Oxidation behavior of 3D Hi-Nicalon/SiC composite exposed in wet and simulated air environments
Source abstract
Abstract
Abstract Oxidation behavior of a 3D Hi-Nicalon/SiC composite was investigated in wet and simulated air with a flow rate of 3.5 cm s −1 at temperatures above 1000 °C. Results showed that oxidation was occurred mainly on the specimens surface and rate-controlled by oxygen diffusion for both oxidation environments. Silica formed in wet air was viscous and thicker. After oxidation, strength deterioration of the composite was associated mainly with the degradation of Hi-Nicalon fiber. Meanwhile, the difference in fracture behavior could be attributed to the change of fiber/matrix interface bonding caused by high temperature oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. Advanced ceramic matrix composite materials for current and future propulsion technology applications10.1016/j.actaastro.2004.05.052 ↗
3. Evaluation of CFCC liners with EBC after field testing in a gas turbine10.1016/S0955-2219(02)00142-5 ↗
4. Comparative study of high temperature composites10.1016/S1359-8368(01)00042-7 ↗
5. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
6. Oxidation of silicon carbide in a wet atmosphere10.1007/BF01106816 ↗
7. Oxidation of silicon carbide in oxygen and water vapor at 1500°C10.3891/acta.chem.scand.35a-0247 ↗
8. Thermal oxidation of sputtered silicon carbide thin films10.1149/1.2115988 ↗
9. Oxidation kinetics of chemical vapor deposited silion carbide in wet oxygen10.1111/j.1151-2916.1994.tb05357.x ↗
10. Variation of the oxidation rate of silicon carbide with water-vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
11. Oxidation behavior of SiC fiber-reinforced SiC10.1016/0022-3115(95)00133-6 ↗
12. Degradation of a SiC/SiC composite in the burner rig investigation by fractography10.1179/mht.2000.17.2.027 ↗
13. Experimental assessment of fiber-reinforced ceramics for combustor walls10.1115/1.1364523 ↗
14. High-temperature stability of SiC-based composites in high-water-vapor-pressure environments10.1111/j.1151-2916.2003.tb03463.x ↗
15. Oxygen transport through silica surface layers on silicon-containing ceramic materials
16. Oxidation of chemically vapor deposited silicon nitride and single-crystal silicon10.1111/j.1151-2916.1989.tb09693.x ↗
17. Silicon oxidation studies: the role of H2O10.1149/1.2133151 ↗
18. Viscosity and glass transition temperature of hydrous float glass10.1016/j.jnoncrysol.2006.11.009 ↗
19. Recent advances in nicalon ceramic fibres including Hi-Nicalon type S10.1016/S0151-9107(01)80004-0 ↗
20. Interfacial characterization of CVI–SiC/SiC composites10.1016/S0022-3115(02)00949-2 ↗
21. Effect of ageing treatments at high temperatures on the microstructure and mechanical behaviour of 2D Nicalon/C/SiC composites. 1: ageing under vacuum or argon10.1016/S0955-2219(96)00067-2 ↗
22. Thermal stability of the low-oxygen-content silicon carbide fiber, Hi-Nicalon™10.1016/S0266-3538(99)00012-3 ↗
23. Temperature dependence of tensile strength for a woven boron–nitride coated Hi-Nicalon™ SiC fiber-reinforced silicon–carbide–matrix composite10.1111/j.1151-2916.2001.tb00961.x ↗