journal article·2012-02

Ni–NiO composites obtained by controlled oxidation of green compacts

S. Cabanas-Polo, R. Bermejo, B. Ferrari, A.J. Sanchez-Herencia

Corrosion Science· Volume 55
Publisher page

Abstract

Abstract Ni–NiO composites have been obtained by the thermally induced oxidation of metallic green compacts at temperatures between 300 and 450 °C and further sintering. Thermogravimetric studies showed that oxidation process in air follows a quadratic dependence with time for temperatures between 300 and 400 °C allowing the control in the metal to oxide ratio. Microstructural analyses of compacts sintered in inert atmosphere reveal a homogeneous distribution of phases. In the mechanical tests the metal to ceramic ratio variation is evident in the ductile to brittle transition of the fracture, making this method suitable to fabricate compacts with tailored mechanical properties.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Microstructural and mechanical characteristics of in situ metal matrix composites10.1016/S0927-796X(00)00024-3 ↗
3. Control of the mechanical properties of metal–ceramic interfaces through interfacial reactions10.1016/0956-7151(90)90089-Y ↗
4. Microstructure and interface characteristics of B4C, SiC and Al2O3 reinforced Al matrix composites: a comparative study10.1016/S0924-0136(03)00815-X ↗
5. Relation between the oxidation mechanism of nickel, the microstructure and mechanical resistance of NiO films and the nickel purity: I. Oxidation mechanism and microstructure of NiO films10.1016/j.msea.2005.08.225 ↗
6. Relation between the oxidation mechanism of nickel, the microstructure and mechanical resistance of NiO films and the nickel purity. II. Mechanical resistance of NiO films10.1016/j.msea.2005.08.228 ↗
7. An investigation on the wetting of polycrystalline alumina by aluminium10.1016/j.jmatprotec.2007.06.024 ↗
8. M. Kouzeli, L. Weber, C. San Marchi, A. Mortensen, Influence of damage on the tensile behaviour of pure aluminium reinforced with >=40vol. pct alumina particles, Acta Mater. 49 (2001) 3699–3709.10.1016/S1359-6454(01)00279-8 ↗
9. The thermodynamics of spinel interphase formation at diffusion-bonded Ni/Al2O3 interfaces10.1016/0956-7151(91)90160-3 ↗
10. Nickel–alumina interfacial fracture toughness using the thick foil technique10.1016/S0013-7944(01)00094-7 ↗
11. Fracture behaviour of pressureless sintered nickel-reinforced alumina composites10.4028/www.scientific.net/KEM.290.324 ↗
12. Solid-state dye-sensitized solar cell with p-type NiO as a hole collector10.1016/j.solmat.2004.05.010 ↗
13. Mechanical properties of tape cast nickel-based anode materials for solid oxide fuel cells before and after reduction in hydrogen10.1016/j.actamat.2004.08.023 ↗
14. Interfacial toughness of the nickel–nickel oxide system10.1023/A:1022697110703 ↗
15. Origin and development of residual-stresses in the Ni–NiO system – in situ studies at high-temperature by X-ray-diffraction10.1016/0921-5093(93)90504-8 ↗
16. An investigation of oxidation effects on hysteresis heating of nickel particles10.1023/A:1021854026668 ↗
17. On the mechanism of low-temperature oxidation (23–450°C) of polycrystalline nickel10.1149/1.2404360 ↗
18. Oxidation kinetics of small nickel particles10.1063/1.369244 ↗
19. Oxidation kinetics of nickel solar absorber nanoparticles10.1088/0022-3727/34/3/325 ↗
20. The oxidation kinetics of nickel thin films studied by spectroscopic ellipsometry10.1016/j.tsf.2005.11.031 ↗
21. Stress effects in high-temperature oxidation of metals10.1179/imr.1995.40.1.1 ↗
22. Surface behavior of nickel powders in aqueous suspensions10.1021/jp0448954 ↗
23. Forming of nickel compacts by a colloidal filtration route10.1016/j.actamat.2004.10.038 ↗
24. Critical notch-root radius effect in SENB-S fracture toughness testing10.1016/0955-2219(95)00197-2 ↗
25. ENV 843-1 Advanced technical ceramics – monolithic ceramics – mechanical tests at room temperature – Part 1: determination of flexural strength. 1995
26. Oxidation investigation of nickel nanoparticles10.1039/b800672e ↗
27. A study of the passivating oxide layer on fine nickel particles10.1016/0965-9773(94)90078-7 ↗
28. Oxygen transport during the high temperature oxidation of pure nickel10.1007/s11085-005-6560-x ↗
29. On the high-temperature oxidation of nickel10.1016/S0010-938X(02)00085-9 ↗
30. Correlations between growth kinetics and microstructure for scales formed by high-temperature oxidation of pure nickel. II. Growth kinetics10.1023/A:1020102604090 ↗
31. Colloidal processing and sintering of porous percolative Ni-YSZ layers10.1016/j.memsci.2010.01.060 ↗
32. Joining of nickel powder grains by thermal-oxidation10.1016/0167-2738(90)90009-G ↗
33. Transport processes in the oxidation of Ni studied using tracers in growing NiO Scales10.1007/BF00812776 ↗
34. ISO/DIS 23146 Fine ceramics (advanced ceramics, advanced technical ceramics) – test methods for fracture toughness of monolithic ceramics – single-edge V-notch beam (SEVNB) method. 2007
35. The work of fracture and its measurement in metals, ceramics and other materials10.1007/BF00550177 ↗