Inhibition of metal dusting corrosion on Fe-based alloy by combined near surface severe plastic deformation (NS-SPD) and thermochemical treatment
Source abstract
Abstract
Combined NS-SPD and thermochemical treatment has been used to improve the metal dusting corrosion resistance of Incoloy 800. After testing under infinite carbon activity for 20−100 h, carbon was not found in the NS-SPD region while corrosion products formed in the non-NS-SPD region. The improved resistance is a result of the NS-SPD yielding a high density of defects in the deformation zone that developed into an ultra-fine-grained structure near the surface during the subsequent thermochemical treatment. These microstructural changes increase the effective diffusion coefficient for Cr in the alloy, hence promoting the formation of a highly protective oxide scale .
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (94)
Show source-provided references
1. Why stainless steel corrodes10.1038/415770a ↗
2. Marcus · 2011
3. Metal dusting of high temperature alloys10.1002/maco.19930440306 ↗
4. On the mechanism of catastrophic carburization: ‘metal dusting’10.1016/0010-938X(93)90334-D ↗
5. Metal dusting10.1002/maco.200303729 ↗
6. In situ environmental scanning electron microscope observations of catalytic processes encountered in metal dusting corrosion on iron and nickel10.1016/S0926-860X(01)00539-7 ↗
7. Mechanisms of metal dusting corrosion of iron10.1149/1.1483099 ↗
8. Szakálos · 2004
9. Investigation of metal-dusting mechanism in Fe-base alloys using raman spectroscopy, x-ray diffraction, and electron microscopy
10. Hummelshøj · 2010
11. Understanding metal dusting mechanisms10.1149/1.3224738 ↗
12. Mechanism of metal dusting corrosion by pitting of a chromia-forming alloy at atmospheric pressure and low gas velocity10.1016/j.corsci.2016.02.033 ↗
13. Studies of the mechanism of metal dusting of 10CrMo9-10 steel after 10 years of operation in the semi-regenerative catalytic reformer10.1016/j.corsci.2015.10.016 ↗
14. Recent advances in understanding metal dusting: a review10.1002/maco.201005675 ↗
15. Thermodynamics, mechanisms and kinetics of metal dusting10.1002/(SICI)1521-4176(199805)49:5<303::AID-MACO303>3.0.CO;2-P ↗
16. Effect of gas composition on coking and metal dusting of 2.25Cr–1Mo steel compared with iron10.1016/j.corsci.2009.08.026 ↗
17. The interaction of surface engineering and high temperature corrosion protection10.1080/09603409.1994.11689470 ↗
18. Protection of high alloy steels against metal dusting by oxide scales10.1002/(SICI)1521-4176(199805)49:5<317::AID-MACO317>3.0.CO;2-5 ↗
19. Inhibition of metal dusting of Alloy 800H by laser surface melting10.1016/j.apsusc.2005.05.040 ↗
20. Resistance of Ni-base alloy UNS N 06696 to metal dusting
21. Effect of pressure on metal dusting initiation on alloy 800H and alloy 600 in CO-rich syngas10.1007/s11085-017-9801-x ↗
22. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
23. Effect of oxide scale compositions on metal dusting corrosion of Fe-based alloys10.5006/1.3287838 ↗
24. Role of alloying elements in steels on metal dusting10.1002/(SICI)1521-4176(199805)49:5<321::AID-MACO321>3.0.CO;2-P ↗
25. Protective behaviour of newly developed coatings against metal dusting10.1002/maco.200303736 ↗
26. A study on the solubility and distribution of carbon in oxides10.1016/0038-1098(85)91021-X ↗
27. Effects of grain size, cold working, and surface finish on the metal-dusting resistance of steels10.1023/A:1018888321213 ↗
28. Metal dusting of Fe–Cr and Fe–Ni–Cr alloys under cyclic conditions10.1023/A:1016032722703 ↗
29. Crystal structure and isothermal compression of Fe2O3, Cr2O3, and V2O3 to 50 kbars10.1063/1.327451 ↗
30. Gas phase initial oxidation of incoloy 800 surfaces10.1007/s11085-012-9316-4 ↗
31. The effect of water vapor on selective oxidation of Fe–Cr alloys10.1007/s11085-007-9090-x ↗
32. Initiation of metal-dusting pits and a method to mitigate metal-dusting corrosion10.1007/s11085-006-9032-z ↗
33. The effect of manganese and chromium on surface oxidation products formed during batch annealing of low carbon steel strip10.1016/j.corsci.2006.06.013 ↗
34. High temperature carburization behaviour of Mn–Cr–O spinel oxides with varied concentrations of manganese10.1016/j.corsci.2011.02.021 ↗
35. Stability of MnCr2O4 spinel and Cr2O3 in high temperature carbonaceous environments with varied oxygen partial pressures10.1016/j.corsci.2010.02.040 ↗
36. Carburization behaviour of Mn–Cr–O spinel in high temperature hydrocarbon cracking environment10.1016/j.corsci.2009.06.006 ↗
37. T. A. Ramanarayanan and C. Chun, "Metal dusting resistant alloys," ed: Google Patents, 2004.
38. Inhibitory effect of MnCr 2 O 4 spinel coating on coke formation during light naphtha thermal cracking10.1039/C6RA13009G ↗
39. The features of metal dusting process in the extremely low nickel austenitic stainless steel (18Cr-21Mn-0.65 N-Fe)10.1016/j.corsci.2020.108926 ↗
40. Effect of yttrium on the coking behavior of Fe-based superalloy in heavy hydrocarbon10.1016/j.corsci.2015.05.018 ↗
41. The evolution and oxidation of carbides in an Alloy 601 exposed to long term high temperature corrosion conditions10.1016/j.corsci.2010.08.015 ↗
42. Oxidation behavior of Incoloy 800 under simulated supercritical water conditions10.1016/j.jnucmat.2008.12.004 ↗
43. Oxidation of heat-resistant Fe-base incoloy 800 alloy10.2320/matertrans1960.18.567 ↗
44. Effect of element diffusion through metallic networks during oxidation of Type 321 stainless steel10.1007/s11665-014-0909-8 ↗
45. Playing with defects in metals10.1038/nmat4929 ↗
46. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
47. Lattice and grain boundary diffusion of chromium in superalloy Incoloy-80010.1016/0022-3115(94)90306-9 ↗
48. Extreme grain refinement by severe plastic deformation: a wealth of challenging science10.1016/j.actamat.2012.10.038 ↗
49. Analytical and numerical approaches to modelling severe plastic deformation10.1016/j.pmatsci.2018.02.001 ↗
50. ARB (Accumulative Roll‐Bonding) and other new techniques to produce bulk ultrafine grained materials10.1002/adem.200310077 ↗
51. Surface nanocrystallization (SNC) of metallic materials-presentation of the concept behind a new approach
52. The influence of nanocrystalline structure and processing route on corrosion of stainless steel: a review10.1016/j.corsci.2014.11.041 ↗
53. Nanostructured materials: basic concepts and microstructure10.1016/S1359-6454(99)00285-2 ↗
54. On the contribution of triple junctions to the structure and properties of nanocrystalline materials10.1016/0956-716X(90)90354-J ↗
55. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
56. Electrochemical corrosion behavior of nanocrystalline materials—a review10.1016/S1005-0302(10)60001-1 ↗
57. Influence of near-surface severe plastic deformation of mild steel on the inhibition performance of sodium molybdate and 1H-benzotriazole in artificial sea water10.1007/s11665-018-3130-3 ↗
58. Effect of cold work on surface reactivity and nano-hardness of alloy 800 in corroding environments10.1016/j.apsusc.2013.01.150 ↗
59. Surface nanocrystallization induced by shot peening and its effect on corrosion resistance of 1Cr18Ni9Ti stainless steel10.1016/j.surfcoat.2005.04.046 ↗
60. The effect of ultrasonic nanocrystal surface modification on low temperature nitriding of ultra-high strength steel10.1016/j.surfcoat.2019.07.006 ↗
61. Diffusion of chromium in nanocrystalline iron produced by means of surface mechanical attrition treatment10.1016/S1359-6454(03)00260-X ↗
62. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
63. A combination of Al diffusion and surface nanocrystallization of carbon steel for enhanced corrosion resistance10.1080/09500830902722806 ↗
64. Effect of grain refinement on corrosion of ferritic-martensitic steels in supercritical water environment10.1002/maco.200905446 ↗
65. Enhancing the mechanical and biological performance of a metallic biomaterial for orthopedic applications through changes in the surface oxide layer by nanocrystalline surface modification10.1039/C5NR00574D ↗
66. Ultrasonic cavitation erosion-corrosion behavior of friction stir processed stainless steel10.1016/j.ultsonch.2018.02.041 ↗
67. Corrosion by carbonaceous gases, carburization and metal dusting, and methods of prevention10.1179/mht.2000.063 ↗
68. The influence of surface condition on the metal dusting behavior of cast and wrought chromia forming alloys10.1002/maco.201106425 ↗
69. Formation of chromium rich oxide scales for protection against metal dusting10.1179/mht.2000.17.2.023 ↗
70. Occurrence and prevention of metal dusting on stainless steels
71. Internal oxidation and carburisation of heat-resistant alloys10.1016/S0010-938X(02)00182-8 ↗
72. Morphological and microstructural aspects of metal dusting on 304L stainless steel with different surface treatments10.1007/s11085-004-7805-9 ↗
73. Metal dusting corrosion of austenitic 304 stainless steel10.1149/1.1872632 ↗
74. Metal dusting of Inconel 625 obtained by laser beam melting: effect of manufacturing process and hot isostatic pressure treatment10.1016/j.corsci.2020.108820 ↗
75. Gunawardana · 2014
76. Effects of metal dusting relevant exposures of alloy 601 surfaces on carbon formation and oxide development
77. Raman spectroscopy as a versatile tool for studying the properties of graphene10.1038/nnano.2013.46 ↗
78. Raman spectroscopy of graphene and related materials
79. Investigation of metal dusting corrosion process over UNS N08800 alloy
80. Selective oxidation synthesis of MnCr2O4 spinel nanowires from commercial stainless steel foil10.1021/cg070514a ↗
81. Hosterman · 2011
82. Characterization of surface oxides by Raman spectroscopy10.1063/1.91429 ↗
83. In-situ Raman spectroscopy combined with x-ray photoelectron spectroscopy and nuclear microanalysis for studies of anodic corrosion film formation on Fe-Cr single crystals10.1149/1.2095605 ↗
84. Coke formation and metal dusting of electroplated Ni3Al–CeO2-based coatings in CO–H2–H2O10.1016/j.corsci.2007.05.016 ↗
85. The influence of the high Fe and Cr contents of Alloy 800 on its inter-and intragranular oxidation tendency in 480° C hydrogenated steam10.1016/j.corsci.2016.01.031 ↗
86. Initiation of metal dusting corrosion in conversion of natural gas to syngas studied under industrially relevant conditions10.1021/ie4024947 ↗
87. Interaction of oxide layers with dislocations for an austenitic stainless steel10.1016/S0921-5093(01)00914-5 ↗
88. Differences in oxides on large-and small-grained 304 stainless steel10.1007/BF02655116 ↗
89. Internal oxidation of alloy 690 in hydrogenated steam10.1016/j.corsci.2014.11.006 ↗
90. An atom probe tomography study of internal oxidation processes in Alloy 60010.1016/j.actamat.2016.02.054 ↗
91. Young · 2008
92. Carburization and oxidation10.1016/0025-5416(87)90357-0 ↗
93. Cyclic oxidation plus carburization of heat-resistant alloys10.5006/1.3294361 ↗
94. Gaseous pretreatment of high-alloy steels used in ethylene furnaces: pretreatment of Incoloy 80010.1021/ie030422s ↗