In situ X-ray diffraction of surface oxide on type 430 stainless steel in breakaway condition using synchrotron radiation
Source abstract
Abstract
Abstract Changes in the crystal structure of type 430 stainless steel and the oxides on its surface were studied in situ at 1373 K using a high-intensity synchrotron X-ray source provided by SPring-8 in Japan. The surface of the steel was initially covered with Cr2O3, which was then converted to FeCr2O4, and finally Fe3O4 and Fe2O3 formed on it. These results indicated that the reason for the breakaway oxidation in type 430 stainless steel is Cr depletion beneath Cr2O3 layer and the subsequent ionisation of Fe, not the simple mechanical failure of Cr2O3.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Breakaway of type 430 stainless steel in water vapor/oxygen atmospheres at elevated temperatures
2. High temperature oxidation of some iron–chromium alloys
3. The unusual scaling behaviour of iron-22.9% chromium in air at 1100°C10.1016/0010-938X(64)90027-7 ↗
4. On the mechanism of oxidation of iron-16.4% chromium at high temperature10.1016/0010-938X(64)90026-5 ↗
5. Limit to adherence of oxide scales10.1179/mst.1990.6.1.81 ↗
6. Scale growth and stress development10.1179/mst.1988.4.12.1079 ↗
7. Mechanisms of breakaway oxidation and application to chromia-forming steel10.1023/A:1018855914737 ↗
8. Chromium depletion at 2-dimensional features during the selective oxidation of a 20Cr–25Ni austenitic steel10.1007/s11085-006-9039-5 ↗
9. Röntgenographische Untersuchung der Systeme Fe2O3–Cr2O3 und Fe2O3–Mn2O3
10. The structure of oxide scales on chromium steels
11. The initial oxidation of type 430 stainless steel in O2–H2O–N2 atmospheres at 1273 K10.1016/0010-938X(96)00093-5 ↗
12. AES/GDS characterization of thin oxide films on Fe–Cr steels10.1002/sia.740170803 ↗
13. Identification by photoelectrochemistry of oxide phases grown during the initial stage of thermal oxidation of AISI 441 ferritic stainless steel in air or in water vapour10.1016/j.corsci.2008.12.002 ↗
14. In situ study of real structure effect on the initial oxidation of FeCrAl alloys by two-dimensional high temperature X-ray diffraction10.4028/www.scientific.net/MSF.522-523.69 ↗
15. Strains in thermally growing alumina films measured in-situ using synchrotron X-rays10.4028/www.scientific.net/MSF.522-523.433 ↗
16. Yonemura · Tetsu-to-Hagane · 2007 · 93 · 68
17. M. Schütze, Protective oxide scales and their breakdown, John Wiley & Sons, 1997.
18. Immiscibility in the Fe3O4–FeCr2O4 spinel binary10.1016/S0022-3697(03)00237-3 ↗
19. A thermodynamic model of Fe–Cr spinels10.1007/s00410-005-0669-4 ↗
20. Chantler · J. Phys. Chem. Ref. Data · 1995 · 24 · 7110.1063/1.555974 ↗
21. Thermodynamics of gas phase chromium species: the chromium oxides, the chromium oxyhydroxides, and volatility calculations in wast incineration processes10.1016/0010-2180(93)90087-J ↗
22. Oxidation of 310 steel in H2O/O2 mixtures at 600 C: the effect of water-vapour-enhanced chromium evaporation10.1016/S0010-938X(02)00056-2 ↗
23. Evaporation of Cr2O3 in atmospheres containing H2O10.1023/A:1023671206976 ↗