journal article·2019-04

High-temperature kinetics study of 430L steel powder oxidized in air at 600–850 °C

J. Karczewski, T. Brylewski, T. Miruszewski, K.B. Andersen, P.Z. Jasinski, S. Molin

Corrosion Science· Volume 149
Publisher page

Abstract

Abstract The 430L stainless steel powder with a mean particle size of 95 μm was studied to determine its high-temperature oxidation properties. Continuous thermogravimetric measurements were carried out for 100 h in air at temperatures in the range of 600–850 °C. Even though a considerable amount of Cr (up to ˜5 wt.% Cr) inside the grains was depleted – especially inside small grains – no breakaway oxidation was observed. This indicates that both the remaining Cr and the formed chromia scale remained protective with regard to the metallic core until the Cr concentration reached very low levels.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Predicting the depletion of chromium in two high temperature Ni alloys10.1016/j.corsci.2012.11.040 ↗
2. Kinetics of breakaway oxidation of Fe–Cr and Fe–Cr–Ni alloys in dry and wet carbon dioxide10.1016/j.corsci.2013.08.008 ↗
3. Corrosion stability of ferritic stainless steels for solid oxide electrolyser cell interconnects10.1016/j.corsci.2010.06.006 ↗
4. Oxidation resitance of sintered stainless steels: effect of yttria additions10.1016/S0010-938X(02)00217-2 ↗
5. High temperature corrosion of pure Fe, Cr and Fe–Cr binary alloys in O2 containing trace KCl vapour at 750°C10.1016/j.corsci.2009.05.014 ↗
6. Effect of substrate thickness on oxide scale spallation for solid oxide fuel cells10.1016/j.corsci.2011.03.025 ↗
7. Progress in metal-supported solid oxide fuel cells: a review10.1016/j.jpowsour.2010.02.035 ↗
8. High temperature oxidation of porous alloys for solid oxide fuel cell applications10.1016/j.ssi.2010.06.049 ↗
9. Development of robust metal-supported SOFCs and stack components in EU METSAPP consortium10.1002/fuce.201600191 ↗
10. Solid oxide cell R&D at Risø National Laboratory—and its transfer to technology10.1007/s10832-008-9458-6 ↗
11. Numerical evaluation of micro-structural parameters of porous supports in metal-supported solid oxide fuel cells10.1016/j.jpowsour.2014.09.185 ↗
12. Creep behaviour of porous metal supports for solid oxide fuel cells10.1016/j.ijhydene.2014.07.138 ↗
13. The effect of the oxidation atmosphere on the initial oxidation of type 430 stainless steel at 1273 K10.1016/S0010-938X(97)00113-3 ↗
14. Recent developments in stainless steels10.1016/j.mser.2009.03.001 ↗
15. Application of Fe–16Cr ferritic alloy to interconnector for a solid oxide fuel cell10.1016/S0167-2738(01)00863-3 ↗
16. Durability of symmetric-structured metal-supported solid oxide fuel cells10.1016/j.jpowsour.2017.09.075 ↗
17. Stainless steel-supported solid oxide fuel cell with La0.2Sr0.8Ti0.9Ni0.1O3−δ/yttria-stabilized zirconia composite anode10.1016/j.jpowsour.2016.05.076 ↗
18. Metal-supported solid oxide fuel cells operated in direct-flame configuration10.1016/j.ijhydene.2017.07.224 ↗
19. Oxidation limited life times of chromia forming ferritic steels10.1002/maco.200303798 ↗
20. In situ X-ray diffraction of surface oxide on type 430 stainless steel in breakaway condition using synchrotron radiation10.1016/j.corsci.2011.10.018 ↗
21. Metal-supported solid oxide fuel cell membranes for rapid thermal cycling10.1016/j.ssi.2004.09.056 ↗
22. Oxidation behavior of highly porous metallic components10.1007/s11085-008-9120-3 ↗
23. Oxidation behaviors of porous Haynes 214 alloy at high temperatures10.1016/j.matchar.2015.07.026 ↗
24. Characterization of porous stainless steel 430 for low- and intermediate-temperature solid oxide fuel cell (SOFC) substrates10.1080/15435070903372510 ↗
25. Fabrication of reactive element oxide coatings on porous ferritic stainless steel for use in metal-supported solid oxide fuel cells10.1016/j.surfcoat.2015.03.041 ↗
26. Porous Fe21Cr7Al1Mo0.5Y metal supports for oxygen transport membranes: thermo-mechanical properties, sintering and corrosion behaviour10.1016/j.ssi.2013.04.006 ↗
27. Oxidation limited lifetime of Ni‐Base metal foams in the temperature range 700–900 °C10.1002/adem.201000139 ↗
28. Processing and mechanical properties of porous Fe–26Cr–1Mo for solid oxide fuel cell interconnects10.1016/j.actamat.2010.07.030 ↗
29. Oxidation of stainless steel powder10.1007/s11085-013-9387-x ↗
30. Zirconia matrix composite dispersed with stainless steel particles: processing and oxidation behavior10.1016/j.jeurceramsoc.2012.11.020 ↗
31. Oxidation kinetics and mechanism of a zirconia based composite dispersed with 304L particles10.1016/j.corsci.2015.08.042 ↗
32. Kinetic model for solid-state reactions10.1063/1.1731812 ↗
33. Evaluation of 316L porous stainless steel for SOFC support10.1016/j.jeurceramsoc.2008.07.027 ↗
34. Metallic interconnects for solid oxide fuel cell: effect of water vapour on oxidation resistance of differently coated alloys10.1016/j.jpowsour.2008.11.041 ↗
35. Mrowec · 1982
36. Investigations of Mn–Co–O and Mn–Co–Y–O coatings deposited by the magnetron sputtering on ferritic stainless steels10.1016/j.surfcoat.2011.08.036 ↗
37. Thin films of La0.7Sr0.3MnO3−δ dip-coated on Fe–Cr alloys for SOFC metallic interconnect10.1016/j.ijhydene.2013.09.048 ↗
38. Pre-treatment and oxidation behavior of sol–gel Co coating on 430 steel in 750°C air with thermal cycling10.1016/j.surfcoat.2012.02.023 ↗
39. Residual stresses in oxide scale formed on Fe–17Cr stainless steel10.1016/j.apsusc.2014.07.195 ↗
40. Young · 2008
41. High temperature oxidation behavior of AISI 304 and AISI 430 stainless steels10.1590/S1516-14392006000400009 ↗
42. Inter-diffusion between Co3O4 coatings and the oxide scale on Fe-22Cr RID B-1852-2010 RID F-5900-201110.1016/j.jallcom.2006.06.086 ↗
43. Chromia scale adhesion on 430 stainless steel: effect of different surface treatments10.1016/j.jpowsour.2008.03.080 ↗
44. Effect of specimen thickness on microstructural changes during oxidation of the NiCrW alloy 230 at 950–1050°C10.1007/s11837-015-1645-8 ↗
45. Oxidation induced lifetime limits of chromia forming ferritic interconnector steels10.1115/1.1782925 ↗