Abstract
The oxidation mechanism and products of U3Si2 accident tolerant nuclear fuel in flowing air up to 750 °C is reported. Differences between observed and theoretical mass gains for complete oxidation is due to un-oxidised Si that forms nano-crystalline regions of Si. Some Si rich regions are protected by the formation of UO2, which is thermodynamically preferential to oxidise before Si. The UO2 is further kinetically oxidised to form nano-crystalline U3O8. The nanostructure formed, accompanied by large volumetric expansions during oxidation produces pulverisation of fragments into powder, which may have serious consequences for fuel integrity if exposed to oxidative atmospheres.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Nuclear materials and radiation effects · Radioactive element chemistry and processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Material selection for accident tolerant fuel cladding
2. Uranium silicide pellet fabrication by powder metallurgy for accident tolerant fuel evaluation and irradiation10.1016/j.jnucmat.2015.06.027 ↗
3. Thermophysical properties of U3Si2 to 1773K10.1016/j.jnucmat.2015.04.031 ↗
4. Temperature-dependent swelling in irradiated U3Si fuel elements10.1016/0022-3115(70)90159-5 ↗
5. Effect of swelling on thermal conductivity and postirradiation densification of U3Si10.1111/j.1151-2916.1972.tb11271.x ↗
6. Oxidation behavior of U-Si compounds in air from 25 to 1000 C10.1016/j.jnucmat.2016.12.016 ↗
7. Oxidation of accident tolerant fuel candidates
8. The stability of SiO solid and gas10.1021/j150514a015 ↗
9. Oxidation of UC: an in situ high temperature environmental scanning electron microscopy study10.1016/j.jnucmat.2017.07.016 ↗
10. Uranium carbide oxidation from 873 K to 1173 K10.1016/j.corsci.2019.01.044 ↗
11. Mechanism and kinetics of oxidation of ZrN ceramics10.1111/jace.13575 ↗
12. Processing and properties of ZrC, ZrN and ZrCN ceramics: a review
13. Atomistic level study of Ce3Si2 oxidation as an accident tolerant nuclear fuel surrogate10.1016/j.corsci.2019.108332 ↗
14. Structure and phase composition of silicon monoxide10.1134/S106378261213009X ↗
15. Crystal chemical studies of the 5f-series of elements. I. New structure types10.1107/S0365110X48000703 ↗
16. Neutron diffraction investigation of U3O810.1107/S0365110X6400158X ↗
17. Williams · 2009 · 257
18. Crystallization of amorphous silicon films10.1002/pssa.2210480207 ↗
19. Softening and melting of SiO2, an important parameter for reactions with quartz in Si production BT - advances in molten slags, fluxes, and salts
20. The effect of aluminum additions on the oxidation resistance of U3Si210.1016/j.jnucmat.2017.02.045 ↗
21. Reducibility of oxides and sulphides in metallurgical processes
22. Volatile fission product behaviour during thermal annealing of irradiated UO2 fuel oxidised up to U3O810.1016/j.jnucmat.2007.03.174 ↗
23. Oxidation of accident tolerant fuel candidates
24. Crystallization of fine silicon particles from silicon monoxide10.1016/S0022-0248(01)02244-8 ↗
25. Photoluminescence from silicon nanoparticles prepared from bulk amorphous silicon monoxide by the disproportionation reaction10.1063/1.2043246 ↗
26. Preparation of fine silicon particles from amorphous silicon monoxide by the disproportionation reaction10.1016/S0022-0248(01)01202-7 ↗