journal article·2025-04

High-temperature self-healing CoCrWSi coating based on defect-filling and pinning effects

Wenlang Huang, Dehao Kong, Nadimullah Hakimi, Xuekui Qian, Kaibo Zhu, Saixiang Zhao, Junlin Wang, Biju Zheng, Taihong Huang, Peng Song

Corrosion Science· Volume 245
Publisher page

Abstract

Co-29Cr-7W-5Si (wt%) was prepared via high-velocity oxygen-fuel system. Its oxidation behavior at 1100 °C in air containing water vapour was investigated. The oxidation kinetics of the coatings for 150 h was established using classical oxidation theory. After multiple cycles of thermal shock oxidation followed by water quenching, a dense Cr 2O 3 protective layer was formed on the surface of the coating, beneath which a SiO 2 pinning layer was generated. Although this significantly enhanced its oxidation resistance, longitudinal cracks occurred because of thermal stress. After 144 cycles, the cracks underwent filling-type self-healing owing to rapid diffusion and oxidation.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Development of strong, oxidation and corrosion resistant nickel-based superalloys: critical review of challenges
2. Oxidation and hot corrosion behavior of nickel-based superalloy for gas turbine applications10.1080/10426914.2014.901530 ↗
3. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
4. Rare earth effect on the microstructure and wear resistance of Ni-based coatings10.1016/j.msea.2006.11.034 ↗
5. Corrosion resistance of CoCrW coatings obtained by electrodeposition10.1007/s10008-018-3929-8 ↗
6. Microstructural features and mechanical properties of a cobalt-based laser coating10.1016/S1359-6454(96)00250-9 ↗
7. Microstructure and phase analyses of Stellite 6 plus 6 wt% Mo alloy10.1016/S0924-0136(97)00027-7 ↗
8. Properties of HVOF-sprayed Stellite-6 coatings10.1016/j.surfcoat.2018.01.078 ↗
9. Powder injection molding of Stellite 6 powder: sintering, microstructural and mechanical properties10.1016/j.msea.2015.11.058 ↗
10. Assessing the kinetics and mechanisms of corrosion of cast and HIPed Stellite 6 in aqueous saline environments10.1016/j.corsci.2004.09.011 ↗
11. Sliding wear of blended cobalt based alloys
12. Friction and wear properties of UHMWPE composites reinforced with carbon fiber10.1016/j.matlet.2004.09.011 ↗
13. A comparative study on Ni-based coatings prepared by HVAF, HVOF, and APS methods for corrosion protection applications10.1007/s11666-016-0474-9 ↗
14. Diffusion of multi-principal elements through stable Cr2O3 and Al2O3 scales10.1016/j.mtla.2022.101497 ↗
15. Carburization susceptibility of chromia-forming alloys in high-temperature CO210.1016/j.corsci.2022.110488 ↗
16. High-temperature oxidation behaviour of CoCrNi medium-entropy alloy10.1016/j.corsci.2020.108755 ↗
17. High-entropy FeNiCoCr alloys with improved mechanical and tribological properties by tailoring composition and controlling oxidation10.1016/j.jmst.2020.12.042 ↗
18. Molecular-scale investigation of the oxidation behavior of chromia-forming alloys in high-temperature CO210.1038/s41529-021-00194-1 ↗
19. Oxidation of a chromia-forming nickel base alloy at high temperature in mixed diluted CO/H2O atmospheres10.1016/j.corsci.2009.01.019 ↗
20. Effects of Ni and Cr on the high-temperature oxidation behavior and mechanisms of Co-and CoNi-base superalloys10.1016/j.matdes.2022.111291 ↗
21. Surface characterisation of Ni-free Co-Cr-W-based dental alloys exposed to high temperatures and the effects of adding silicon10.1016/j.corsci.2015.02.030 ↗
22. Multi-spectroscopic analysis of high temperature oxides formed on cobalt-chrome-molybdenum alloys10.1016/j.jmrt.2022.08.071 ↗
23. Effect of Si content of CrSi-based coatings on their oxidation resistance in high temperature air10.1016/j.ceramint.2020.01.165 ↗
24. Effect of Si addition to improve the performance of type II and type I hot corrosion resistance of aluminide coating10.1016/j.corsci.2022.110937 ↗
25. Corrosion behaviour of Fe-25Cr alloy in wet CO2 gas at 650 ℃: Effects of chloride deposits and Si+Mn alloying addition10.1016/j.corsci.2021.110001 ↗
26. Influence of Si on microstructures and high-temperature properties of MCrAlY type coating10.1016/S1875-5372(18)30204-2 ↗
27. Porosity of electrodeposited coatings: its cause, nature, effect and management10.1515/CORRREV.1992.10.3-4.217 ↗
28. Effect of processing parameters on MCrAlY bondcoat roughness and lifetime of APS-TBC systems10.1016/j.surfcoat.2014.06.075 ↗
29. Failure aspects of thermal barrier coatings10.1179/mht.2001.027 ↗
30. Oxide scale adhesion and impurity segregation at the scale/metal interface10.1007/BF00665658 ↗
31. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
32. Calculations of parabolic reaction rate constants10.1007/BF00667057 ↗
33. Growth rates of alumina scales on Fe-Cr-Al alloys10.1023/B:OXID.0000016274.78642.ae ↗
34. Young · 2008
35. Correlation between the microstructure, growth mechanism, and growth kinetics of alumina scales on a FeCrAlY alloy10.1007/s11661-007-9342-z ↗
36. The isothermal oxidation of Co-Cr alloys in 760 Torr oxygen at 1000 ℃10.1007/BF00606542 ↗
37. Development of new Co-Cr-W-based biomedical alloys: effects of microalloying and thermomechanical processing on microstructures and mechanical properties10.1016/j.matdes.2013.10.052 ↗
38. High-temperature oxidation of Co-10 w/o Cr alloys: I. microstructure of oxide scales10.1149/1.2411802 ↗
39. High temperature oxidation of Co-10 w/o Cr alloys: II. oxidation kinetics10.1149/1.2411803 ↗
40. The Scherrer formula for X-ray particle size determination10.1103/PhysRev.56.978 ↗
41. Suryanarayana · 1998
42. The influence of manganese and silicon on the oxidation behavior of Co-20Cr10.1007/BF00603486 ↗
43. Effects of silicon on the oxidation behavior of Ni-base chromia-forming alloys10.1007/s11085-006-9003-4 ↗
44. CrO2(OH)2 volatilization rate and oxidation behavior prediction of the NiCr coating in air-H2O environment at 650 ℃10.1016/j.corsci.2021.109303 ↗
45. The oxidation of silicon carbide at 1150 to 1400 ℃ and at 9× 10−3 to 5× 10−1 torr oxygen pressure10.1149/1.2423812 ↗
46. Passivity during the oxidation of silicon at elevated temperatures10.1063/1.1723429 ↗
47. Passivity and inhibition during the oxidation of metals at elevated temperatures10.1016/S0010-938X(65)80003-8 ↗
48. R.I. Jaffee, N.E. Promisel, The Science, Technology and application of titanium: proceedings of an international conference organized by the institute of metals, the Metallurgical Society of Aime, and the American Society for Metals in Association with the Japan Institute of Metals and the Academy of Sciences, USSR, and Held at th, Elsevier, 2013.
49. Engineering, Effect of Si on hot corrosion resistance of CoCrAlY coating10.1016/S1875-5372(18)30011-0 ↗
50. Characterization of oxide films on wrought Co-Cr-Mo-xSi alloys exposed to high-temperature oxidation10.1016/j.corsci.2021.109753 ↗
51. Effect of Si addition on microstructures and oxidation behavior of CoCrW alloy prepared by spark plasma sintering10.1016/j.corsci.2023.111011 ↗
52. Thermodynamics and phase stability in the Si-O system10.1016/j.jnoncrysol.2003.12.057 ↗
53. A Model for stress generation and relief in Oxide-Metal systems during a temperature change10.1007/BF00665449 ↗
54. On the formation of porosity and microchannels in growing scales10.1007/BF00657061 ↗
55. Kofstad · 1988