Anodizing of Al-Ti alloys, containing 3, 12, 15, 30 and 45at.%Ti, is examined at 5mAcm -2 in 1moldm -3 sulphuric acid at 293K. Porous films are formed up to 15at.%Ti, with titanium increasing the anodizing voltage and pore size. In contrast, a barrier-type film is formed at 30at.%Ti, with a finely porous outer region, while at 45at.%Ti, barrier-type film growth is accompanied by oxygen generation. Ti:Al atomic ratios in the films are similar to those in the respective alloys. Reduced levels of sulphur occur in barrier-type films compared with porous films. © 2011 Elsevier Ltd.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Anodic Oxide Films and Nanostructures · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Passivity and its breakdown on sputter-deposited amorphous Al–Ti alloys in a neutral aqueous solution with Cl-10.1016/0010-938X(90)90138-U ↗
2. S.K. Lazarouk, A.A. Leshok, Nanoporous anodic oxide on aluminum–titanium alloys, in: Proceedings of Nanomeeting 2003: Physics, Chemistry and Application of Nanostructures, Minsk, Belarus, 20–23 May, 2003, pp. 249–252.10.1142/9789812796738_0058 ↗
3. Recent advances in photocurrent spectroscopy of passive films10.1016/S0013-4686(02)00842-3 ↗
4. Composition and structure of anodic oxide films on titanium–aluminium alloys by fast electron reflection diffraction, Rutherford backscattering and secondary neutral particle mass spectrometry10.1023/A:1024113613516 ↗
5. Anodic oxidation behaviour of Al–Ti alloys in acidic media10.1023/A:1012746926209 ↗
6. Formation of barrier-type anodic films on sputtering-deposited Al–Ti alloys10.1016/j.corsci.2010.07.022 ↗
7. Algortihms for the rapid simulation of Rutherford backscattering spectra10.1016/0168-583X(85)90762-1 ↗
8. Main features of magnetron sputtered aluminium-transition metal alloy coatings10.1016/S0257-8972(01)01197-5 ↗
9. Migration of sulphate ions in anodic alumina10.1016/S0013-4686(99)00397-7 ↗
10. Breakdown and efficiency of anodic oxide growth on titanium10.1149/1.2131616 ↗
11. Evidence of oxygen bubbles formed within anodic films on aluminium–copper alloys10.1080/01418619708214206 ↗
12. The behaviour of iron during anodic oxidation of sputter-deposited Al–Fe alloys10.1016/S0010-938X(00)00151-7 ↗
13. Lj.D. Arsov, C. Kormann, W. Plieth, Electrochemical synthesis and in situ Raman spectroscopy of thin films on titanium dioxide. J. Raman Spectrosc. 22 (1991) 573–575.
14. Nanoscale enrichments of substrate elements in the growth of thin oxide films10.1016/S0010-938X(97)89339-0 ↗
15. Study by nuclear microanalysis and O18 tracer techniques of the oxygen transport processes and the growth laws for porous anodic oxide layers on aluminum10.1149/1.2403563 ↗
16. An O18 study of field-assisted pore formation in compact anodic oxide films on aluminium10.1149/1.2133446 ↗
17. A flow model of porous anodic film growth on aluminium10.1016/j.electacta.2006.05.054 ↗
18. Volume expansion factor and growth efficiency of anodic alumina formed in sulphuric acid10.1149/1.3578028 ↗
19. A mechanism for the formation of porous anodic oxide films on aluminium10.1016/0022-3697(59)90199-4 ↗
20. S. Ono, K. Takeda, N. Masuko, Cell dimension of porous anodic alumina films, in: 2nd Int. Symp. on Aluminium Surface Science and Technology (Manchester U.K.), ATB Metallurgie, 2000, pp. 398–403.
21. Porous anodic film formation on aluminium10.1038/290230a0 ↗
22. Tracer studies relating to alloying element behaviour in porous anodic alumina formed in phosphoric acid10.1016/j.electacta.2010.01.038 ↗
23. The use of Rutherford Backscattering to study the behavior of ion-implanted atoms during anodic oxidation of aluminum: Ar, Kr, Xe, K, Rb, Cs, Cl, Br, and l10.1149/1.2403637 ↗
24. The anodic oxidation of valve metals – I. Determination of ionic transport numbers by α-spectrometry10.1016/0013-4686(86)80148-7 ↗
25. The morphology and mechansim of porous anodic film formation on aluminum
26. Self-organized porous and nanotubular oxide layers on TiAl alloys10.1016/j.elecom.2007.07.013 ↗
27. Transition from nanopores to nanotubes: self-ordered anodic oxide structures on titanium aluminides10.1021/cm8004024 ↗