Microstructural evolution of coating-modified 3D C/SiC composites after annealing in wet oxygen at different temperatures
Source abstract
Abstract
National Natural Science Foundation of China [90405015, 50532010, 50672076, 50425208, 50642039]
The source flagged this abstract for review. Check formulas and completeness against the original publication.
Source: openaire · Quality: needs review · Source record ↗
Source flags: short_text
Source flags: short_text
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Ceramic matrix composites10.1098/rsta.1995.0048 ↗
2. Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
3. Relationship between high-temperature development of fibre–matrix interfaces and the mechanical behaviour of SiC–SiC composites10.1016/0266-3538(90)90099-Q ↗
4. Preparation and oxidation resistance of 2D C/SiC composites modified by partial boron carbide self-sealing matrix10.1016/j.msea.2008.08.022 ↗
5. Oxidation protection of multilayer CVD SiC/B/SiC coatings for 3D C/SiC composite10.1016/j.msea.2007.02.059 ↗
6. Oxidation protective multilayer CVD SiC coatings modified by a graphitic b–c interlayer for 3D C/SiC composite10.1007/s10443-006-9025-8 ↗
7. The oxidation behaviour of two- and three-dimensional C/SiC thermostructural materials protected by chemical-vapour-deposition polylayers coatings10.1007/BF00354562 ↗
8. Oxidation tests of carbonaceous composite materials protected by Si–B–C CVD coatings10.1016/0040-6090(94)90882-6 ↗
9. Oxidation behavior of 2D and 3D carbon/carbon thermostructural materials protected by CVD polylayer coatings10.1016/0040-6090(94)90783-8 ↗
10. Synthesis of highly tailored ceramic matrix composites by pressure-pulsed CVI10.1016/S0167-2738(01)00743-3 ↗
11. Oxidation-resistant carbon-fiber-reinforced ceramic-matrix composites10.1016/S0266-3538(98)00146-8 ↗
12. Self-healing mechanisms of a SiC fiber reinforced multi-layered ceramic matrix composite in high pressure steam environments10.1016/j.jeurceramsoc.2006.06.007 ↗
13. Preparation and oxidation protection of CVD SiC/a-BC/SiC coatings for 3D C/SiC composites10.1016/j.corsci.2009.01.026 ↗
14. Enhancement of the oxidation resistance of interfacial area in C/C composites. Part I: oxidation resistance of B–C, Si–B–C and Si–C coated carbon fibres10.1016/S0955-2219(01)00410-1 ↗
15. Enhancement of the oxidation resistance of interfacial area in C/C composites. Part II: oxidation resistance of B–C, Si–B–C and Si–C coated carbon preforms densified with carbon10.1016/S0955-2219(01)00411-3 ↗
16. Enhancement of the oxidation resistance of interfacial area in C/C composites. Part III: the effect of oxidation in dry or wet air on mechanical properties of C/C composites with internal protections10.1016/S0955-2219(01)00412-5 ↗
17. Influence of carbide coatings on the oxidation behaviour of carbon fibres10.1016/0008-6223(94)00170-5 ↗
18. Design of multilayer plasma-assisted CVD coatings for the oxidation protection of composite materials10.1016/0257-8972(95)02424-7 ↗
19. A global approach to fiber nD architectures and self-sealing matrices: from research to production10.1111/j.1744-7402.2005.02011.x ↗
20. Measurement of scratch-induced residual stress within SiC grains in ZrB2–SiC composite using micro-Raman spectroscopy10.1016/j.actamat.2008.07.031 ↗
21. Variation of the oxidation rate of silicon carbide with water-vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
22. Oxidation of silicon carbide in a wet atmosphere10.1007/BF01106816 ↗
23. Reactivity of a C/SiC composite in water vapour10.1016/S0955-2219(00)00207-7 ↗
24. N.J. Shaw, J.A. Dicarlo, N.S. Jacobson, S.R. Levine, J.A. Nesbitt, H.B. Probst, S.W.A. Anders, C.A. Stearns, Materials for Engine Applications Above 3000°F – An Overview, NASA TM-100169, 1987.
25. Mass spectrometric identification of Si–O–H(g) species from the reaction of silica with water vapor at atmospheric pressure10.1111/j.1151-2916.1997.tb02935.x ↗
26. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
27. Structure and vibrational properties of icosahedral B4C boron carbide10.1103/PhysRevLett.83.3230 ↗
28. Lattice dynamics of icosahedral a-boron under pressure10.1103/PhysRevLett.78.693 ↗
29. FT-Raman spectra of isotope-enriched boron carbide10.1016/j.jssc.2003.04.004 ↗
30. Raman spectra of K2O–B2O3 glasses and melts10.1016/S0022-3093(01)00752-9 ↗
31. FT-IR and Raman spectroscopic studies on B2O3–PbO–Ag2O glasses doped with manganese ions10.1016/j.solidstatesciences.2007.07.006 ↗
32. Study of the TiO2–H2O–B2O3 ternary system at 7.7 GPa and high temperatures10.1021/cm0103242 ↗
33. Raman study of B2O3–SrO–CuO glasses10.1016/S0924-2031(01)00184-9 ↗
34. High temperature oxidation of boron nitride. Part I. Monolithic boron nitride10.1111/j.1551-2916.1999.tb20075.x ↗
35. High temperature oxidation of boron nitride. Part II. BN layers in composites10.1111/j.1151-2916.1999.tb01944.x ↗
36. Effects of high water vapor pressures on the oxidation of SiC-based fiber-reinforced composites10.4028/www.scientific.net/MSF.369-372.385 ↗
37. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
38. The influence of an interphase on the deflection of a matrix crack in a ceramic-matrix composite10.1016/S0266-3538(01)00143-9 ↗
39. Improvement of mechanical properties of SiC/SiC composites by various surface treatments of fiber10.1016/S0022-3115(00)00678-4 ↗
40. The concept of a strong interface applied to SiC/SiC composites with a BN interphase10.1016/S1359-6454(00)00247-0 ↗
41. TEM structure of (PyC/SiC)n multilayered interphases in SiC/SiC composites10.1016/S0955-2219(99)00086-2 ↗
42. Kinetic monte carlo simulations of C diffusion on 3×3 β-SiC(111) based on ab initio calculations10.1016/j.cpc.2005.03.013 ↗