Abstract This study investigates the flowback water impacts on the corrosion of mild steel pipelines used to transport the saline wastewater generated during fracturing of the Bakken shale. The uniform corrosion rates were high under acidic conditions compared to those under neutral and alkaline conditions. The pitting attack on the flowback water pipelines was 100-fold and 10-fold higher for acidic and alkaline conditions, respectively, than those for the neutral conditions. The corrosion deposits on the mild steel were characterized by a large specific surface area and high reactivity. These results suggest that the flowback water pipelines become a potential source of contaminants that threaten agricultural land and water resources.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Groundwater flow and contamination studies · Hydrogen embrittlement and corrosion behaviors in metals · Water Treatment and Disinfection

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Gadhamshetty · 2015
2. Potential water resource impacts of hydraulic fracturing from unconventional oil production in the Bakken shale10.1016/j.watres.2016.11.006 ↗
3. Comparison of water use for hydraulic fracturing for unconventional oil and gas versus conventional oil10.1021/es502506v ↗
4. Brine spills associated with unconventional oil development in North Dakota10.1021/acs.est.5b06349 ↗
5. Jacobson · 2015
6. EERC · 2015
7. Jones · 1992
8. Cyclic voltammetric studies of carbon steel corrosion in chloride-formation water solution and effect of some inorganic salts10.1016/j.ejpe.2012.02.005 ↗
9. NACE · 2016
10. Effect of pH and chloride on the micro-mechanism of pitting corrosion for high strength pipeline steel in aerated NaCl solutions10.1016/j.apsusc.2015.05.053 ↗
11. Role of chloride ion in passivity breakdown on iron and nickel10.1149/1.2048247 ↗
12. Chloride threshold level for corrosion of steel in concrete10.1016/j.corsci.2007.05.007 ↗
13. Handling produced water from hydraulic fracturing10.2118/0212-0022-OGF ↗
14. Stepan · 2010
15. Kurz · 2016
16. North Dakota Department of Health · 2015
17. Microbial communities in flowback water impoundments from hydraulic fracturing for recovery of shale gas10.1111/1574-6941.12183 ↗
18. Henthorn, M., 1972. Localized Corrosion—Cause of Metal Failure. ASTM STP 516 ASTM.10.1520/STP516-EB ↗
19. Influence of chloride and sulfate on formation of akaganeite and schwertmannite through ferrous biooxidation by acidithiobacillus ferrooxidans cells10.1021/es801646j ↗
20. Strontium concentrations in corrosion products from residential drinking water distribution systems10.1021/es4000609 ↗
21. Competitive ligand exchange on akaganéite surfaces enriches bulk chloride loadings10.1016/j.jcis.2012.03.006 ↗
22. Adsorptive characteristics of akaganeite and its environmental applications: a review10.1080/09593330.2012.701239 ↗
23. Novel cationic surfactants for corrosion inhibition of carbon steel pipelines in oil and gas wells applications10.1016/j.molliq.2015.11.047 ↗
24. The effect of atomic hydrogen on the anodic dissolution of iron in a sulfate electrolyte studied with impedance spectroscopy10.1134/S0033173208060039 ↗
25. Pitting corrosion of metals a review of the critical factors10.1149/1.1838615 ↗
26. Mechanism and equivalent circuits in electrochemical impedance spectroscopy10.1016/j.electacta.2011.01.067 ↗
27. Negative resistances and inductances in equivalent circuits for adsorption-reaction kinetics10.1149/1.3555059 ↗
28. Orazem · 2011
29. Effects of Ag and Cu ions on the microbial corrosion of 316L stainless steel in the presence of Desulfovibrio sp10.1016/j.bioelechem.2016.03.008 ↗
30. Shaw · 2003
31. Environmental factors affecting the critical potential for pitting in 18–8 stainless steel10.1149/1.2423801 ↗
32. Jones · 1992 · 455
33. Environmental signatures and effects of an oil and gas wastewater spill in the Williston Basin, North Dakota10.1016/j.scitotenv.2016.11.157 ↗
34. Influence of water hardness and sulfate on the acute toxicity of chloride to sensitive freshwater invertebrates10.1002/etc.454 ↗
35. Potential water resource impacts of hydraulic fracturing from unconventional oil production in the Bakken shale10.1016/j.watres.2016.11.006 ↗
36. Galvanic corrosion
37. Synthesis of single-crystalline hollow β-FeOOH nanorods via a controlled incomplete-reaction course10.1007/s11051-005-9054-5 ↗
38. Snow · 2010
39. Egerton · 2005
40. Corrosion of cannon 75/27, model 1911 Déport, from the collection of the military museum in belgrade
41. Corrosion of an archaeological find from the Roman period in Serbia
42. Environmental conditions for akaganeite formation in marine atmosphere mild steel corrosion products and its characterization10.5006/1672 ↗
43. The corrosion of excavated archaeological iron with details on weeping and akaganeite10.1179/sic.1999.44.4.217 ↗
44. The internal structure of colloidal crystals of β-FeOOH and remarks on their assemblies in schiller layers10.1021/j100816a001 ↗
45. Synthesis and anion exchange of tunnel structure akaganeite10.1021/cm010310w ↗
46. On the formation of β-FeOOH (akaganéite) in chloride-containing environments10.1016/j.corsci.2006.06.003 ↗
47. Role of akaganeite (β-FeOOH) in the growth of hematite (α-Fe2O3) in an inorganic silica hydrogel10.1021/acs.cgd.5b00475 ↗
48. Orbital detection and implications of akaganeite on Mars10.1016/j.icarus.2015.01.020 ↗
49. The interfacial behavior between biochar and soil minerals and its effect on biochar stability10.1021/acs.est.5b03656 ↗
50. Coordination of Sr and Mg in calcite and aragonite10.1180/minmag.2007.071.5.539 ↗
51. A study of the interaction of strontium ions in aqueous solution with the surfaces of calcite and kaolinite10.1016/S0016-7037(98)00072-6 ↗
52. Mode of incorporation of Sr2+ in calcite: determination by X-ray absorption spectroscopy10.1016/0016-7037(92)90222-5 ↗
53. Study of the scavenging behavior and structural changes accompanying the interaction of aqueous Pb2+ and Sr2+ ions with calcite10.2343/geochemj.39.317 ↗
54. Harbison · 2015