↗
33. Influence of loading rate on the hydrogen-assisted micro-damage in bluntly notched samples of pearlitic steel
34. Generalised gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
35. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
36. Evaluation of finite element based analysis of 3D multicrystalline aggregates plasticity: Application to crystal plasticity model identification and the study of stress and strain fields near grain boundaries10.1016/j.ijplas.2004.05.017 ↗
37. Crystal space analysis by means of Voronoi–Dirichlet polyhedra10.1107/S0108767395006799 ↗
38. Effect of microstructure on hydrogen embrittlement of various stainless steels10.1016/j.msea.2013.07.004 ↗
39. Effect of retained austenite on the hydrogen embrittlement of a medium carbon quenching and partitioning steel with refined microstructure10.1016/j.msea.2016.04.025 ↗
40. The effect of grain size and aging on hydrogen embrittlement of a maraging steel10.1016/j.corsci.2008.06.044 ↗
41. Grain refinement and hydrogen embrittlement in iron aluminide alloy FA129
42. Effect of grain refinement on hydrogen embrittlement behaviors of high-Mn TWIP steel10.1016/j.msea.2015.11.017 ↗
43. The advantage of grain refinement in the hydrogen embrittlement of Fe–18Mn–0.6C twinning-induced plasticity steel10.1016/j.corsci.2015.01.012 ↗
44. Effect of ultrafine grain refinement on hydrogen embrittlement of metastable austenitic stainless steel10.1016/j.ijhydene.2017.04.249 ↗
45. Effect of hydrogen on the fracture behavior of high strength steel during slow strain rate test10.1016/j.corsci.2007.03.038 ↗
46. Effect of hydrogen content on the embrittlement in a Fe-Mn-C ternary twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
47. Studies of evaluation of hydrogen embrittlement property of high-strength steels with consideration of the effect of atmospheric corrosion10.1007/s11661-012-1403-2 ↗
48. Hydrogen-trapping mechanisms in nanostructured steels10.1007/s11661-013-1795-7 ↗
49. Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel
50. Diff ;usion of hydrogen into and through iron by density functional theory10.1016/j.susc.2018.02.001 ↗
51. Overview of hydrogen embrittlement in high-Mn steels10.1016/j.ijhydene.2017.02.214 ↗