journal article·2020-02Open access

Oxidation of Fe-2.25Cr-1Mo in presence of KCl(s) at 400 °C – Crack formation and its influence on oxidation kinetics

A. Persdotter, M. Sattari, E. Larsson, M.A. Olivas Ogaz, J. Liske, T. Jonsson

Corrosion Science· Volume 163

Abstract

Accelerated corrosion of boiler equipment remains a challenge for efficiently utilising biomass- and waste for power production. To overcome this challenge a better understanding of the influence of corrosive species present is required. This study focuses on the influence of KCl(s) on corrosion of Fe-2.25Cr-1Mo at 400 °C. This is done by well-controlled laboratory exposures and detailed microstructural investigation with ion and electron microscopy (TEM, FIB, SEM, EDX, XRD, TKD). The scale microstructures are linked to oxidation kinetics. The results indicate that KCl(s) increases the ionic diffusion through the oxide scale as well as introduces cracks and delamination resulting in a rapid periodic growth process.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. The implications of chlorine-associated corrosion on the operation of biomass-fired boilers10.1016/S0360-1285(00)00003-4 ↗
2. Fundamental aspects of chlorine induced corrosion in power plants10.1179/mht.2003.018 ↗
3. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400–700 °C10.1016/S0010-938X(99)00142-0 ↗
4. Accelerated corrosion of pure Fe, Ni, Cr and several Fe-based alloys induced by ZnCl2-KCl at 450 °C in oxidizing environment10.1016/S0921-5093(02)00386-6 ↗
5. Influence of Cr content on the corrosion of Fe-Cr alloys: the synergistic effect of NaCl and water vapor10.1023/A:1023083309041 ↗
6. Local reactions of KCl particles with iron, nickel and chromium surfaces10.1002/maco.200503903 ↗
7. High temperature corrosion of pure Fe, Cr and Fe-Cr binary alloys in O2 containing trace KCl vapour at 750 °C10.1016/j.corsci.2009.05.014 ↗
8. The effects of chlorides, hydrogen-chloride, and sulfur-dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
9. The influence of alloying elements on the chlorine-induced high temperature corrosion of Fe-Cr alloys in oxidizing atmospheres10.1002/(SICI)1521-4176(199910)50:10<561::AID-MACO561>3.0.CO;2-L ↗
10. High temperature corrosion of coatings and boiler steels in oxidizing chlorine-containing atmosphere10.1016/S0921-5093(02)00537-3 ↗
11. High temperature corrosion of coatings and boiler steels below chlorine-containing salt deposits10.1016/j.corsci.2003.09.026 ↗
12. KCl induced corrosion of a 304-type austenitic stainless steel at 600 °C: the role of potassium10.1007/s11085-005-5704-3 ↗
13. Laboratory scale tests on corrosion behavior of boiler materials in simulated combustion atmospheres (EU Project – OPTICORR)10.1002/maco.200503931 ↗
14. Initial stages of the HCl-induced high-temperature corrosion of alloy 31010.1149/1.2754174 ↗
15. Alkali induced corrosion of 304-type austenitic stainless steel at 600 °C: comparison between KCl, K2CO3 and K2SO410.4028/www.scientific.net/MSF.595-598.367 ↗
16. The influence of small amounts of KCl(s) on the initial stages of the corrosion of alloy Sanicro 28 at 600 °C10.1007/s11085-008-9118-x ↗
17. An ESEM in-situ investigation of the influence of H2O on iron oxidation at 500 °C10.1016/j.corsci.2009.05.016 ↗
18. Microstructural investigation of the KCl-induced corrosion of the austenitic alloy Sanicro 28 (35Fe27Cr31Ni) at 600 °C10.3184/096034009X464339 ↗
19. Alkali induced high temperature corrosion of stainless steel: the influence of NaCl, KCl and CaCl210.1007/s11085-012-9293-7 ↗
20. The effects of KCl, NaCl and K2CO3 on the high-temperature oxidation onset of Sanicro 28 steel10.1007/s11085-016-9613-4 ↗
21. Einfluß von HCl und Cl2auf die Hochtemperaturkorrosion des 2 1/4 Cr 1 Mo-Stahls in Atmosph”aren mit hohen Sauerstoffdr“ucken10.1002/maco.19900410602 ↗
22. Einflun von Chloriden auf die Oxidat ion10.1002/maco.19920431202 ↗
23. High temperature oxidation behaviour of boiler steels under simulated combustion gases10.4028/www.scientific.net/MSF.461-464.981 ↗
24. The influence of small amounts of KCl(s) on the high temperature corrosion of a Fe-2.25Cr-1Mo steel at 400 and 500 °C10.1002/maco.201005942 ↗
25. An ESEM in situ investigation of initial stages of the KCl induced high temperature corrosion of a Fe-2.25Cr-1Mo steel at 400 °C10.1016/j.corsci.2011.03.007 ↗
26. Larsson · 2016
27. The influence of oxide-scale microstructure on KCl(s)-induced corrosion of low-alloyed steel at 400 °C10.1007/s11085-018-9881-2 ↗
28. McNallan · 1983 · 316
29. Kofstad · 1988
30. Oxidation driven permeation of iron oxide scales by chloride from experiment guided 1st principles modelling10.1021/acs.jpcc.9b06497 ↗
31. Initial corrosion attack of 304L and T22 in 2 MW biomass gasifier: a microstructural investigation10.1179/0960340914Z.000000000101 ↗
32. Low temperature oxidation of pure iron: growth kinetics and scale morphologies10.4028/www.scientific.net/MSF.461-464.591 ↗
33. The influence of KCl on the corrosion of an Austenitic stainless steel (304L) in oxidizing humid conditions at 600 °C: a microstructural study10.1007/s11085-009-9156-z ↗
34. Oxidation of iron at 400–600 °C in dry and wet O210.1016/j.corsci.2010.01.002 ↗
35. Oxidation of binary FeCr alloys (Fe-2.25Cr, Fe-10Cr, Fe-18Cr and Fe-25Cr) in O2 and in O2 + H2O environment at 600 °C10.1007/s11085-010-9229-z ↗
36. Point defects and cation tracer diffusion in (Crx,Fe1−x)3−δO4 spinels
37. Diffusion in oxides10.2138/rmg.2010.72.17 ↗
38. Thermo-Calc & DICTRA, computational tools for materials science10.1016/S0364-5916(02)00037-8 ↗
39. Corrosion of furnace wall materials in waste-wood fired power plant10.1179/1743278214Y.0000000228 ↗
40. Effect of sewage sludge addition on initial corrosion of 16Mo3 and 310S when exposed in a used wood fired boiler10.1002/maco.201508693 ↗
41. da Silva · 2007
42. Effect of substrate grain size on the growth, texture and internal stresses of iron oxide scales forming at 450 °C10.1007/s11085-009-9162-1 ↗
43. Mössbauer study of the effect of potassium on iron oxide catalysts10.1007/BF02320299 ↗
44. The oxidation of metals at high temperatures
45. The lateral growth strain accompanying the formation of a thermally grown oxide10.1016/S1359-6454(02)00532-3 ↗
46. Some electrical properties of the defective γ phases of spinel structure during their transformation to the rhombohedral α phases10.1007/BF02396954 ↗
47. Influence of synthesis conditions on the γ-Fe203 properties
48. Creep properties of heat resistant steels and superalloys ċ 2.25Cr-1Mo steel