Detection and analysis of anodic current transients associated with nanoscale β-phase precipitates on an Al–Mg microelectrode
Source abstract
Abstract
Abstract The metastable pitting of Al–5 wt%Mg microelectrode (diameter 50 μm) after aging at 150 °C for 10 h has been investigated under a constant potential in deaerated 0.6 M NaCl solution (pH 3.5). Current transients (pA size) associated with the dissolution of nanoscale β-phase precipitates have been detected. Taking the cathodic current of H 2 evolution inside the pit into account, the average volume determined from a charge associated with individual current transients is about 39% of those measured by TEM. This result implies that the selective dissolution of Mg in β-phase precipitates (Al 3 Mg 2 ) may occur during the metastable pitting process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Repetitive nucleation of corrosion pits on stainless steel and the effects of surface roughness10.1149/1.1416503 ↗
2. Initiation events for pitting corrosion of stainless steel?10.1016/0010-938X(91)90050-Y ↗
3. Metastable pitting corrosion of stainless steel and the transition to stability10.1098/rsta.1992.0114 ↗
4. Metastable pitting of aluminum and criteria for the transition to stable pit growth10.1149/1.2059275 ↗
5. Metastable pitting characteristics of aluminium alloys measured using current transients during potentiostatic polarisation10.1016/j.electacta.2012.01.090 ↗
6. Electrochemical characteristics of the Al2Cu, Al3Ta and Al3Zr intermetallic phases and their relevancy to the localized corrosion of Al alloys10.1016/0010-938X(93)90148-A ↗
7. A compilation of corrosion potentials reported for intermetallic phases in aluminum alloys10.1149/1.2048447 ↗
8. Electrochemical characteristics of intermetallic phases in aluminum alloys10.1149/1.1869984 ↗
9. Combined anodic/cathodic transient currents within nucleating pits on Al–Fe alloy surfaces10.1016/j.corsci.2010.11.008 ↗
10. Relating the early evolution of microstructure with the electrochemical response and mechanical performance of a Cu-rich and Cu-lean 7xxx aluminum alloy10.1149/2.062211jes ↗
11. The reliability of electrochemical noise and current transients characterizing metastable pitting of Al–Mg–Si microelectrodes10.1016/j.corsci.2013.11.008 ↗
12. SVET, SKP and EIS study of the corrosion behaviour of high strength Al and Al–Li alloys used in aircraft fabrication10.1016/j.corsci.2014.03.001 ↗
13. Metastable pitting of stainless steel10.5006/1.3583880 ↗
14. The nucleation, growth and stability of micropits in stainless steel10.1016/0010-938X(94)90145-7 ↗
15. Depassivation current transients measured between identical twin microelectrodes in open circuit10.1016/j.corsci.2006.06.036 ↗
16. Effects of constituent particles and sensitization on surface spreading of intergranular corrosion on a sensitized AA5083 alloy10.1016/j.electacta.2013.06.036 ↗
17. Microelectrodes for studies of localized corrosion processes10.1016/S0013-4686(98)00025-5 ↗
18. Direct visualization of β phase causing intergranular forms of corrosion in Al–Mg alloys10.1016/j.matchar.2013.03.014 ↗
19. Correlations between stress corrosion cracking susceptibility and grain boundary microstructures for an Al–Zn–Mg alloy10.1016/j.corsci.2013.07.032 ↗
20. Spreading of intergranular corrosion on the surface of sensitized Al–4.4Mg alloys: a general finding10.1016/j.corsci.2012.02.018 ↗
21. Role of Mg in the stress corrosion cracking of an Al–Mg alloy10.1007/s11661-001-0148-0 ↗
22. Y.D. Yuan, Localized corrosion and stress corrosion cracking of aluminium–magnesium alloys, Ph.D. Dissertation, University of Birmingham, 2005.
23. Metallurgical factors influencing the corrosion of aluminum, Al–Cu, and Al–Si alloy thin films in dilute hydrofluoric solution
24. Characterization of atomic layer deposition HfO2, Al2O3, and plasma-enhanced chemical vapor deposition Si3N4 as metal–insulator–metal capacitor dielectric for GaAs HBT technology10.1116/1.4769207 ↗
25. Stress corrosion cracking of sensitized AA5083 (Al–4.5Mg–1.0Mn)10.1007/s11661-001-1036-3 ↗
26. Transport processes and the mechanism of pitting of metals10.1149/1.2132857 ↗
27. Salt film formation during corrosion of aluminum10.1016/0013-4686(84)87098-X ↗
28. Corrosion of magnesium of high anodic potentials10.1149/1.2119940 ↗
29. A first quantitative XPS study of the surface films formed, by exposure to water, on Mg and on the Mg–Al intermetallics: Al3Mg2 and Mg17Al1210.1016/j.corsci.2009.02.017 ↗