journal article·2014-11

Carbon steel corrosion in clay-rich environment

Y. El Mendili, A. Abdelouas, A. Ait Chaou, J.-F. Bardeau, M.L. Schlegel

Corrosion Science· Volume 88
Publisher page

Abstract

We investigated the carbon steel corrosion in carbon dioxide clay-rich environment to understand its behavior under geological conditions. The results show the formation of magnetite as the main corrosion product in the first step of the corrosion process, followed by the formation of different corrosion products with complex mixtures of iron-oxide, hydroxycarbonate, hydroxychloride and sulfide phases. These results strongly contrast with similar experiments conducted under H2 atmosphere where the major corrosion products consisted of iron sulfides. It appears then important to consider all the geochemical parameters including gas composition to better study corrosion of steel buried in geological formations. 2014 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. Kim · 2002
2. Kang · 2002
3. Nuclear Energy Agency, Organization for Economic Cooperation and Development, Partnering for Long-term Management of Radioactive Wastes: Evolution and Current Practice in Thirteen Countries, NEA No. 6823, 2010.
4. Modelling iron-clay interactions in deep geological disposal conditions10.1016/j.pce.2006.04.014 ↗
5. Prediction of long term corrosion behaviour in nuclear waste systems10.1557/PROC-932-35.1 ↗
6. Microbial corrosion of P235GH steel under geological conditions10.1016/j.pce.2010.04.007 ↗
7. Nuclear Energy Agency of the Organisation for Economic Co-operation and Development, Safety Cases for Deep Geological Disposal of Radioactive Waste: Where Do We Stand?, Symposium Proceedings Paris, France, 2007.
8. B. Kursten, F. Druyts, P. Van Iseghem, Geological disposal of conditioned high-level and long lived radioactive waste, Studies on container materials – laboratory corrosion tests on stainless steel, Belgian Nuclear Research Centre Report, SCK⋅CEN-R-3774, 2003.
9. Cation exchanged Fe(II) and Sr compared to other divalent cations (Ca, Mg) in the Bure Callovian-Oxfordian formation. Implications for porewater composition modelling10.1016/j.apgeochem.2007.11.002 ↗
10. Feasibility and behavior of a full scale disposal cell in a deep clay layer, Rock Mechanics for Resources, Energy and Environment
11. H. El Hajj, A. Abdelouas, B. Grambow, Role of microbial activity on corrosion of steel used for radioactive waste disposal, Clays in Natural & Engineered Barriers for Radioactive Waste Confinement, 4th International Meeting, Nantes, France, 2010.
12. P. Van Iseghem, B. Kursten, E. Valcke, H. Serra, J. Fays, A. Sneyers. In situ testing of waste forms and container materials: contribution to the identification of their long term behaviour, in: D. Féron, D.D. Macdonald (Eds.), Proceedings of the International Workshop on Prediction of Long Term Corrosion Behaviour in Nuclear Systems, Cadarache, France, November 26–29, 2001, EFC Publications n° 36, 2002.
13. R.M. Maier, I.L. Pepper, C.P. Gerba, Environmental microbiology, second ed., Elsevier, 2009, pp. 387–439, doi: B978-0-12-370519-8.00020-1.
14. Insight into the mechanism of carbon steel corrosion under aerobic and anaerobic conditions10.1039/c3cp50853f ↗
15. Corrosion of carbon steel under sequential aerobic–anaerobic environmental conditions10.1016/j.corsci.2013.07.017 ↗
16. Bacteriological influence in the development of iron sulfide species in marine immersion environments10.1016/S0010-938X(02)00147-6 ↗
17. Mineralogical characteristics and transformations during long-term operation of a zerovalent iron reactive barrier10.2134/jeq2003.2033 ↗
18. A computational approach to predicting the formation of iron sulfide species using stability diagrams10.1016/S0098-3004(97)00038-1 ↗
19. Biocorrosion: the action of sulfate-reducing bacteria
20. Mackinawite formation during microbial corrosion10.5006/1.3585154 ↗
21. Impact of sulphidogenic environment on the corrosion behavior of carbon steel at 90°C10.1039/c3ra42221f ↗
22. Corrosion of P235GH carbon steel in simulated Bure soil solution
23. Preferred orientations and anisotropy in shales: Callovo-Oxfordian shale (France) and Opalinus Clay (Switzerland)10.1346/CCMN.2008.0560301 ↗
24. Alteration of Callovo-Oxfordian clay from Meuse-Haute Marne underground laboratory (France) by alkaline solutions: II. Modelling of mineral reactions at 120°C and at hyperalkaline solutions10.1016/j.apgeochem.2004.03.010 ↗
25. A thermodynamic model for the prediction of pore water composition of clayey rock at 25 and 80°C - Comparison with results from hydrothermal alteration experiments10.1016/j.chemgeo.2012.09.040 ↗
26. New evidences of in situ laser irradiation effects on γ-Fe2O3 nanoparticles: a Raman spectroscopic study10.1002/jrs.2762 ↗
27. Insights into the mechanism related to the phase transition from γ-Fe2O3 to α-Fe2O3 nanoparticles induced by thermal treatment and laser irradiation10.1021/jp308418x ↗
28. Phase transformation in CaCO3/iron oxide composite induced by thermal treatment and laser irradiation10.1002/jrs.4200 ↗
29. Raman study of magnetite (Fe3O4): laser induced thermal effects and oxidation10.1016/S0022-4596(03)00294-9 ↗
30. Raman micro spectroscopy of some iron oxides and oxyhydroxides10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B ↗
31. Advances in understanding atmospheric corrosion of iron. I. Rust characterisation of ancient ferrous artefacts exposed to indoor atmospheric corrosion10.1016/j.corsci.2003.09.027 ↗
32. Remote-Raman spectroscopic study of minerals under supercritical CO2 relevant to Venus exploration10.1016/j.saa.2011.01.033 ↗
33. Formation of poorly crystalline iron monosulfides: surface redox reactions on high purity iron, spectroelectrochemical studies10.1016/j.corsci.2006.03.010 ↗
34. Effect of sulfide on carbon steel corrosion in anaerobic near-neutral pH saline solutions10.5006/0687 ↗
35. E. Chan, D. John, S. Bailey, B. Kinsella, S. Nesic, Formation of magnetite scale under anaerobic conditions at low temperatures, Paper presented at the Australasian Corrosion Association, Coffs Harbour, 2009.
36. A Raman spectroscopic study of selected minerals of the rosasite group10.1002/jrs.1521 ↗
37. Determination of standard Gibbs free energy of formation of chukanovite and Pourbaix diagrams of iron in carbonated media10.1016/j.corsci.2012.01.033 ↗
38. Iron hydroxy carbonate formation in zerovalent iron permeable reactive barriers: characterization and evaluation of phase stability10.1016/j.jconhyd.2010.05.009 ↗
39. An in situ synchrotron radiation grazing incidence X-ray diffraction study of carbon dioxide corrosion10.1149/1.2007227 ↗
40. Fe(II) hydroxycarbonate Fe2(OH)2CO3 (chukanovite) as iron corrosion product: synthesis and study by Fourier Transform Infrared Spectroscopy10.1016/j.poly.2008.12.034 ↗
41. Anodic activation of iron corrosion in clay media under water-saturated conditions at 90°C: characterization of the corrosion interface10.1021/es9021987 ↗
42. Mechanism of long-term anaerobic corrosion of iron archaeological artefacts in seawater10.1016/j.corsci.2009.08.022 ↗
43. Corrosion of iron archaeological artefacts in soil: characterisation of the corrosion system10.1016/j.corsci.2004.05.029 ↗
44. Buried iron archaeological artefacts: corrosion mechanisms related to the presence of Cl-containing phases10.1016/j.corsci.2006.11.009 ↗
45. Factors affecting the amount of corroded iron converted into adherent rust in steels submitted to immersion tests10.1016/j.corsci.2010.04.005 ↗
46. A corrosion study of the ferrous medieval reinforcement of the Amiens cathedral. Phase characterisation and localisation by various microprobes techniques10.1016/j.corsci.2009.10.028 ↗
47. Vorkommen, Entstehung und Phasenumwandlung von β-FeOOH in Rost10.1002/maco.19690200205 ↗
48. The mechanisms of oxidation of ferrous hydroxychloride β-Fe2(OH)3Cl in aqueous solution: the formation of akaganeite vs goethite10.1016/S0010-938X(97)86102-1 ↗
49. On the formation of β-FeOOH (akaganéite) in chloride-containing environments10.1016/j.corsci.2006.06.003 ↗
50. Corrosion of press-hardened galvanized steel10.1016/j.corsci.2012.04.048 ↗
51. Assignment of Raman-active vibrational modes of tetragonal mackinawite: Raman investigations and ab-initio calculations10.1039/c4ra03442b ↗
52. W. Sun, Kinetics of iron carbonate and iron sulfide scale formation in CO2/H2 S corrosion, Ph.D. dlss Ohio University, Chemical and Biomolecular Engineering Department, 2006.
53. Equilibrium expressions related to the solubility of the sour corrosion product mackinawite10.1021/ie070750i ↗
54. Chemistry of iron sulphides10.1021/cr0503658 ↗
55. Localized corrosion of iron in alkaline sulfide solutions iron sulfide formation and the breakdown of passivity10.1149/1.2108602 ↗
56. A.R. Lennie, D.J. Vaughan, in: M.D. Dyar, C. McCammon, M.W. Schaefer (Eds.), Mineral Spectroscopy: A Tribute to Roger G. Burns, The Geochemical Society, Houston, 1996, p. 117.
57. M. Robert, J. Berthelin, Role of biological and biochemical factors in soil mineral weathering, in: P.M. Huaing, M. Schnitzer (Eds.), Interaction of Soil Minerals with Natural Organics and Microbes, Soil Sci. Soc. Am. Special Publication 17, Soil Science Society of America, Madison, 1986, pp. 453–496.10.2136/sssaspecpub17.c12 ↗
58. J. Ning, Y. Zheng, D. Young, B. Brown, S. Nesic, A thermodynamic study of hydrogen sulfide corrosion of mild stee, NACE International Corrosion Conference & Expo, Paper No. 2462, 2013.10.5006/C2013-02462 ↗
59. Green rusts in electrochemical and microbially influenced corrosion of steel10.1016/j.crte.2006.04.012 ↗
60. An electrochemical model for prediction of corrosion of mild steel in aqueous carbon dioxide solutions10.5006/1.3293640 ↗
61. Carbonic acid corrosion of steel10.5006/0010-9312-31.5.177 ↗
62. Studies of the corrosion mechanism of unalloyed steels in oxygen-free carbon dioxide solutions. Part I. Kinetics of the liberation of hydrogen10.1002/maco.19770281203 ↗
63. Effects of carbon dioxide on reactions at iron electrodes in aqueous salt solutions10.1016/0368-1874(84)83604-7 ↗
64. L.G.S. Gray, B.G. Anderson, M.J. Danysh, P.G. Tremaine, Mechanism of carbon steel corrosion in brines containing dissolved carbon dioxide at pH 4, corrosion/89, paper no. 464, Houston, TX: NACE International, 1989.10.5006/C1989-89464 ↗
65. M.R. Bonis, J.L. Crolet, Basics of the prediction of the risks of CO2 corrosion in oil and gas wells, CORROSION/89, paper no. 466, Houston, TX: NACE International, 1989.10.5006/C1989-89466 ↗
66. Fe3C influence on the corrosion rate of mild steel in aqueous CO2 systems under turbulent flow10.1016/S0010-938X(01)00141-X ↗
67. The influence of carbon steel microstructure on corrosion layers: an XPS and SEM characterization10.1016/S0169-4332(02)01218-7 ↗
68. Metal corrosion and argillite transformation at the water-saturated high-temperature iron-clay interface. A microscopic-scale study10.1016/j.apgeochem.2008.05.019 ↗
69. J.L. Palandri, Y.K. Kharaka, A compilation of rate parameters of water-mineral interaction kinetics for application to geochemical modeling, U.S. Geological survey, Open file report, 2004–1068.10.3133/ofr20041068 ↗