journal article·2020-02Open access

Comparison of ZrB2-SiC, HfB2-SiC and HfB2-SiC-Y2O3 oxidation mechanisms in air using LIF of BO2(g)

V. Guérineau, G. Vilmart, N. Dorval, A. Julian-Jankowiak

Corrosion Science· Volume 163

Abstract

Abstract The oxidation behaviour of ZrB2-SiC, HfB2-SiC and HfB2-SiC-Y2O3 is studied using the real-time Laser-Induced Fluorescence (LIF) detection of BO2(g) evaporated from samples heated up to 1873K in dry air. For each composition, the relevant steps of oxidation (silica formation, volatilization, etc.) can be precisely determined. Moreover, the influence of composition on the oxidation behaviour, and more precisely on the B2O3/SiO2 ratio in the glassy phase, can be understood and described by monitoring the LIF signal from the BO2(g) radical. Thus, this technique has confirmed the potential of the HfB2-SiC-Y2O3 composition as a Ultra High Temperature Ceramic (UHTC) material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Nuclear materials and radiation effects

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. Oxidation of ZrB2- and HfB2-based ultra-high temperature ceramics: effect of Ta additions10.1023/B:JMSC.0000041693.32531.d1 ↗
2. Oxidation of ZrB2 ceramics modified with SiC and group IV-VI transition metal diborides
3. Oxidation of ZrB2-SiC ultra-high temperature composites over a wide range of SiC content10.1016/j.jeurceramsoc.2012.05.021 ↗
4. Processing and characterization of ZrB2-SiCW ultra-high temperature ceramics10.1016/j.jallcom.2008.04.082 ↗
5. Oxidation of ZrB2 and ZrB2-SiC ceramics with tungsten additions. High temperature corrosion and materials chemistry
6. Oxidation behavior of zirconium diboride silicon carbide produced by the spark plasma sintering method10.1111/j.1551-2916.2009.03134.x ↗
7. Oxidation of ultra-high temperature transition metal diboride ceramics10.1179/1743280411Y.0000000012 ↗
8. The thermal stability in air of hot-pressed diboride matrix composites for uses at ultra-high temperatures10.1016/j.corsci.2004.09.019 ↗
9. Oxidation resistance of hafnium diboride-silicon carbide from 1400 to 2000 °C10.1007/s10853-009-3799-7 ↗
10. SiC depletion in ZrB2-30 vol% SiC at ultrahigh temperatures10.1111/jace.13519 ↗
11. Initial stages of ZrB2-30 vol% SiC oxidation at 1500°C10.1111/jace.12843 ↗
12. Oxidation mechanism and resistance of ZrB2-SiC composites10.1016/j.corsci.2009.07.005 ↗
13. Oxidation mechanisms under water vapour conditions of ZrB2-SiC and HfB2-SiC based materials up to 2400°C10.1016/j.jeurceramsoc.2017.09.015 ↗
14. Oxidation of ZrB2-SiC10.1002/9780470294680.ch27 ↗
15. Oxidation of ultrahigh temperature ceramics in water vapor10.1149/1.1786929 ↗
16. Microstructural characterization of ZrB2–SiC based UHTC tested in the MESOX plasma facility10.1016/j.jeurceramsoc.2010.02.013 ↗
17. Temperature jump phenomenon during plasmatron testing of ZrB2-SiC ultrahigh-temperature ceramics10.2514/1.T3798 ↗
18. Qualitative analysis of hafnium diboride based ultra high temperature ceramics under oxyacetylene torch testing at temperatures above 2100°C10.1016/j.jeurceramsoc.2013.11.018 ↗
19. UHTC-carbon fibre composites: preparation, oxyacetylene torch testing and characterisation10.1016/j.jeurceramsoc.2012.08.018 ↗
20. Thermogravimetric study of the oxidation of ZrB2 in the temperature range of 800° to 1500°C10.1149/1.2408279 ↗
21. Oxidation-based materials selection for 2000°C + hypersonic aerosurfaces: theoretical considerations and historical experience10.1023/B:JMSC.0000041686.21788.77 ↗
22. Effect of heat flux on ablation behaviour and mechanism of C/C–ZrB2–SiC composite under oxyacetylene torch flame10.1016/j.corsci.2013.04.052 ↗
23. Behavior of a sample of the ceramic material HfB2-SiC (45 vol %) in the flow of dissociated air and the analysis of the emission spectrum of the boundary layer above its surface10.1134/S0036023615110133 ↗
24. Optical emission spectroscopy during plasmatron testing of ZrB2-SiC ultrahigh-temperature ceramic composites10.2514/1.39974 ↗
25. In situ study of the oxidation of ZrB2 and ZrB2-SiC materials by monitoring the LIF signal of BO2 radicals10.1016/j.corsci.2018.11.032 ↗
26. The absorption spectrum of BO210.1139/p61-199 ↗
27. Oxidation of ZrB2–SiC: influence of SiC content on solid and liquid oxide phase formation10.1111/j.1551-2916.2008.02874.x ↗
28. Convection patterns in liquid oxide films on ZrB2-SiC composites oxidized at a high temperature10.1111/j.1551-2916.2007.01784.x ↗
29. Formation of oxide scales on zirconium diboride–silicon carbide composites during oxidation: relation of subscale recession to liquid oxide flow10.1111/j.1551-2916.2008.02639.x ↗
30. The ZrB2 volatility diagram10.1111/j.1551-2916.2005.00599.x ↗
31. Thermodynamic calculation of HfB2 volatility diagram10.1007/s11669-011-9930-x ↗
32. Thermodynamic analysis of ZrB2–SiC oxidation: formation of a SiC-depleted region10.1111/j.1551-2916.2006.01329.x ↗
33. Modeling oxidation kinetics of SiC-containing refractory diborides10.1111/j.1551-2916.2011.04927.x ↗
34. Promising ultra-high-temperature ceramic materials for aerospace applications10.1134/S0036023613140039 ↗
35. Refractory diborides of zirconium and hafnium10.1111/j.1551-2916.2007.01583.x ↗
36. Effect of yttrium oxide on the viscosity and crystallization of borosilicate glass at high temperature10.4028/www.scientific.net/AMR.750-752.974 ↗
37. SiC recession caused by SiO2 scale volatility under combustion conditions: II, thermodynamics and gaseous-diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
38. Ionic conductivity of the fluorite-type hafnia–RE2O3 solid solutions10.1111/j.1151-2916.1991.tb06790.x ↗
39. Phase equilibria and ionic conductivity in the system ZrO2-Yb2O3-Y2O310.1111/j.1151-2916.1985.tb15293.x ↗