journal article·2007-02Open access

Effects of blending on surface characteristics of copper corrosion products in drinking water distribution systems

Weizhong Xiao, Seungkwan Hong, Zhijian Tang, Sudipta Seal, James S. Taylor

Corrosion Science· Volume 49· Issue 2

Abstract

Abstract Copper scales formed over 6-months during exposure to ground, surface and saline waters were characterized by EDS, XRD and XPS. Scale color and hardness were light red–brown–black/hard for high alkalinity and blue–green/soft for high SO 4 or Cl waters. Cl was present in surface or saline copper scales. The Cu/Cu 2 O ratio decreased with time indicating an e transfer copper corrosion mechanism. Cu 2 O, CuO, and Cu(OH) 2 dominated the top 0.5–1 A° scale indicating continuous corrosion. Cu 2 O oxidation to CuO increased with alkalinity, and depended on time and pH. Total copper release was predicted using a Cu(OH) 2 model.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Water Treatment and Disinfection · Water Systems and Optimization · Urban Stormwater Management Solutions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (22)

Show source-provided references
1. Thermographic study of the dehydration of copper hydroxide in alkaline solutions
2. Mechanism of aging of individual metal hydroxides and hydroxide systems
3. Solubility constants of metal oxides, metal hydroxides, and metal hydroxide salts in aqueous solution10.1351/pac196306020125 ↗
4. Corrosion in drinking water distribution systems: a major contributor of copper and lead to wastewater and effluent10.1021/es970185i ↗
5. Wieckowski · 1999
6. Alkaline prediction and aging of copper from dilute cupric nitrite10.1021/es00022a016 ↗
7. Preparation and properties of monodispersed colloidal metal hydrous oxides10.1351/pac197850091193 ↗
8. The corrosion behavior of copper in neutral tap water part I: corrosion mechanisms10.1016/0010-938X(96)00110-2 ↗
9. Hamann · 1998
10. Jones · 1995
11. American Water Works Association Research Foundation, Internal Corrosion of Water Distribution Systems, second ed., DVGW-TZW, Denver, CO, 1996.
12. Pankow · 1991
13. Copper corrosion in drinking water distribution systems—the influence of water quality10.1016/S0010-938X(97)00026-7 ↗
14. On the corrosion of copper in pure water10.1016/0010-938X(89)90071-1 ↗
15. R.S. Michael, A.L. Darren, Effect of pH, DIC, orthophosphate and sulfate on drinking water cuprosolvency. EPA/600/R-95/085 1995.
16. Alkalinity, pH, and copper corrosion by-product release10.1002/j.1551-8833.1996.tb06521.x ↗
17. Surface characterization of artificial corrosion layers on copper alloy reference materials10.1016/S0169-4332(02)00005-3 ↗
18. Role of temperature and pH in Cu(OH)2 solubility10.1021/es981121q ↗
19. Alkaline precipitation and aging of Cu(II) in the presence of sulfate10.1016/0043-1354(94)00286-G ↗
20. Copper corrosion by-product release in long-term stagnation experiments10.1016/S0043-1354(01)00366-9 ↗
21. Standard Methods for the Examination of Water and Wastewater, 18th ed., APHA–AWWA–WPCF Washington, DC, 1999.
22. On the nature of the use of adventitious carbon as binding energy standard10.1116/1.579868 ↗