journal article·2017-12

Simultaneous oxidation and carburization of a Fe-9Cr alloy under different oxygen pressures at 800 °C

J. Shen, S. Liu, X.H. Guo, Y. Niu

Corrosion Science· Volume 129
Publisher page

Abstract

Abstract A model Fe-9Cr alloy was exposed to various H 2 CO 2 CH 4 mixtures providing different oxygen pressures and carbon activities at 800 °C. Three oxidation modes and three oxygen pressure ranges have been observed. At low pressures (Range I) only thin external Cr 2 O 3 scales formed. An intermediate range (Range II) produced an internal precipitation of Cr 2 O 3 and Cr carbide without an external scale. Higher pressures (Range III) produced external FeO x scales plus an internal oxidation of Cr. Two critical oxygen pressures for the transitions between the three oxidation modes were observed and also calculated in reasonable agreement with the experimental results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Metal Alloys Wear and Properties · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Corrosion of austenitic alloys in high temperature supercritical carbon dioxide10.1016/j.corsci.2012.03.029 ↗
2. Fireside issues in advanced power Generation systems10.1179/1743284712Y.0000000133 ↗
3. Refractory metals − an exploration of high-temperature materials10.1007/s11837-010-0147-y ↗
4. Influence of novel cycle concepts on the high-temperature corrosion of power plants10.1002/maco.200804116 ↗
5. Effect of element diffusion through metallic networks during oxidation of type 321 stainless steel10.1007/s11665-014-0909-8 ↗
6. Young · 2008
7. High-temperature corrosion and creep of Ni-Cr-Fe alloys in carburizing and oxidizing environments10.1007/BF00612086 ↗
8. Effect of scale constitution on the carburization of heat-resistant steels10.1007/BF00659345 ↗
9. Water vapor effects on the oxidation behavior of Fe-Cr and Ni-Cr Alloys in atmospheres relevant to oxy-fuel combustion10.1007/s11085-012-9302-x ↗
10. Carburization and metal dusting on iron10.2355/isijinternational.41.Suppl_S1 ↗
11. Carburisation and metal dusting in hydrogen rich gas10.3184/096034007X267385 ↗
12. Thermodynamic roles of metallic elements in carburization and metal dusting10.1023/B:OXID.0000025338.74215.31 ↗
13. Carburization of Fe-Cr alloys during oxidation in dry carbon dioxide10.1149/1.2426622 ↗
14. A thermodynamic analysis of the Fe-Cr-C System
15. Carburisation of ferritic Fe-Cr alloys by low carbon activity gases10.1016/j.corsci.2011.05.013 ↗
16. Kubaschewski · 1983
17. Type 304 stainless steel vs flowing CO2 at atmospheric pressure and 1100–1800F10.5006/0010-9312-21.3.84 ↗
18. Corrosion of metals and alloys in mixed gas environments at elevated temperatures10.1007/BF00603609 ↗
19. Scale formation mechanisms of martensitic steels in high CO2/H2O-containing gases simulating oxyfuel environments10.3184/096034009X438185 ↗
20. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe-Cr and Fe-Cr-X alloys10.1007/s11085-010-9215-5 ↗
21. Mechanism of breakaway oxidation of Fe-Cr and Fe-Cr-Ni alloys in dry and wet carbon dioxide
22. Kinetics of breakaway oxidation of Fe-Cr and Fe-Cr-Ni alloys in dry and wet carbon dioxide10.1016/j.corsci.2013.08.008 ↗
23. Effects of cerium and manganese on corrosion of Fe-Cr and Fe-Cr-Ni alloys in Ar-20CO2 gas at 818°C10.1016/j.corsci.2013.06.046 ↗
24. Microstructures of chromia scales grown in CO210.1179/0960340914Z.00000000056 ↗
25. Water vapour effects on corrosion of Fe-Cr and Fe-Cr-Ni alloys containing cerium and manganese in CO2 gas at 818°C10.1016/j.corsci.2014.08.029 ↗
26. Effect of Mn on oxide formation by Fe-Cr and Fe-Cr-Ni alloys in dry and wet CO2 gases at 650°C10.1016/j.corsci.2016.07.014 ↗
27. Effects of silicon on high temperature corrosion of Fe-Cr and Fe-Cr-Ni alloys in carbon dioxide10.1007/s11085-013-9467-y ↗
28. R.A., HSC chemistry version 6.0, Outokumpu Research Oy, Finland 2006.
29. Internal oxidation of binary A-B alloys by two oxidants: double internal oxidation of B in the presence of an external AXm scale10.1007/s11085-014-9523-2 ↗
30. Barin · 1993
31. Carburization of three Fe-19Ni-21Cr-xAl (x=0, 2, 6 at.%) alloys at 900 °C in oxygen-contaminated CH4/H2 atmospheres10.1016/j.corsci.2016.05.008 ↗
32. The thermo-calc databank system: calphad: comput10.1016/0364-5916(85)90021-5 ↗
33. Isothermal phase diagrams of binary alloys and two oxidants10.1007/s11085-009-9186-6 ↗
34. Performance of Cr oxide coatings on 304 stell against metal dusting surf10.1016/j.surfcoat.2013.08.038 ↗
35. Gaskell · 1995
36. The nature of the third-element effect in the oxidation of Fe-xCr-3 at.% Al alloys in 1atm O2 at 1000°C10.1016/j.corsci.2007.06.019 ↗
37. Formation of composite scales containing of oxides of different metals10.1149/1.2430176 ↗
38. Solute diffusion in alpha-iron and gamma-iron10.1007/BF02642019 ↗
39. Refinement of the Fe-C diagram on the basis of results of a thermodynamic analysis and generalization of data for Fe-C and Fe-C-Cr systems10.1007/BF02469111 ↗
40. Determination of diffusion-coefficient of oxygen in gamma-iron from measurements of internal oxidation in Fe-Al alloys10.1007/BF02643898 ↗
41. The formation of two layers in the internal oxidation of binary alloys by two oxidants in the absence of external scales10.1023/A:1018858303891 ↗
42. Ahmed · 2000 · Vol. 99 · 77
43. Effect of magnetic transition on solubility of carbon in bcc Fe and fee Co-Ni alloys10.1007/BF02814843 ↗
44. Diffusion of thorium protactinium and uranium in face-centred cubic thorium10.1016/0022-3115(67)90183-3 ↗
45. Activation-energy of sulfur diffusion in ferromagnetic alpha-iron determined by surface segregation studies10.1016/0036-9748(86)90393-5 ↗
46. Transition from internal to external oxidation for binary-alloys in the presence of an outer scale10.1007/BF01072908 ↗