Abstract

Abstract Based on the results of thermochemical analysis, NH 4 I + NH 4 Cl proved to be a more favorable activator for codepositing Co–Al–Y compared to NH 4 I or NH 4 Cl. Coating deposition experiments were also demonstrated that codeposition of Co–Al–Y with high concentration of Co and minute quantities of Y could be achieved at 1323 K in the NH 4 I + NH 4 Cl activated packs. The coating exhibited the best cyclic oxidation resistance at 1323 K when NH 4 I + NH 4 Cl were used as activator.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Metallurgical and Alloy Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. High temperature corrosion behaviour of a gradient NiCoCrAlYSi coating II: oxidation and hot corrosion10.1016/j.corsci.2010.03.032 ↗
2. Coating service experience with industrial gas turbines10.1179/mst.1986.2.3.302 ↗
3. Electrochemical study on hot corrosion of si-modified aluminide coated in-738LC in Na2SO4–20wt.% NaCl melt at 750°C10.1016/S0010-938X(02)00127-0 ↗
4. Influence of sulfur, platinum, and hafnium on the oxidation behavior of CVD NiAl bond coatings10.1023/A:1020525123056 ↗
5. Microstructure and corrosion resistance of magnesium alloy ZE41 with laser surface cladding by Al–Si powder10.1016/j.surfcoat.2008.04.052 ↗
6. A comparative study of two inward grown Pt modified Al diffusion coatings on a single crystal Ni base superalloy10.1016/S0921-5093(01)01236-9 ↗
7. Codeposition of Co and Al on nickel base superalloys by pack cementation process10.1016/j.surfcoat.2011.12.019 ↗
8. Hot corrosion behavior of Co modified nial coating on nickel base superalloys10.1016/j.corsci.2012.06.027 ↗
9. Effect of Ce and La additions in low temperature aluminization process by CVD–FBR on 12% Cr ferritic/martensitic steel and behaviour in steam oxidation10.1016/j.corsci.2008.05.008 ↗
10. Effect of trivalent rare earth dopants in nanocrystalline ceria coatings for high-temperature oxidation resistance10.1016/j.actamat.2007.01.043 ↗
11. Oxidation behaviour of ion-implanted NiCrAl10.1016/0257-8972(88)90143-0 ↗
12. The reactive element effect in high-temperature corrosion10.1016/0921-5093(89)90730-2 ↗
13. The development of Cr2O3 scales on iron-chromium alloys containing reactive elements10.1016/0010-938X(89)90057-7 ↗
14. Thermodynamics and kinetics of pack aluminide coating formation on IN-10010.1149/1.2401976 ↗
15. Codeposited chromium–aluminide coatings10.1149/1.2059176 ↗
16. Pack cementation aluminide coatings on superalloys: codeposition of Cr and reactive elements10.1149/1.2056219 ↗
17. Barin · 1973
18. Conditions for codeposition of Al and Cr on Ni base superalloys by pack cementation process10.1179/026708401101517890 ↗
19. Aluminide coating formation on nickel-base superalloys by pack cementation process10.1023/A:1012534220165 ↗
20. Mechanisms of formation of diffusion aluminide coatings on nickel-base superalloys10.1007/BF00604047 ↗
21. JCPDS File NO. 44-1185, JCPDS-International Center for Diffraction Data, ICDD 2001.
22. JCPDS File NO. 46-1212, JCPDS-International Center for Diffraction Data, ICDD 2001.
23. JCPDS File NO. 47-1049, JCPDS-International Center for Diffraction Data, ICDD 2001.
24. JCPDS File NO. 09-0097, JCPDS-International Center for Diffraction Data, ICDD 2001.
25. Oxidation behaviour of Kanthal Al and Kanthal AF at 1173K: effect of Yttrium alloying addition10.1016/S0169-4332(02)01506-4 ↗
26. Effect of reactive element oxide inclusions on the growth kinetics of protective oxide scales10.1016/j.actamat.2007.07.007 ↗
27. Yttrium-promoted selective oxidation of aluminium in the oxidation at 1100°C of an eutectic Ni–Al–Cr3C2 alloy10.1016/S0010-938X(98)00162-0 ↗
28. The influence of alloying elements on the development and maintenance of protective scales10.1007/BF01046725 ↗
29. Effect of Cr, Co and Ti additions on the high temperature oxidation behavior of Ni3Al10.1007/BF01046886 ↗