Role of temper conditions on the hydrogen embrittlement behavior of AA 7010
Source abstract
Abstract
Abstract This paper reports an attempt to understand the influence of temper conditions on the hydrogen embrittlement (HE) behaviour of AA 7010. A novel heat treatment technique reported in this paper exhibited crack growth rates on par with over aged temper in 3.5 wt.% NaCl under freely corroding conditions (@OCP). Copper enrichment on the grain boundary precipitates curtailed the hydrogen evolution and enhanced the alloy resistance to hydrogen embrittlement (@OCP) for both the temper conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Aluminum Alloy Microstructure Properties · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Environmentally-assisted cracking of engineering materials—an insight10.1515/CORRREV.2009.27.S1.147 ↗
2. Molybdate inhibition of environmental fatigue crack propagation in Al – Zn – Mg – Cu10.1016/j.ijfatigue.2009.01.016 ↗
3. Effect of corrosion severity on fatigue evolution in Al–Zn–Mg–Cu10.1016/j.corsci.2009.10.006 ↗
4. Atmospheric stress corrosion cracking of a superplastic 7475
5. Influence of multistep aging on the stress corrosion cracking behavior of aluminum alloy 701010.5006/1.3287709 ↗
6. Correlations between intergranular stress corrosion cracking, grain-boundary microchemistry, and grain-boundary electrochemistry for Al-Zn-Mg-Cu alloys10.1016/j.corsci.2010.08.024 ↗
7. Some effects of alloy composition on stress corrosion cracking in Al–Zn–Mg–Cu alloys10.1016/j.corsci.2015.05.016 ↗
8. Effect of heat treatments on the tensile strength and SCC-resistance of AA7050 in an alkaline saline solution10.1016/j.corsci.2005.11.009 ↗
9. Key microstructural features responsible for improved stress corrosion cracking resistance and weldability in 7xxx series Al alloys containing micro/trace alloying additions10.4028/www.scientific.net/MSF.519-521.315 ↗
10. Effect of Cu content and aging conditions on pitting corrosion damage of 7xxx series
11. Aluminium alloys—a century of age hardening
12. Influence of high-temperature pre-precipitation on local corrosion behaviors of Al-Zn-Mg alloy10.1016/j.scriptamat.2006.09.028 ↗
13. Improvements in mechanical and stress corrosion cracking properties in Al-alloy 7075 via retrogression and reaging10.1016/j.msea.2007.08.025 ↗
14. Influence of retrogression and reaging on fracture toughness of 7010 aluminium alloy10.1179/026708303225008383 ↗
15. Improvements in strength and stress corrosion cracking properties in aluminum alloy 7075 via low-temperature retrogression and re-aging heat treatments10.5006/1.3277583 ↗
16. Retrogression and reaging and the role of dislocations in the stress corrosion of 7000-type aluminum alloys10.1007/BF02650294 ↗
17. The effect of RRA on the strength and SCC resistance on AA7050 and AA7150 aluminium alloys10.1016/j.msea.2004.02.052 ↗
18. Evolution of precipitate microstructures during the retrogression and re-ageing heat treatment of an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2010.05.017 ↗
19. Development of high strength AA 7010 aluminum alloy resistant to environmentally assisted cracking10.1016/j.corsci.2016.03.025 ↗
20. Mitigating intergranular stress corrosion cracking in age-hardenable Al-Zn-Mg-Cu alloys
21. Krishnan · 2016
22. Hydrogen bubbles in embrittled Al-Zn-Mg alloys10.1007/BF00739268 ↗
23. The effect of copper content and microstructure on the hydrogen embrittlement of AI-6Zn-2Mg alloys10.1007/BF02668893 ↗
24. The postulated mechanisms for stress corrosion cracking of aluminum alloys: a review of the literature 1980–198910.5006/1.3585235 ↗
25. Astm · 2013 · 1
26. 2005 · vol. 99 · 1
27. Astm · 2010 · 1
28. Environmentally assisted cracking behaviour of Al-Zn-Mg-Cu-Cr alloy bonded with polymer matrix composite stiffener10.1016/j.corsci.2013.06.015 ↗
29. Stress corrosion cracking in Al-Zn-Mg-Cu aluminum alloys in saline environments10.1007/s11661-012-1528-3 ↗
30. Environmental fatigue-crack surface crystallography for Al-Zn-Cu-Mg-Mn/Zr10.1007/s11661-008-9522-5 ↗
31. Hydrogen-enhanced local plasticity in aluminum: An Ab initio study
32. Hydrogen embrittlement understood10.1007/s11661-015-2836-1 ↗
33. Atmospheric stress corrosion cracking of a superplastic 7475 aluminum alloy10.1007/BF02652355 ↗
34. Early-stage precipitation in Al-Zn-Mg-Cu alloy (7050)10.1016/j.actamat.2004.06.025 ↗
35. Environmentally assisted cracking behavior of peak-aged 7010 aluminum alloy containing scandium10.1007/s11661-005-0098-z ↗
36. Crack tip chemistry and electrochemistry of environmental cracks in AA 705010.1016/j.corsci.2006.12.001 ↗
37. Effect of microstructure on stress corrosion cracking of an Al-Zn-Mg-Cu alloy10.1016/S0010-938X(98)00002-X ↗
38. Electrochemical behavior of thin film analogs of Mg(Zn, Cu, Al)210.1149/1.1386626 ↗
39. Evolution of grain boundary precipitates in Al 7075 upon aging and correlation with stress corrosion cracking behavior10.1007/s11661-012-1413-0 ↗
40. Hydrogen solubility, diffusion and trapping in high purity aluminum and selected Al-base alloys10.4028/www.scientific.net/MSF.331-337.1583 ↗
41. The diffusion and trapping of hydrogen in high purity aluminum10.1016/S1359-6454(98)00333-4 ↗
42. Hydrogen embrittlement and trapping
43. Hydrogen diffusion and trapping in a low copper 7xxx aluminium alloy investigated by Scanning Kelvin Probe Force Microscopy10.1016/j.msea.2017.08.119 ↗
44. Evidence for dislocation transport of hydrogen in aluminum10.1007/BF02642394 ↗
45. Role of heat-treatment and cathodic charging conditions on the hydrogen embrittlement of Hp-7075 aluminum-alloy10.1007/BF02782426 ↗
46. Microstructural effects on hydrogen embrittlement in a high purity 7075 aluminum alloy10.1016/0001-6160(87)90139-8 ↗