Alternating current anodizing of titanium in halogen acids combined with Anodic Spark Deposition: Morphological and structural variations
Source abstract
Abstract
The identification of anodic processes able to generate high surface area TiO2 layers is a key requirement, whenever applications focused on its photoactivity or the integration between titanium implants and human body are considered. To achieve this goal, this research proposes an innovative two-step anodizing procedure. The first step consists of supplying alternating current to titanium in halogen acid electrolyte which quickly modifies its morphology. HCl and HBr were found to roughen effectively the metal surface, thus increasing its surface area. The successive step, an Anodic Spark Deposition treatment, generates a thick, semicrystalline oxide, containing both anatase and rutile crystals.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Anodic Oxide Films and Nanostructures · Bone Tissue Engineering Materials · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Leyens · 2003
2. Winston Revie · 2000
3. The effects of spark anodizing treatment of pure titanium metals and titanium alloys on corrosion characteristics10.1016/j.surfcoat.2006.11.022 ↗
4. Increasing of the corrosion resistance of the Ti6Al4V alloy by thickness anodic oxidation10.1007/BF00701236 ↗
5. Anodic Spark Deposition treatments to increase reliability of Ti6Al4V modular prostheses
6. Electrochemical oxidation of titanium surfaces10.1149/1.2425674 ↗
7. Galvanostatic anodization of titanium – structures and compositions of the anodic films10.1016/0013-4686(88)80223-8 ↗
8. The effect of film formation conditions on the structure and composition of anodic oxide films on titanium10.1016/0010-938X(94)00133-Q ↗
9. Surface modification of titanium, titanium alloys, and related materials for biomedical applications10.1016/j.mser.2004.11.001 ↗
10. The colours due to thin films on metals10.1098/rspa.1925.0017 ↗
11. Self-colour anodizing of titanium10.1016/0376-4583(82)90033-4 ↗
12. Colour properties of barrier anodic oxide films on aluminium and titanium studied with total reflectance and spectroscopic ellipsometry10.1016/j.surfcoat.2004.01.021 ↗
13. Pedeferri · 1982
14. Preparation and characterisation of titanium dioxide films for catalytic applications generated by anodic spark deposition10.1016/j.tsf.2003.11.168 ↗
15. Ceramic coatings by anodic spark deposition10.1080/10426919108934737 ↗
16. Osteointegration of titanium and its alloys by anodic spark deposition and other electrochemical techniques: a review
17. Crystallization of anodic titania on titanium and its alloys10.1016/S0010-938X(03)00040-4 ↗
18. Titanium oxide nanotube arrays prepared by anodic oxidation10.1557/JMR.2001.0457 ↗
19. Hydrogen sensing using titania nanotubes10.1016/S0925-4005(03)00222-3 ↗
20. Enhanced photocleavage of water using titania nanotube arrays10.1021/nl048301k ↗
21. Self-organized porous titanium oxide prepared in Na2SO4/NaF electrolytes10.1016/j.electacta.2005.01.014 ↗
22. Titanium oxide nanotubes prepared in phosphate electrolytes10.1016/j.elecom.2005.03.007 ↗
23. Dye-sensitized anodic TiO2 nanotubes10.1016/j.elecom.2005.08.013 ↗
24. A review on highly ordered, vertically oriented TiO2 nanotube arrays: fabrication, material properties, and solar energy applications10.1016/j.solmat.2006.04.007 ↗
25. S. Goidanich, L. Lazzari, M. Ormellese, MP. Pedeferri, Influence of AC on carbon steel corrosion in simulated soil conditions, in: 16th International Corrosion Congress ICC, Beijing, China, Paper 04-03, September 2005.
26. Tuning of titanium oxide morphology at micro and nano scale by alternating current anodising10.4028/www.scientific.net/JNanoR.6.61 ↗
27. Photocatalytic destruction of VOCs in the gas-phase using titanium dioxide10.1016/S0926-3373(97)00012-X ↗
28. Photocatalysis: a promising route for 21st century organic chemistry10.1039/b700395c ↗
29. Titanium dioxide photocatalysis10.1016/S1389-5567(00)00002-2 ↗
30. Photocatalytic removal of nitrogen oxides via titanium dioxide10.1007/s10311-004-0087-2 ↗
31. Photocatalytic decomposition and reduction reactions of nitric oxide over Degussa P2510.1016/j.apcatb.2005.07.014 ↗
32. Structure of the interface between rabbit cortical bone and implants of gold, zirconium and titanium10.1023/A:1018579605426 ↗
33. Formation and characterization of anodic titanium oxide films containing Ca and P10.1002/jbm.820290110 ↗
34. Characterization of thin hydroxyapatite layers formed on anodic titanium oxide films containing Ca and P by hydrothermal treatment10.1002/jbm.820290907 ↗
35. Nanostructured surfaces for biomedical applications. Part I: nanotopography
36. Electrochemical surface modification of titanium for implant abutments can affect oral bacteria contamination
37. Effect of anodic oxidation parameters on the titanium oxides formation10.1016/j.corsci.2006.04.002 ↗
38. Pitting corrosion of titanium10.1149/1.2054783 ↗
39. A study on metastability phenomena of passive films for corrosion resistant alloys10.1016/j.electacta.2006.12.037 ↗