Abstract

The vital role of hydrogen on lead-induced localized corrosion of Alloy 690TT in the simulated secondary crevice chemistries of pressurized water reactor at 25 °C is investigated by using surface analysis techniques and calculations. Density functional theory (DFT) calculation reveals that there is a coupling effect between lead and hydrogen on inhibiting the kinetic diffusion of oxygen vacancies. Experimental results show that hydrogen causes the change of most easily-corroded location from the grain/carbide interface to the TiN/nucleus interface in the lead-induced corrosion process, which provides a new interpreting sight as for lead-induced stress corrosion cracking mode of nickel-based Alloys.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Quantitative assessment of submodes of stress corrosion cracking on the secondary side of steam generator tubing in pressurized water reactors: part 310.5006/1.3287716 ↗
2. Transgranular SCC mechanism of thermally treated alloy 600 in alkaline water containing Pb10.1016/j.corsci.2007.03.040 ↗
3. SCC mechanism of Ni base alloys in Pb contaminated water
4. Effect of lead on Inconel 600 and Incoloy 800 oxide layers formed in simulated steam generator secondary environments10.1016/S0029-5493(97)85102-3 ↗
5. The mode of stress corrosion cracking in Ni-base alloys in high temperature water containing Pb10.1016/S0022-3115(99)00111-7 ↗
6. Correlation between film rupture ductility and PbSCC of alloy 80010.1016/j.electacta.2007.12.070 ↗
7. The mechanism of stress corrosion cracking of Alloy 690TT in a caustic solution containing lead10.1016/j.corsci.2017.09.015 ↗
8. On the nanomechanical characteristics of thermally-treated alloy 690: grain boundaries versus grain interior10.1016/j.jallcom.2013.08.044 ↗
9. The role of TiN inclusions in stress corrosion crack initiation for Alloy 690TT in high-temperature and high-pressure water10.1016/j.corsci.2009.11.015 ↗
10. Effects of lead on oxidation behavior of Alloy 690TT within a high temperature aqueous environment10.1016/j.apsusc.2017.07.201 ↗
11. Cavitation erosion behavior of inconel 690 alloy10.1016/j.msea.2007.12.007 ↗
12. CS-AFM study on Pb-induced degradation of passive film on nickel-based alloy in high temperature and high pressure water10.1016/j.corsci.2018.08.054 ↗
13. Investigation of passive films on nickel Alloy 690 in Pb-containing environments10.1016/j.jnucmat.2008.06.037 ↗
14. Effects of pH on Pb-induced passivity degradation of nuclear steam generator tubing alloy in high temperature crevice chemistries10.1016/j.electacta.2012.10.006 ↗
15. Passivity degradation of nuclear steam generator tubing alloy induced by Pb contamination at high temperature10.1016/j.jnucmat.2012.06.021 ↗
16. A mechanistic study on Pb-induced passivity-degradation of nickel-based alloy10.1149/1.2741204 ↗
17. Trans-twins stress corrosion cracking behaviors of Alloy 690TT in Pb-containing caustic solution at 330°C10.1016/j.nucengdes.2011.09.025 ↗
18. Effects of hydrogen on the anodic behavior of Alloy 690 at 60 °C10.1016/j.corsci.2009.11.039 ↗
19. States and transport of hydrogen in the corrosion process of an AZ91 magnesium alloy in aqueous solution10.1016/j.corsci.2008.01.028 ↗
20. Effect of hydrogen in Inconel Alloy 600 on corrosion in high temperature oxygenated water10.1016/j.corsci.2009.11.037 ↗
21. Effects of hydrogen on pitting susceptibility of type 310 stainless steel10.5006/1.3287639 ↗
22. Effect of hydrogen on pitting susceptibility of 2507 duplex stainless steel10.1016/j.corsci.2013.01.022 ↗
23. Hydrogen and chloride ions effects on the automobile interstitial-free steel corrosion10.5006/1126 ↗
24. Role of hydrogen in stress corrosion cracking of austenitic stainless steels10.1080/14786435.2010.515262 ↗
25. First-principles investigation of hydrogen interaction with TiC precipitates in α-Fe10.1103/PhysRevB.93.184108 ↗
26. New knowledge on localized corrosion obtained from local measuring techniques10.1016/S0013-4686(01)00642-9 ↗
27. Local potential measurements with the SKPFM on aluminium alloys10.1016/j.electacta.2004.01.045 ↗
28. Characterization of cast AlSi (Cu) alloys by scanning Kelvin probe force microscopy10.1016/j.electacta.2006.03.027 ↗
29. Volta potential of second phase10.1016/j.electacta.2005.10.010 ↗
30. Integrated AFM and SECM for in situ studies of localized corrosion of Al alloys10.1016/j.electacta.2006.12.073 ↗
31. Characterization of AA2024-T3 by scanning kelvin probe force microscopy10.1149/1.1838633 ↗
32. Corrosion study of AA2024-T3 by scanning kelvin probe force microscopy and in situ atomic force microscopy scratching10.1149/1.1838634 ↗
33. Characterization of corrosion interfaces by the scanning Kelvin probe force microscopy technique10.1149/1.1359199 ↗
34. Influence of dichromate ions on corrosion of pure aluminum and AA2024-T3 in NaCl solution studied by AFM scratching10.1149/1.1392659 ↗
35. Potential-pH diagrams for Pb adsorption on Cu and Ni surfaces at 25°C and 300°C10.1149/2.017303jes ↗
36. ToF-SIMS study of the behavior of thermally oxidized films formed on nickel-based 690 alloy in high temperature water10.1002/sia.5060 ↗
37. ToF-SIMS study of oxide films thermally grown on nickel-base alloys10.1016/j.corsci.2018.06.043 ↗
38. Potential-pH diagrams of Cr-H2O system at elevated temperatures10.1016/S1003-6326(10)60006-4 ↗
39. Electrochemical properties and growth mechanism of passive films on Alloy 690 in high-temperature alkaline environments10.1016/j.corsci.2010.06.016 ↗
40. Prevent hydrogen damage in α-Cr2O3 / α-Fe2O3 (0001) interface10.1016/j.apsusc.2018.12.272 ↗
41. The history of the point defect model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
42. Oxide properties and stress corrosion cracking behaviour for Alloy 600 in leaded caustic solutions at high temperature10.1016/j.corsci.2010.12.016 ↗
43. Migration of ion vacancy in hydroxylated oxide film formed on Cr: a density functional theory investigation10.1021/jp309898c ↗
44. Dependence of electron work function of Al-Mg alloys on surface structures and relative humidity10.1016/j.physb.2011.08.017 ↗
45. Changes in surface morphology and work function caused by corrosion in aluminum alloys10.1016/j.jpcs.2012.01.025 ↗
46. A study on the kinetic response of the electron work function to wear10.1016/S0043-1648(03)00153-4 ↗
47. Relation between an atomic electronegativity scale and the work function10.1147/rd.221.0072 ↗
48. Correlation of photosensitive electrode properties with electronegativity10.1016/0009-2614(77)80027-4 ↗
49. The absolute energy positions of conduction and valence bands of selected semiconducting minerals10.2138/am-2000-0416 ↗
50. Photo-electrochemical analysis of passive film formed on Cr in pH 8.5 buffer solution10.1016/S0013-4686(01)00729-0 ↗
51. Effect of hydrogen on semiconductive properties of passive film on ferrite and austenite phases in a duplex stainless steel10.1038/s41598-017-03480-8 ↗
52. Band gap widening of nanocrystalline nickel oxide thin films via phosphorus doping10.1016/j.physe.2009.11.047 ↗
53. Effects of addition of different carbon materials on the electrochemical performance of nickel hydroxide electrode10.1016/j.jpowsour.2009.12.094 ↗
54. C. Elsasser. First-principles investigation of hydrogen interaction with TiC precipitates in α-Fe10.1103/PhysRevB.93.184108 ↗
55. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
56. The detrimental effect of hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-C-X alloys: an experimental proof of the HELP mechanism10.1016/j.ijhydene.2017.12.109 ↗
57. Atomic-scale investigation of deep hydrogen trapping in NbC/α-Fe semi-coherent interfaces10.1016/j.actamat.2020.09.031 ↗
58. Hydrogen in chromium: influence on the high-temperature oxidation kinetics in O2, oxide-growth mechanisms, and scale adherence10.1023/A:1018866505708 ↗
59. The role of titanium in the pitting corrosion of commercial stainless steels10.5006/1.3582048 ↗
60. Effects of heat-treatment on the extent of chromium depletion and caustic corrosion resistance of alloy 69010.1016/j.corsci.2006.05.043 ↗