The effect of Zn coating layers on the hydrogen embrittlement of hot-dip galvanized twinning-induced plasticity steel
Source abstract
Abstract
Abstract The effect of Zn coating layers on hydrogen embrittlement (HE) was investigated using hot-dip galvanized (HDG) twinning-induced plasticity (TWIP) steel. The Zn coating layers consisted of an η-Zn layer and Fe-Zn intermetallic layers of ζ and δ without ο. H was trapped particularly at the ζ layer without Zn-H compounds. The activation energies of H desorption from the δ and ζ layers were 60.0 kJ mol 1 and 75.4 kJ mol 1 , respectively. The H-charged HDG_TWIP steel did not reveal HE due to the intermetallic layers, which are exceptionally brittle even when H is not enriched.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
2. Effects of inclusions on delayed fracture properties of three twinning induced plasticity (TWIP) steels10.1007/s11661-012-1472-2 ↗
3. Effects of Al addition on deformation and fracture mechanisms in two high manganese TWIP steels10.1016/j.msea.2010.12.085 ↗
4. Effect of hydrogen content on the embrittlement in a FeMnC twinning-induced plasticity steel10.1016/j.corsci.2012.03.009 ↗
5. State-of-the-knowledge on TWIP steel10.1179/1743284711Y.0000000095 ↗
6. Microstructural evolution during plastic deformation of twinning-induced plasticity steels10.1016/j.scriptamat.2011.12.016 ↗
7. In situ observation of the influence of Al on deformation-induced twinning in TWIP steel10.2355/isijinternational.55.870 ↗
8. Hydrogen embrittlement in a Fe-Mn-C ternary twinning-induced plasticity steel10.1016/j.corsci.2011.09.022 ↗
9. Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe-Mn-C TWIP steels10.1016/j.corsci.2014.01.022 ↗
10. Delayed static failure of twinning-induced plasticity steels10.1016/j.scriptamat.2012.02.038 ↗
11. The effects of sacrificial coatings on hydrogen embrittlement and re-embrittlement of ultra high strength steels10.1016/j.corsci.2007.11.023 ↗
12. Hydrogen embrittlement susceptibility of galvanized 4135 steel in cement environment10.1016/0010-938X(93)90183-H ↗
13. Hydrogen entry into steel during atmospheric corrosion process10.1016/j.corsci.2004.10.006 ↗
14. Hydrogen-assisted failure in a twinning-induced plasticity steel studied under in situ hydrogen charging by electron channeling contrast imaging10.1016/j.actamat.2013.04.030 ↗
15. Hydrogen-induced cracking at grain and twin boundaries in an Fe-Mn-C austenitic steel10.1016/j.scriptamat.2011.12.015 ↗
16. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe-18Mn-1.5Al-0.6C TWIP steel10.2355/isijinternational.49.1952 ↗
17. Interaction of aluminium with hydrogen in twinning-induced plasticity steel10.1016/j.scriptamat.2014.06.007 ↗
18. The mechanism of enhanced resistance to the hydrogen delayed fracture in Al-added Fe-18Mn-0.6C twinning-induced plasticity steels10.1016/j.ijhydene.2012.03.100 ↗
19. Effects of grain size on hydrogen embrittlement in a Fe-22Mn-0.6C TWIP steel10.1016/j.ijhydene.2015.06.112 ↗
20. The advantage of grain refinement in the hydrogen embrittlement of Fe-18Mn-0.6C twinning-induced plasticity steel10.1016/j.corsci.2015.01.012 ↗
21. Electrochemical studies on the corrosion of a range of zinc alloy coated steel in alkaline solutions10.1016/0257-8972(95)02428-X ↗
22. Hydrogen permeation inhibition by thin layer ZnNi alloy electrodeposition10.1023/A:1003408230951 ↗
23. Hydrogen embrittlement risk of high strength galvanized steel in contact with alkaline media10.1016/j.corsci.2011.05.023 ↗
24. Tailoring the catalytic activity of electrodes with monolayer amounts of foreign metals10.1039/c3cs60026b ↗
25. Hydrogen absorption during zinc plating on steel10.1016/S0010-938X(97)86101-X ↗
26. The effects of an Fe-Zn intermetallic-containing coating on the stress corrosion cracking behavior of a hot-dip galvanized steel10.1016/S0257-8972(01)01017-9 ↗
27. Kinetics of hydrogen movement in zinc10.3938/jkps.51.1320 ↗
28. Hydrogen effects on cathodically charged twinning-induced plasticity steel10.1016/j.scriptamat.2011.12.012 ↗
29. Cathodic hydrogen charging of zinc10.1016/j.corsci.2013.10.016 ↗
30. The metallurgy of zinc-coated steel10.1016/S0079-6425(98)00006-1 ↗
31. Formability of galvanized interstitial-free steel sheets10.1016/j.jmatprotec.2005.10.016 ↗
32. Effect of microstructure and texture on formability and mechanical properties of hot-dip galvanized steel sheets10.1016/j.jmatprotec.2007.05.035 ↗
33. The effect of Ti precipitates on hydrogen embrittlement of Fe-18Mn-0.6C-2Al-xTi twinning-induced plasticity steel10.1016/j.corsci.2014.08.005 ↗
34. Reaction kinetics of the formation of intermetallic FeZn during hot-dip galvanizing of steel
35. Zinc/iron phase transformation studies on galvannealed steel coatings by X-ray diffraction
36. Effect of chemical composition of steel on the structure of hot-dip galvanized coating
37. The lattice hardening due to dissolved hydrogen in iron and steel10.1016/0036-9748(76)90119-8 ↗
38. Synthesis and characterization of the Fe-Zn intermetallic phases using the Rietveld method
39. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
40. Trap theory of Hydrogen embrittlement10.1016/0001-6160(80)90106-6 ↗
41. Wall · 1985
42. Orientation domains and texture in hot-dipped galvanized coatings10.1007/s11661-002-0391-z ↗
43. Solidification and spangle formation of hot-dip-galvanized zinc coatings10.1007/s11661-998-0144-8 ↗
44. Temperature programmed desorption studies of hydrogen on Zn (0001) surfaces10.1016/0039-6028(84)90774-X ↗
45. Galvannealing of (high-)maganese-alloyed TRIP- and X-IP®-steel10.1002/srin.201000115 ↗
46. Phase diagram study of Fe-Zn intermetallics10.1361/105497101770338978 ↗
47. Reaction kinetics in differential thermal analysis10.1021/ac60131a045 ↗
48. Thermal analysis of trapped hydrogen in pure iron10.1007/BF02642424 ↗
49. Hydrogen trapping in ferritic steel weld metal10.1179/095066002225006548 ↗
50. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗