Abstract

Abstract The corrosion effects on the tensile and stress relaxation behavior of an extruded AZ31 magnesium alloy subjected to immersion and salt-spray environments have been investigated. Specimens were simultaneously corroded and stress relaxed in a 3.5 wt.% NaCl solution and then put under a tensile test to failure to determine the stress–strain response over a 60 h test matrix. The AZ31 magnesium alloy shows an evident relaxation in 3.5 wt.% NaCl at room temperature. According to optical and scanning electron microscopy investigations, the fracture surfaces for the immersion environment show a high sensitivity to stress corrosion cracking.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. E. Ghali, Magnesium and magnesium alloys, in: Uhligs Corros. Handb., 2000, p. 793.
2. Effects of extrusion ratio on the microstructure and mechanical properties of AZ31 Mg alloy10.1016/j.jmatprotec.2006.08.012 ↗
3. Microstructural effects of AZ31 magnesium alloy on its tensile deformation and failure behaviors10.1016/j.msea.2005.12.003 ↗
4. Corrosion behaviour of magnesium/aluminium alloys in 3.5wt.% NaCl10.1016/j.corsci.2007.11.005 ↗
5. Stress corrosion cracking behavior of the wrought magnesium alloy AZ31 under controlled cathodic potentials10.1016/j.msea.2011.10.052 ↗
6. The electrochemical corrosion of pure magnesium in 1N NaCl10.1016/S0010-938X(96)00172-2 ↗
7. Atmospheric corrosion of magnesium alloys AZ31 and AZ61 under continuous condensation conditions10.1016/j.corsci.2011.02.003 ↗
8. Corrosion relationships as a function of time and surface roughness on a structural AE44 magnesium alloy10.1016/j.corsci.2010.01.018 ↗
9. Fatigue behaviour of bare and pre-corroded magnesium alloy AZ3110.1016/j.matdes.2010.04.031 ↗
10. Corrosion mechanisms of magnesium alloys10.1002/(SICI)1527-2648(199909)1:1<11::AID-ADEM11>3.0.CO;2-N ↗
11. Influence of texture on corrosion rate of AZ31 Mg alloy in 3.5wt.% NaCl10.1016/j.matdes.2011.04.031 ↗
12. Corrosion behaviour of stressed magnesium alloys10.1016/S0010-938X(01)00101-9 ↗
13. Microstructure evolution and deformation features of AZ31 Mg-alloy during creep10.1016/j.msea.2005.10.015 ↗
14. Mechanoelectrochemical behavior of pure magnesium and magnesium alloys stressed in aqueous solutions10.1023/A:1011399723559 ↗
15. Corrosion stress relaxation in pure magnesium and die-cast Mg alloys
16. Magnesium and its alloys applications in automotive industry10.1007/s00170-007-1279-2 ↗
17. Understanding magnesium corrosion—a framework for improved alloy performance10.1002/adem.200310405 ↗
18. Corrosion resistance of magnesium alloys
19. Quantification of corrosion mechanisms under immersion and salt-spray environments on an extruded AZ31 magnesium alloy10.1016/j.corsci.2011.12.008 ↗
20. Structure–property quantification of corrosion pitting under immersion and salt-spray environments on an extruded AZ61 magnesium alloy10.1016/j.corsci.2010.12.025 ↗
21. ASTM B117-07a. Standard Practice for Operating Salt Spray (Fog) Apparatus, vol. 03.02, 2007.
22. ASTM G31-72. Standard Practice for Laboratory Immersion Corrosion Testing of Metals, vol. 03.02, 2004.
23. Accelerated corrosion tests for aerospace materials: current limitations and future trends10.1108/00022669910270718 ↗
24. Accelerated corrosion tests in the automotive industry: a comparison of the performance towards cosmetic corrosion10.1002/maco.200804168 ↗
25. The corrosion performance of magnesium alloy AM-SC1 in automotive engine block applications10.1007/s11837-005-0097-y ↗
26. Pre-exposure embrittlement and stress corrosion failure in AlZnMg alloys10.1016/0010-938X(76)90065-2 ↗
27. Stress corrosion cracking of magnesium alloys10.1002/adem.200900287 ↗
28. Characterisation of stress corrosion cracking (SCC) of Mg–Al alloys10.1016/j.msea.2007.11.064 ↗
29. Transgranular see in Mg–Al alloys10.1016/S0010-938X(71)80020-3 ↗
30. Stress corrosion cracking of rapidly solidified magnesium–aluminum alloys10.1016/0010-938X(93)90090-4 ↗
31. Stress corrosion cracking of a recent rare-earth containing magnesium alloy, EV31A, and a common Al-containing alloy, AZ91E10.1016/j.corsci.2013.01.001 ↗
32. Stress corrosion cracking of AZ61 magnesium alloy friction stir weldments in ASTM D1384 solution10.1179/174327808X315704 ↗
33. Stress corrosion cracking of gas-tungsten arc welds in continuous-cast AZ31Mg alloy sheet10.1016/j.corsci.2009.05.037 ↗
34. In situ observation of crack initiation and propagation of the charged magnesium alloy under cyclic wet–dry conditions10.1016/j.corsci.2008.05.013 ↗
35. Stress corrosion cracking of new Mg–Zn–Mn wrought alloys containing Si10.1016/j.corsci.2008.02.012 ↗
36. States and transport of hydrogen in the corrosion process of an AZ91 magnesium alloy in aqueous solution10.1016/j.corsci.2008.01.028 ↗
37. Role of chlorides on pitting and hydrogen embrittlement of Mg–Mn wrought alloy10.1016/j.corsci.2013.05.030 ↗
38. Stress relaxation in selected magnesium alloys10.4028/www.scientific.net/KEM.345-346.1613 ↗
39. Internal stress and thermally activated dislocation motion in an AZ63 magnesium alloy10.1016/j.matchemphys.2011.08.045 ↗
40. Metals Handbooks vol. 2: Properties and Selection, 10th ed., ASM International, [S.l.], 1990.
41. Stress relaxation in AX41 magnesium alloy studied at elevated temperatures10.1002/adem.200700018 ↗
42. Surface plasticity modification using electrolytic etching10.1016/S0257-8972(05)80037-4 ↗
43. S. Matsuoka, M. Oguri, T. Murai, Mechanical properties and extrudability of magnesium alloys, in: Proc. 41st Gen. Meet., 2004, pp. 215–216.10.1299/jsmehs.2004.41.215 ↗
44. Failure Analysis, in: Met. Handb., ASM International, 1997.
45. Pitting-induced hydrogen embrittlement of magnesium–aluminium alloy10.1016/j.matdes.2012.06.007 ↗
46. Propagation of stress-corrosion cracking in a magnesium-based alloy as determined by several techniques
47. Environmentally-induced cracking of magnesium10.1016/0010-938X(84)90017-9 ↗