Abstract The corrosion resistance of Fe-Cr-Al alloy in four types of eutectic molten salts under thermal cycling conditions has been investigated using X-ray diffraction and scanning electron microscope techniques. The results show that thermal cycling can result in relatively higher corrosion rates compared with isothermal conditions, which might be connected closely to the thermal stress. Under the same conditions, the corrosion strength of the four eutectic salts should be in the order of chloride salt > mixture composed of carbonate salt and magnesium oxide > carbonate salt > nitrate salt for Fe-Al-Cr alloy, no matter for static corrosion or thermal cycling corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Phase Change Materials Research · Molten salt chemistry and electrochemical processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. The oxidation-sulfidation behaviour of iron alloys containing 16–40 AT% aluminium10.1016/0010-938X(93)90325-B ↗
2. Critical factors affecting the high-temperature corrosion performance of iron aluminides10.1016/S0921-5093(98)00924-1 ↗
3. Oxide scales formed on Fe–Cr–Al-based model alloys exposed to oxygen containing molten lead10.1016/j.jnucmat.2013.02.044 ↗
4. Corrosion resistance and microstructural stability of austenitic Fe–Cr–Al–Ni model alloys exposed to oxygen-containing molten lead10.1016/j.jnucmat.2019.06.043 ↗
5. Oxidative passivation of Fe–Cr–Al steels in lead-bismuth eutectic under oxygen-controlled static conditions at 700℃ and 800 ℃10.1016/j.jnucmat.2019.06.004 ↗
6. High temperature oxidation of Fe–Al and Fe–Cr–Al alloys: the role of Cr as a chemically active element10.1016/j.corsci.2010.06.019 ↗
7. Oxidation and corrosion behaviour of Fe–Cr and Fe–Cr–Al alloys with minor alloying additions10.1016/S0921-5093(97)00500-5 ↗
8. Oxidation studies of Fe10CrAl-RE alloys exposed to Pb at 550 °C for 10,000 h10.1016/j.jnucmat.2013.07.023 ↗
9. Microstructural control of FeCrAl alloys using Mo and Nb additions10.1016/j.matchar.2017.08.008 ↗
10. Influence of Ta/Zr minor-alloying on the high-temperature microstructural stability of cladding Fe–Cr–Al ferritic stainless steels10.1016/j.jnucmat.2019.05.008 ↗
11. 20 - high-temperature molten salts for solar power application10.1016/B978-0-12-398538-5.00020-2 ↗
12. Corrosion evaluation of eutectic chloride molten salt for new generation of CSP plants. Part 2: materials screening performance10.1016/j.est.2020.101381 ↗
13. Corrosion behaviour of metallic alloys in molten chloride salts for thermal energy storage in concentrated solar power plants: a review
14. Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies10.1016/j.solmat.2016.05.052 ↗
15. Corrosion resistance of alumina-forming alloys against molten chlorides for energy production. I: Pre-oxidation treatment and isothermal corrosion tests10.1016/j.solmat.2017.02.019 ↗
16. Molten chloride salts for next generation concentrated solar power plants: mitigation strategies against corrosion of structural materials10.1016/j.solmat.2018.12.020 ↗
17. Corrosion of steel alloys in eutectic NaCl+Na2CO3 at 700°C and Li2CO3+ K2CO3+ Na 2CO3 at 450°C for thermal energy storage10.1016/j.solmat.2017.05.063 ↗
18. Corrosion of stainless steel 316 in eutectic molten salts for thermal energy storage10.1016/j.solener.2018.03.053 ↗
19. Corrosion of Iron stainless steels in molten nitrate salt10.1016/j.egypro.2014.03.095 ↗
20. Constant extension rate testing of IN514LCF in molten nitrate salt10.1016/S0010-938X(98)00175-9 ↗
21. Corrosion monitoring and mitigation techniques on advanced thermal energy storage materials for CSP plants10.1016/j.solmat.2018.12.028 ↗
22. Corrosion evaluation of alumina-forming alloys in carbonate molten salt for CSP plants10.1016/j.renene.2019.03.087 ↗
23. Corrosion resistance of stainless steels during thermal cycling in alkali nitrate molten salts
24. Cyclic corrosion behaviour of Ni-Based superalloys in hot Lithium molten salt10.1007/s11085-012-9297-3 ↗
25. Damage analysis of 601 nickel superalloy in eutectic Na2CO3/NaCl molten salt under isothermal and thermal cycling conditions10.1016/j.solener.2019.09.030 ↗
26. Evaluation of cyclic hot corrosion resistance of plasma-sprayed composite coating in Na2SO4-60%V2O5 molten salt10.1007/s11666-020-01010-z ↗
27. Experimental investigations on the thermal stability of Na2CO3–K2CO3 eutectic salt/ceramic composites for high temperature energy storage10.1016/j.renene.2019.08.027 ↗
28. High-temperature phase change materials for thermal energy storage10.1016/j.rser.2009.11.011 ↗
29. High-temperature corrosion performance of austenitic stainless steels type AISI 316L andAISI321H,in molten Solar Salt10.1016/j.solener.2018.11.019 ↗
30. Corrosion mechanisms in molten salt thermal energy storage for concentrating solar power10.1016/j.rser.2019.109328 ↗
31. Corrosion behaviours of iron-chromium-aluminium steel near the melting point of various eutectic salts10.1016/j.solmat.2020.110510 ↗
32. Corrosion behaviour of various model alloys with NaCl–KCl coating10.1016/j.matchemphys.2005.03.015 ↗
33. Comparison of the high-temperature chloride-induced corrosion between Duplex steel and Ni based alloy in presence of H2S10.1016/j.corsci.2018.04.042 ↗
34. Internal oxidation and phase transformations of multi-phase Fe–Ni–Al and Fe–Ni–Al–Cr alloys induced by KCl corrosion10.1016/j.corsci.2011.02.034 ↗
35. Mahajan · 2001
36. Hafizul Faiz Maksom, Aiman Zawawi, corrosion behavior of eutectic molten salt solution on stainless steel 316L10.1016/j.sbspro.2015.06.465 ↗
37. Corrosion characterization in components for thermal energy storage applications
38. Corrosion of stainless steels and carbon steel by molten mixtures of commercial nitrate salts10.1361/10599490417542 ↗