Improving the corrosion behaviour of powder metallurgical 316L alloy by prepassivation in 20% nitric acid
Source abstract
Abstract
The electrochemical improvement of PM 316L stainless steels by pre-alloyed powder prepassivation in 20% nitric acid in comparison with as-received specimens has been studied in this work. For comparison purposes a simultaneous study was carried out on similar composition wrought AISI 316L steels. Corrosion resistance was studied using evolution of the corrosion potential vs. time, anodic polarisations curves and Zero Resistance Ammeter technique. Reductions of the corrosion rate (icorr) were observed in prepassivated specimens in neutral chloride media. Crevice resistance was higher for prepassivated specimens and for higher densities and annealing as post-heat treatments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. A study of the influence of nitric acid concentration on the corrosion resistance of sintered austenitic stainless steel10.1016/0010-938X(96)00039-X ↗
2. Corrosion behaviour of sintered austenitic stainless steel filters in sulphuric acid solutions10.1179/000705988798270992 ↗
3. Sintered austenitic stainless steels: corrosion behaviour in sulphate and chloride media10.1002/maco.19940450705 ↗
4. Corrosion behaviour of AISI 304L and 316L stainless steels prepared by powder metallurgy in the presence of sulphuric and phosphoric acid10.1016/S0010-938X(98)00047-X ↗
5. Corrosion behavior of powder metallurgical stainless steels in urban and marine environments10.3989/revmetalm.2006.v42.i3.17 ↗
6. Pitting corrosion behaviour of PM austenitic stainless steels sintered in nitrogen–hydrogen atmosphere10.1016/j.corsci.2006.10.009 ↗
7. Electrochemical reactivation methods applied to PM austenitic stainless steels sintered in nitrogen–hydrogen atmosphere10.1016/j.corsci.2007.10.001 ↗
8. Effect of admixing Ni and Cu powders on property of sintered 316L alloy
9. B. Vetayanugul, O. Coovattanachai, R. Krataitong, R. Tongsri, P. Burke, Effect of Sintering Temperature on Mechanical Properties of Parts from 316L Stainless Steel Powders, 28th Congress on Science and Technology of Thailand, Bangkok, 2002, pp. 637–641.
10. German · 1998
11. Corrosion mechanisms of an AlSl type 316L sintered stainless steel in sodium chloride solution10.1002/maco.19910420804 ↗
12. The corrosion behaviour of AISI 304L and 316L stainless steels prepared by powder metallurgy in the presence of organic acids10.1016/S0010-938X(97)86097-0 ↗
13. Mechanical properties and pitting corrosion behaviour of 316L stainless steel parts obtained by a modified metal injection moulding process10.1016/S0924-0136(03)00402-3 ↗
14. The environmental behavior of SAE 304L stainless steel sintered in the presence of a copper base additive10.1016/S0921-5093(96)10543-8 ↗
15. Corrosion resistance of alloyed powder metallurgy austenitic stainless steels in acid solutions10.1179/bcj.1996.31.4.295 ↗
16. P.K. Samal, J.B. Terrell, Corrosion resistance of boron containing P/M 316L, Advances in Powder Metallurgy and Particulate Materials 10 (2000) (7–17)–(7–31).
17. Effect of MnS powder addition and sintering temperature on the corrosion resistance of sintered 3030LSC stainless steels10.1016/S0010-938X(02)00181-6 ↗
18. Atmosphere influence in sintering process of stainless steels matrix composites reinforced with hard particles10.1016/S0266-3538(02)00179-3 ↗
19. Electrochemical behavior of sintered oxide dispersion strengthened stainless steels10.1016/S0010-938X(03)00144-6 ↗
20. Aqueous corrosion behaviour of sintered stainless steels manufactured from mixes of gas atomized and water atomized powders10.1016/j.corsci.2009.04.017 ↗
21. Characteristic of the porous 316 stainless steel for the friction element of prosthetic joint10.1016/j.wear.2007.01.119 ↗
22. Corrosion of 304 stainless steels exposed to nitric acid-chloride environments10.1016/S0010-938X(97)00092-9 ↗
23. Klar · 2007
24. Scully · 2003
25. Sedricks · 1998