Combined effects of irradiation and hydrogen ions on surface oxidation of 308 L austenite stainless steel
Source abstract
Abstract
Abstract The harsh environment in pressurized water reactor involving neutron irradiation and hydrogen from the water radiolysis poses significant challenges on the passivation of materials therein. Here, we probed the combined effects of hydrogen and irradiation on the oxidation of 308 L austenite stainless steel. Hydrogen lowers the electron work function of the steel. Oxide film on the irradiated and hydrogenated surface is thicker, and has a higher electrical conductivity than that on the unirradiated surface. The findings are associated with the interaction between hydrogen and irradiation-induced voids which prompts the oxidation kinetics and considerably changes the scale structure and composition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Ion-surface interactions and analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (90)
Show source-provided references
1. Deformation in metals after low-temperature irradiation: Part II – Irradiation hardening, strain hardening, and stress ratios10.1016/j.actamat.2007.10.056 ↗
2. Corrosion of phase and phase boundary in proton-irradiated 308L stainless steel weld metal in simulated PWR primary water10.1016/j.corsci.2019.108401 ↗
3. Effect of irradiation on corrosion of 304 nuclear grade stainless steel in simulated PWR primary water10.1016/j.corsci.2017.08.010 ↗
4. Proton irradiation effects on the electron work function, corrosion and hardness of austenitic stainless steel phases10.1016/j.corsci.2019.06.011 ↗
5. Environmentally assisted crack growth in 308L stainless steel weld metal in simulated primary water10.1016/j.corsci.2016.12.011 ↗
6. Characterization of microstructure of A508III/309L/308L weld and oxide films formed in deaerated high-temperature water10.1016/j.jnucmat.2017.10.030 ↗
7. Environmentally assisted fatigue behavior of 308L weld metal in borated and lithiated high-temperature water10.1016/j.jnucmat.2020.152365 ↗
8. Investigation of the oxide film on 308L weld surface produced during welding process10.1016/j.matchar.2018.09.011 ↗
9. Intergranular oxidation of Ni-based Alloy 600 in a simulated PWR primary water environment10.1016/j.corsci.2016.02.040 ↗
10. Characterization of interfacial reactions and oxide films on 316L stainless steel in-various simulated PWR primary water environments10.1016/j.jnucmat.2017.03.029 ↗
11. The corrosion behaviour of alloy 690 tube in simulated PWR secondary water with the effect of solid diffusing hydrogen10.1016/j.jnucmat.2019.02.019 ↗
12. Oxidation kinetics and mechanisms of Ni-base alloys in pressurised water reactor primary conditions: influence of subsurface defects10.1016/j.corsci.2011.07.024 ↗
13. Effect of implantation defects on the corrosion of 316L stainless steels in primary medium of pressurized water reactors10.1016/j.corsci.2016.02.007 ↗
14. Influence of irradiation on the oxide film formed on 316L stainless steel in PWR primary water10.1007/s11085-013-9401-3 ↗
15. Accelerated corrosion and oxide dissolution in 316L stainless steel irradiated in situ in high temperature water10.1016/j.jnucmat.2017.05.043 ↗
16. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
17. Characterization of ion irradiation effects on the microstructure, hardness, deformation and crack initiation behavior of austenitic stainless steel:heavy ions vs protons10.1016/j.jnucmat.2018.01.013 ↗
18. Current understanding of radiation-induced degradation in light water reactor structural materials10.1080/00223131.2013.772448 ↗
19. Proton irradiation effects on hardness and the volta potential of welding 308L duplex stainless steel10.3390/mi10010011 ↗
20. The oxidation of alloy 690 in simulated pressurized water reactor primary water10.1016/j.corsci.2017.07.004 ↗
21. Effect of surface machining on the corrosion behaviour of 316 austenitic stainless steel in simulated PWR water10.1016/j.corsci.2017.06.019 ↗
22. ToF-SIMS study of oxide films thermally grown on nickel-base alloys10.1016/j.corsci.2018.06.043 ↗
23. The mechanism of high temperature aqueous corrosion of steel10.1016/0010-938X(89)90120-0 ↗
24. Effect of surface preparation on the corrosion of austenitic stainless steel 304L in high temperature steam and simulated PWR primary water10.1016/j.corsci.2011.12.007 ↗
25. The effect of post-irradiation annealing on the stress corrosion crack growth rate of neutron-irradiated 304L stainless steel in boiling water reactor environment10.1016/j.corsci.2019.108183 ↗
26. A transmission electron microscopy study of EBR-II neutron-irradiated austenitic stainless steel 304 and nickel-base alloy X-75010.1016/j.jnucmat.2019.151851 ↗
27. Radiolysis driven changes to oxide stability during irradiation-corrosion of 316L stainless steel in high temperature water10.1016/j.jnucmat.2017.05.042 ↗
28. The mechanism of hydrogen-induced pitting corrosion in duplex stainless steel studied by SKPFM10.1016/j.corsci.2012.04.010 ↗
29. Atomic origins of water-vapour-promoted alloy oxidation10.1038/s41563-018-0078-5 ↗
30. Hydrogen-modified dislocation structures in a cyclically deformed ferritic-pearlitic low carbon steel10.1016/j.actamat.2017.10.034 ↗
31. Hydrogen effects on pitting corrosion and semiconducting properties of nitrogen-containing type 316L stainless steel10.1016/j.electacta.2009.06.003 ↗
32. Coupling effect of microstructure and hydrogen absorbed during service on pitting corrosion of 321 austenitic stainless steel weld joints10.1016/j.corsci.2019.108339 ↗
33. Hydrogen induced vacancy clustering and void formation mechanisms at grain boundaries in palladium10.1016/j.actamat.2020.06.007 ↗
34. Temperature dependence of vacancy concentration and void growth mechanism in Al with constant hydrogen concentration: a first-principles study10.1016/j.engfracmech.2019.106508 ↗
35. Effect of hydrogen atom and hydrogen filled vacancies on stacking fault energy in γ-Fe by first-principles calculations10.1016/j.ijhydene.2019.04.229 ↗
36. First principles investigations of hydrogen interaction with vacancy-oxygen complexes in vanadium alloys10.1016/j.ijhydene.2019.08.123 ↗
37. Fundamentals of radiation materials science
38. A study to compute integrated dpa for neutron and ion irradiation environments using SRIM-201310.1016/j.jnucmat.2018.02.039 ↗
39. Proton irradiation and characterization of additively manufactured 304L stainless steels10.1016/j.jnucmat.2020.152007 ↗
40. An abnormal correlation between electron work function and corrosion resistance in Ti-Zr-Be-(Ni/Fe) metallic glasses10.1016/j.corsci.2019.108392 ↗
41. Mechanical and metallurgical changes on 308L wires drawn by electropulses10.1016/j.matdes.2015.11.067 ↗
42. Microstructure and mechanical properties of 308L stainless steel fabricated by laminar plasma additive manufacturing10.1016/j.msea.2019.138523 ↗
43. The effects of proton irradiation on the microstructural and mechanical property evolution of inconel X-750 with high concentrations of helium10.1016/j.jnucmat.2017.04.045 ↗
44. Linear relation between surface roughness and work function of light alloys10.1016/j.jallcom.2016.09.102 ↗
45. Effect of surface roughness on electron work function of AZ31 Mg alloy and their correlation10.1016/j.jallcom.2017.10.007 ↗
46. Effect of annealing temperature on the corrosion behavior of duplex stainless steel studied by in situ techniques10.1016/j.corsci.2011.07.019 ↗
47. Surface preparation effect on duplex stainless steel passive film electrical properties studied by in situ CSAFM10.1557/jmr.2015.245 ↗
48. Insight into the corrosion behaviour and degradation mechanism of pure zinc in simulated body fluid10.1016/j.corsci.2020.109071 ↗
49. Experimental study on the diffusion of hydrogen along individual grain boundaries in nickel10.1016/j.elecom.2018.05.012 ↗
50. CS-AFM study on Pb-induced degradation of passive film on nickel-based alloy in high temperature and high pressure water10.1016/j.corsci.2018.08.054 ↗
51. Determination of hydrogen trapping mechanisms by microprinting in Ni and Co coatings obtained by HVOF10.1016/j.surfcoat.2019.01.111 ↗
52. Hydrogen emission at grain boundaries in tensile-deformed Al-9%Mg alloy by hydrogen microprint technique10.1016/S1003-6326(14)63318-5 ↗
53. Behavior of hydrogen in an Ni3Al compound investigated by means of hydrogen microprint technique10.1016/S0966-9795(99)00166-1 ↗
54. Oxide layer growth on nickel-base alloy surfaces in high temperature water and in O2 studied by ToF-SIMS with isotopic tracers10.1016/j.corsci.2018.10.009 ↗
55. Ion transport mechanisms in the passive film formed on 304 L stainless steel studied by ToF-SIMS with 18O isotopic tracer10.1016/j.corsci.2020.108779 ↗
56. Comparative study of the surface oxide films on lean duplex and corresponding single phase stainless steels by XPS and ToF-SIMS10.1016/j.corsci.2018.08.009 ↗
57. ToF-SIMS depth profile of the surface film on pure magnesium formed by immersion in pure water and the identification of magnesium hydride10.1016/j.corsci.2009.06.002 ↗
58. Surface roughness optimisation for selective laser melting (SLM): accommodating relevant and irrelevant surfaces
59. Radiation-induced solute segregation in metallic alloys10.1016/j.cossms.2015.11.001 ↗
60. On the effect of radiation-induced segregation on void shape and growth rate10.1016/0022-3115(91)90511-5 ↗
61. Effect of aging treatment on irradiation-induced segregation of high Mn-Cr steel10.1016/S1003-6326(11)61061-3 ↗
62. Correlation between electron work functions of multiphase Cu-8Mn-8Al and de-alloying corrosion10.1016/j.apsusc.2018.01.018 ↗
63. Effects of elastic and plastic deformations on the electron work function of metals during bending tests10.1080/14786430412331305294 ↗
64. Proton irradiation damage in cold worked Nb-stabilized 20Cr-25Ni stainless steel10.1016/j.apsusc.2018.05.128 ↗
65. Effect of chromium on void swelling in ion irradiated high purity Fe–Cr alloys10.1016/j.actamat.2016.02.027 ↗
66. Effects of 3d electron configurations on helium bubble formation and void swelling in concentrated solid-solution alloys10.1016/j.actamat.2019.10.013 ↗
67. Depth dependent damage profile in stainless steel irradiated with He-ions10.1016/0022-3115(83)90019-3 ↗
68. A Technique for preparing the cross-section of proton-irradiated 316 stainless steel foils for transmission electron microscopy10.1016/0022-3115(72)90046-3 ↗
69. AFM study of austeno-ferritic stainless steel microstructure after cathodic hydrogen charging10.1016/j.jallcom.2005.02.084 ↗
70. Effects of oxides produced during welding on oxidation behavior of the 304L welded joint in simulated primary circuit solution of PWR10.1016/j.corsci.2020.108515 ↗
71. Methodology for determining void swelling at very high damage under ion irradiation10.1016/j.jnucmat.2016.05.026 ↗
72. Microstructural changes of 316L stainless steel under energetic alpha particle and proton irradiation at 500°C10.1016/0022-3115(92)90568-6 ↗
73. Formation process of dislocation loops in iron under irradiations with low-energy helium, hydrogen ions or high-energy electrons10.1016/S0022-3115(02)01251-5 ↗
74. The influence of hydrogen on void swelling in fusion reactor materials10.1016/0022-3115(88)90431-X ↗
75. Hydrogen pickup during oxidation in aqueous environments: the role of nano-pores and nano-pipes in zirconium oxide films10.1016/j.actamat.2019.09.005 ↗
76. Effects of alloying elements on vacancies and vacancy-hydrogen clusters at coherent twin boundaries in nickel alloys10.1016/j.actamat.2018.01.037 ↗
77. Correlation between resistivity and oxygen vacancy of hydrogen-doped indium tin oxide thin films10.1016/j.tsf.2011.01.249 ↗
78. Mechanistic understanding of the roles of hydrogen in modification of oxide film of alloy 600 in high temperature high pressure water environment10.1016/j.corsci.2020.108656 ↗
79. Effects of surface oxide films on hydrogen permeation and susceptibility to embrittlement of X80 steel under hydrogen atmosphere10.1016/j.ijhydene.2017.12.170 ↗
80. Atomistic simulations of Ni segregation to irradiation induced dislocation loops in Zr-Ni alloys10.1016/j.actamat.2017.08.016 ↗
81. Precipitation behavior in G-phase strengthened ferritic stainless steels10.1016/j.actamat.2020.116542 ↗
82. Defect structure and transport properties of (Co,Cr,Fe,Mn,Ni)3O4 spinel-structured high entropy oxide10.1016/j.jeurceramsoc.2019.10.026 ↗
83. Electrocatalytic behavior of transition metal (Ni, Fe, Cr) doped metal oxide nanocomposites for oxygen evolution reaction10.1016/j.apsusc.2017.12.014 ↗
84. Insights into high-temperature oxidation of Fe-Mn-Si-Cr-Ni shape memory stainless steels and its relationship to alloy chemical composition10.1016/j.corsci.2019.108269 ↗
85. Impact of the voids on the cracking behavior of the duplex oxide scale on the 18%Cr austenite alloy surface10.1016/j.corsci.2019.108298 ↗
86. Bubble-to-void transition promoted by oxide nanoparticles in ODS-EUROFER steel ion implanted to high He content10.1016/j.jnucmat.2020.152724 ↗
87. Defect and void evolution in oxide dispersion strengthened ferritic steels under 3.2 MeV Fe+ ion irradiation with simultaneous helium injection10.1016/S0022-3115(00)00066-0 ↗
88. The effects of temperature and oxygen pressure on the initial oxidation of stainless steel 44110.1016/j.ijhydene.2014.04.188 ↗
89. The transient oxidation of alloys10.1007/BF00604477 ↗
90. The initial oxidation of type 430 stainless steel in O2-H2O-N2 atmospheres at 1273 K10.1016/0010-938X(96)00093-5 ↗