New insight on study of Ni-base alloy clad layer after oxidation at 650 °C
Source abstract
Abstract
Abstract The investigation was carried out on the Ni-based alloy (Inconel 625) clad layer after oxidation at a temperature of 650 °C for a duration of 2000 h in an atmosphere of ash from a waste incineration plant. The characterization of the oxide scale was performed using phase mapping technique (ASTAR) of transmission electron microscopy. The investigation revealed formation of two-layered continuous passive oxide scale on the surface of the superalloy. Its outer zone is built from NiO and inner zone is composed mainly of Cr2O3. Between the above mentioned oxide layers, the NiCr2O4 spinel and NbCrO4 oxide have been observed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Catalytic Processes in Materials Science · High-Temperature Coating Behaviors · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Hot corrosion & erosion problems in coal based power plants in india and possible solutions – a review
2. Wastes and biomass materials as sustainable-renewable energy resources for Jordan10.1016/j.rser.2016.09.035 ↗
3. Solid particle erosion on different metallic materials
4. New technologies for waste to energy plants
5. Padding of the components of waste combustion boilers with the use of nickel alloys
6. Improving corrosion properties of high-velocity oxy-fuel sprayed inconel 625 by using a high- power continuous wave neodymium-doped yttrium aluminum garnet laser10.1007/BF02608555 ↗
7. Singbelil · 1997
8. Microstructure and mechanical properties of Inconel 625 superalloy10.1016/S0022-3115(00)00723-6 ↗
9. 2013 · 1
10. Characterization of microstructures in Inconel 625 using X-ray diffraction peak broadening and lattice parameter measurements10.1016/j.scriptamat.2004.03.017 ↗
11. High temperature corrosion of power boiler components cladded with nickel alloys10.1016/j.matchar.2009.03.017 ↗
12. DuPont · 2009
13. Dokument · 2001
14. 2013
15. Characterisation of the cold metal transfer (CMT) process and its application for low dilution cladding10.1016/j.jmatprotec.2010.11.005 ↗
16. Evaluation of cold metal transfer (CMT) process for welding aluminium alloy10.1179/174329306X120886 ↗
17. Mechanical properties of Inconel 625 laser cladded coatings: depth sensing indentation analysis10.1016/j.msea.2014.01.026 ↗
18. Solidification and weldability of Nb-bearing superalloys
19. High temperature oxidation behaviour of NbC-reinforced cast superalloys
20. McCafferty · 2010
21. Uhlig · 2008
22. High-temperature corrosion and materials applications
23. Gas corrosion of metals
24. Kofstad · 1988
25. Effect of dissolved oxygen content on the oxide structure of Alloy 625 in supercritical water environments at 700°C10.1016/j.corsci.2013.11.034 ↗
26. Microsctructure, chemical and phase composition of clad layers of Inconel 625 and Inconel 686
27. Microstructure, microsegregation and nanohardness of CMT clad layers of Ni-base alloy on 16Mo3 steel10.1016/j.jallcom.2018.04.102 ↗
28. High-temperature corrosion of Ni-base alloys by waste incineration ashes10.12693/APhysPolA.130.1045 ↗
29. Sulfur recirculation for increased electricity production in waste to energy plants10.1016/j.wasman.2013.09.002 ↗
30. Hot corrosion behavior of boiler tube materials in refuse incineration environment10.1016/S0042-207X(01)00468-7 ↗
31. A novel approach to the characterization of thin oxide layers10.1016/j.matlet.2016.02.104 ↗
32. Studies of the oxidation of nickel in the temperature range of 900° to 1400°C10.1149/1.2423553 ↗
33. High temperature oxidation
34. Oxidation of Ni-Cr-Al alloys between 1000° and 1200°C10.1149/1.2407837 ↗
35. Neil Birks · 2006
36. The oxidation behaviour of a niobium- chromium-nickel alloy10.1016/0010-938X(76)90048-2 ↗
37. Hot corrosion of inconel 625 overlay weld cladding in smelting off-gas environment10.1007/s11661-013-1803-y ↗