journal article·2018-07

The study on the corrosion mechanism of protective ternary Zn Fe Mo alloy coatings deposited on carbon steel in 0.5 mol dm–3 NaCl solution

J. Winiarski, W. Tylus, A. Lutz, I. De Graeve, B. Szczygieł

Corrosion Science· Volume 138
Publisher page

Abstract

Abstract The passive layer on Zn Fe Mo coating (7.6 at.% Fe, 1.6 at.% Mo) became damaged in 0.5 M NaCl solution, as shown in ionic current density maps that were observed during 10 h of exposure. The ZnO and Zn(OH)2 slowly transformed into Zn5(OH)6(CO3)2 and Zn5(OH)8Cl2·H2O. At the same time, MoO2 transformed to MoO3 and MoO(OH)2. The barrier properties of the layer of corrosion products deteriorated so the charge transfer resistance decreased from 13 to 7.4 kΩ cm2 and the double layer capacitance increased from 4.5 to 62 μF cm–2 after 0.5 h and 10 h exposure, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Electrodeposition and Electroless Coatings · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Corrosion resistance of Zn–Co–Fe alloy coatings on high strength steel10.1016/j.surfcoat.2008.11.019 ↗
2. EIS and XPS investigations on the corrosion mechanism of ternary Zn–Co–Mo alloy coatings in NaCl solution10.1016/j.apsusc.2015.12.183 ↗
3. MoO42− as a soluble inhibitor for zn in neutral and alkaline solutions10.1016/j.corsci.2015.05.005 ↗
4. Self-repairing oxides to protect zinc: review, discussion and prospects10.1016/j.corsci.2013.01.011 ↗
5. The effect of pH of plating bath on electrodeposition and properties of protective ternary Zn–Fe–Mo alloy coatings10.1016/j.surfcoat.2016.04.073 ↗
6. The influence of molybdenum on the electrodeposition and properties of ternary Zn–Fe–Mo alloy coatings10.1016/j.electacta.2016.03.027 ↗
7. Structure and growth of oxides on polycrystalline nickel surfaces10.1002/sia.2565 ↗
8. Tougard · 2010
9. Calculations of electron inelastic mean free paths. V. Data for 14 organic compounds over the 50–2000 eV range10.1002/sia.740210302 ↗
10. 1990 · vol. 1 · 244
11. The influence of iron and molybdenum on the corrosion process of protective ternary Zn–Fe–Mo alloy coatings in chloride solution
12. The delamination of polymeric coatings from electrogalvanised steel – a mechanistic approach.: Part 1: delamination from a defect with intact zinc layer10.1016/S0010-938X(00)00047-0 ↗
13. Tylus · 2015
14. An ESCA method for determining the oxide thickness on aluminium alloys10.1002/sia.740150109 ↗
15. X-ray photoelectron spectroscopic chemical state quantification of mixed nickel metal, oxide and hydroxide systems10.1002/sia.3026 ↗
16. Theoretical and experimental study of the electronic structures of MoO3 and MoO210.1021/jp9093172 ↗
17. Generalized molybdenum oxide surface chemical state XPS determination via informed amorphous sample model10.1016/j.apsusc.2014.11.077 ↗
18. ESCA studies of MoO2 and MoO310.1002/sia.740130103 ↗
19. XPS study of passive films formed on molybdenum-implanted austenitic stainless steels10.1002/sia.740190175 ↗
20. Cation profiling of passive films on stainless steel formed in sulphuric and acetic acid by deconvolution of angle-resolved X-ray photoelectron spectra10.1016/j.apsusc.2013.07.158 ↗
21. Angle-resolved XPS analysis of molybdenum and tungsten in passive films on stainless steel PVD alloys10.1002/sia.1268 ↗
22. The nature and role of passive films in controlling the corrosion resistance of MoSi2-based nanocomposite coatings10.1039/c3ta11813d ↗
23. The influence of molybdenum on the corrosion resistance of ternary Zn–Co–Mo alloy coatings deposited from citrate–sulphate bath10.1016/j.corsci.2014.11.037 ↗
24. Influence of molybdenum on properties of Zn–Ni and Zn–Co alloy coatings10.1016/j.surfcoat.2009.09.042 ↗
25. Identification of Mo(V) commonly observed in passive films formed on stainless steels10.1002/(SICI)1096-9918(199802)26:2<155::AID-SIA353>3.0.CO;2-B ↗
26. Preparation and characterization of zinc hydroxide carbonate and porous zinc oxide particles10.1016/j.jeurceramsoc.2008.05.003 ↗
27. Simonkolleite nano-platelets: synthesis and temperature effect on hydrogen gas sensing properties10.1016/j.apsusc.2012.04.073 ↗
28. Hydrogen bonding in solid hydroxides with strongly polarising metal ions, β-Be(OH)2 and ε-Zn(OH)210.1016/S1386-1425(98)00017-1 ↗
29. Synthesis and vibrational spectroscopic characterisation of synthetic hydrozincite and smithsonite10.1016/j.poly.2007.07.002 ↗
30. Leygraf · 2016
31. Initial NaCl-particle induced atmospheric corrosion of zinc – effect of CO2 and SO210.1016/j.corsci.2007.06.005 ↗
32. Pourbaix · 1974
33. Corrosion and passivation behaviors of molybdenum in aqueous solutions of different pH10.1016/S0013-4686(98)00180-7 ↗
34. On the anodic dissolution of molybdenum in acidic and alkaline electrolytes10.1016/S0022-0728(72)80100-1 ↗
35. SVET study of the corrosion protection of electrodeposited zn and zn-Co-Fe alloy coated steels10.1002/maco.200804162 ↗
36. The localized breakdown and repair of passive surfaces during pitting10.1016/0010-938X(89)90038-3 ↗
37. Cut-edge corrosion study on painted aluminum rich metallic coated steel by scanning vibrating electrode and micro-potentiometric techniques10.1016/j.electacta.2011.11.110 ↗
38. Scanning Kelvin force microscopy study at the cut-edge of aluminum rich metal coated steel10.1002/maco.201307145 ↗
39. Study of local Na+ and Cl− distributions during the cut-edge corrosion of aluminum rich metal-coated steel by scanning vibrating electrode and micro-potentiometric techniques10.1016/j.electacta.2013.03.186 ↗
40. Study of the electrochemical behaviour of aluminized steel10.1016/j.surfcoat.2014.06.064 ↗
41. Measurements of corrosion at defects in painted zinc and zinc alloy coated steels using current density mapping10.5006/1.3292109 ↗
42. Use of the scanning vibrating electrode technique for detecting defects in ion vapor-deposited aluminum on steel10.5006/1.3583835 ↗
43. A shape recovery polymer coating for the corrosion protection of metallic surfaces10.1021/am505621x ↗
44. Dissolution characteristics of duplex stainless steels in acidic environments10.1016/S0010-938X(98)00053-5 ↗
45. SVET, SKP and EIS study of the corrosion behaviour of high strength Al and Al–Li alloys used in aircraft fabrication10.1016/j.corsci.2014.03.001 ↗
46. A multiple-action self-healing coating10.3389/fmats.2015.00073 ↗
47. On the corrosion resistance of porous electroplated zinc coatings in different corrosive media10.1016/j.corsci.2010.02.024 ↗
48. Dielectric properties of materials showing Constant-Phase-Element (CPE) impedance response10.1149/2.033306jes ↗
49. Evolution of corrosion resistance and passive film properties of Ni–Mo alloy coatings during exposure to 0.5 M NaCl solution10.1016/j.surfcoat.2017.03.043 ↗
50. Determination of effective capacitance and film thickness from constant-phase-element parameters10.1016/j.electacta.2009.10.065 ↗