Selective dissolution of amorphous Zr–Cu–Ni–Al alloys
Source abstract
Abstract
Amorphous Zr–Ni–Cu–Al ribbons were dealloyed by electrochemical selective dissolution. As a result three-dimensional microporous structures were obtained at different conditions (electrochemical potential, temperature, dissolution time). The smallest porous were obtained at low temperatures and potentials. To study the effect of precursor microstructure on the porous structure the as-cast alloys were annealed at two different temperatures – above Tg to cause structural relaxation of the amorphous material and at temperature above Tx to produce crystalline alloy. It is shown that only the entirely amorphous (as-cast and low-temperature annealed) alloys form homogeneous microporous structures as a result of the selective dissolution.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nanoporous metals and alloys · Metallic Glasses and Amorphous Alloys · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Nanoporous metals: fabrication strategies and advanced electrochemical applications in catalysis, sensing and energy systems10.1039/c2cs35210a ↗
2. Nanoporous metals by alloy corrosion: formation and mechanical properties10.1557/mrs2009.157 ↗
3. A general dealloying strategy to nanoporous intermetallics, nanoporous metals with bimodal, and unimodal pore size distributions10.1016/j.corsci.2012.01.023 ↗
4. Dependency of the formation of Au-stabilized nanoporous copper on the dealloying temperature10.1016/j.micromeso.2013.12.003 ↗
5. Selective dissolution sensitive to minor alloying in CuZr-based metallic glasses10.1016/j.corsci.2013.07.021 ↗
6. Synthesis of nanoporous Cu films by dealloying of electrochemically deposited Cu–Zn alloy films10.1016/j.corsci.2013.11.043 ↗
7. Dealloying behaviour of Cu–20Zr alloy in hydrochloric acid solution10.1016/j.corsci.2005.08.009 ↗
8. Microstructure of the mechanically alloyed and electrochemically etched Ti–6Al–4V and Ti–15Zr–4Nb nanocrystalline alloys10.1016/j.matchemphys.2010.08.057 ↗
9. Synthesis of nanoporous copper by dealloying of Al–Cu–Mg amorphous alloys in acidic solution: the effect of nickel10.1016/j.corsci.2011.01.033 ↗
10. Fabrication of nanoporous nickel by electrochemical dealloying10.1021/cm0497881 ↗
11. Copper nanowires and silver micropit arrays from the electrochemical treatment of a directionally solidified silver–copper eutectic10.1016/j.electacta.2007.07.048 ↗
12. Electrochemical production of nanopore arrays in a nickel aluminium alloy10.1016/j.electacta.2004.12.046 ↗
13. Fabrication of aligned pores in aluminum by electrochemical dissolution of monotectic alloys solidified under a magnetic field10.1016/j.scriptamat.2005.10.059 ↗
14. On the electrochemical dealloying of Mg–Cu alloys in a NaCl aqueous solution10.1016/j.corsci.2010.08.005 ↗
15. Selective dissolution of the γ phase in a binary Ni(γ)/Ni3Al(γ′) two-phase alloy10.1016/j.corsci.2010.07.036 ↗
16. Selective matrix dissolution in an Al–Si eutectic10.1016/j.corsci.2008.10.031 ↗
17. Synthesis of porous copper from nanocrystalline two-phase Cu–Zr film by dealloying10.1016/j.scriptamat.2006.09.009 ↗
18. Review of the techniques for the extraction of second-phase particles from aluminum alloys10.1016/S1044-5803(96)00046-0 ↗
19. Effect of preparation conditions on morphology and thermal stability of nanoporous copper10.1016/j.corsci.2012.03.032 ↗
20. Mechanochemical synthesis, thermal stability and selective electrochemical dissolution of Cu–Ag solid solutions10.1016/j.jallcom.2008.12.005 ↗
21. Investigation of dealloying in Au–Ag thin films by quantitative electron probe microanalysis10.1016/j.scriptamat.2006.12.022 ↗
22. Formation of nanoporous nickel by selective anodic etching of the nobler copper component from electrodeposited nickel–copper alloys10.1021/jp0772474 ↗
23. Nanometer-sized porous Ti-based metallic glass10.1016/j.scriptamat.2006.07.054 ↗
24. Nanostructuring of NiAl–Mo eutectic alloys by selective phase dissolution10.1016/j.electacta.2009.01.049 ↗
25. Fabrication and characterization of metallic glasses with a specific microstructure for micro-electro-mechanical system applications10.1016/j.jnoncrysol.2008.01.030 ↗
26. Dealloying of an Au-based amorphous alloy10.1016/j.intermet.2010.08.005 ↗
27. Electrochemical catalytic activities of nanoporous palladium rods for methanol electrooxidation10.1016/j.jpowsour.2010.03.098 ↗
28. Nanoporous metals by dealloying multicomponent metallic glasses10.1021/cm8009644 ↗
29. Dealloying of rapidly solidified amorphous and crystalline alloys10.1016/j.jallcom.2010.12.209 ↗
30. Novel nanoporous Au–Pd alloy with high catalytic activity and excellent electrochemical stability10.1021/jp907682x ↗
31. Nano-porous surface states of Ti–Y–Al–Co phase separated metallic glass10.1016/j.intermet.2009.05.008 ↗
32. Ti oxide nano-porous surface structure prepared by dealloying of Ti–Cu amorphous alloy10.1016/j.elecom.2010.12.025 ↗
33. Nucleation and growth of nanoporous copper ligaments during electrochemical dealloying of Mg-based metallic glasses10.1016/j.corsci.2012.10.010 ↗
34. Amorphous alloy: promising precursor to form nanoflowerpot10.1155/2014/263681 ↗
35. Effects of the initial microstructure of Ti–Cu alloys on final nanoporous copper via dealloying10.1016/j.jallcom.2013.01.010 ↗
36. Fabrication of nanoporous copper by dealloying of amorphous Ti–Cu–Ag alloys10.1016/j.jallcom.2013.01.087 ↗
37. Nanoporous gold by dealloying of an amorphous precursor10.1016/j.jallcom.2012.11.029 ↗
38. Nanoporous palladium fabricated from an amorphous Pd42.5Cu30Ni7.5P20 precursor and its ethanol electro-oxidation performance10.1016/j.electacta.2013.07.047 ↗
39. Synthesis of nanoporous gold by free corrosion of an amorphous precursor10.1016/j.jallcom.2014.01.239 ↗
40. Selective dissolution of amorphous and nanocrystalline Zr2Ni10.1016/j.corsci.2013.05.004 ↗
41. Microstructural design by controlled crystallization and alloying of Zr–Cu–Ni–Al based metallic glasses10.4028/www.scientific.net/JMNM.15-16.23 ↗
42. Estimating surface diffusion coefficients10.1016/0079-6816(95)00039-2 ↗