Corrosion of titanium alloys in pressurised water at 300 °C: Kinetics and modelling

Sabrina Selva, Quentin Bignon, Amandine Raynal, Frantz Martin, Quentin Auzoux, Gilles Renou, Michel Tabarant, Frédéric Miserque, Laurence Latu-Romain, Yves Wouters

Corrosion Science· Volume 190

Abstract

Abstract The corrosion of titanium alloys in primary water at 300 °C led to a global weight gain due to oxidation and surface precipitation, despite some dissolution. A model was proposed, taking into account the weight contribution of each oxide type to the global mass evolution with exposure time. Based on this model, on mass variation and GD-OES results, a corrosion rate ranging between 2 and 6.6 μm.year-1 at 300 °C for all tested materials was estimated. Due to the simultaneous corrosion of the used stainless steel reactors, a protective ilmenite layer finally precipitated at the surface of the samples.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. M. Zucchetti, D. Boerman, and G. Piatti, Characterisation of a titanium alloy for nuclear fusion applications, p. 17.
2. Oxide formation on titanium alloys in primary water of nuclear pressurised water reactor10.1016/j.corsci.2019.01.020 ↗
3. Study of corrosion kinetics and microstructure of α-phase pure titanium tube in environment 300°C and 8.6MPa water10.1016/j.corsci.2019.108217 ↗
4. General corrosion properties of titanium based alloys for the fuel claddings in the supercritical water-cooled reactor
5. Corrosion of Zirconium-Base Alloys—An Overview10.1520/STP35573S ↗
6. Influence of light ion irradiation of the oxide layer on the oxidation rate of Zircaloy-410.1016/j.corsci.2015.05.045 ↗
7. The corrosion of the alloy M5: an overview
8. « The history of the Point Defect Model for the passive state: a brief review of film growth aspects »10.1016/j.electacta.2010.11.005 ↗
9. « corrosion behavior of SUS 304 stainless steel in high temperature and high pressure water adding metal ions »10.3323/jcorr1991.47.275 ↗
10. Machet · 2004
11. « Evaluation of galvanic corrosion behaviour of SA-508 low alloy steel and type 309 L stainless steel cladding of reactor pressure vessel under simulated primary water environment »10.5516/NET.07.2011.054 ↗
12. Oxydation et prise d’hydrogène d’alliages de titane en milieu primaire de réacteur à eau pressurisée: mécanismes, cinétiques et effet sur le comportement mécanique
13. The ionization constant of water over wide ranges of temperature and density10.1063/1.1928231 ↗
14. Slow strain rate stress corrosion tests on A508-III and A533B steel in de-ionized and PWR water at 56K10.1016/0010-938X(85)90004-6 ↗
15. « simulation of porous magnetite deposits on steam generator tubes in circulating water at 270 °C »
16. « A detailed TEM and SEM study of Ni-base alloys oxide scales formed in primary conditions of pressurized water reactor
17. Automated crystal orientation and phase mapping in TEM10.1016/j.matchar.2014.08.010 ↗
18. Formulation for XPS spectral change of oxides by ion bombardment as a function of sputtering time10.1016/j.susc.2004.03.002 ↗
19. Ti(IV) hydrolysis constants derived from rutile solubility measurements made from 100 to 300°C10.1016/S0883-2927(00)00081-0 ↗
20. Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.002 ↗
21. Transitions from Parabolic to Linear Kinetics in Scaling of Metals10.1149/1.2427495 ↗
22. Loi d’oxydation du cérium métallique. Généralisation à d’autres métaux