journal article·2026-04

Corrosion behavior of AA2024 aluminum alloy manufactured by solid state additive manufacturing – Additive friction stir deposition

Ziyu Li, Dawei Guo, Hongchang Qian, Dawei Zhang, Zhongyu Wu, Qian Qiao, Lap Mou Tam, Chi Tat Kwok

Corrosion Science· Volume 262
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Additive Manufacturing Materials and Processes · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Recent developments in additive friction stir deposition (AFSD)10.1016/j.jmrt.2024.04.179 ↗
2. Friction stir additive manufacturing – An innovative tool to enhance mechanical and microstructural properties10.1016/j.mseb.2020.114832 ↗
3. Solid-State Metal Additive Manufacturing for Structural Repair10.1021/accountsmr.1c00098 ↗
4. Recent progress on the additive manufacturing of aluminum alloys and aluminum matrix composites: Microstructure, properties, and applications10.1016/j.ijmachtools.2023.104047 ↗
5. Review on laser directed energy deposited aluminum alloys10.1088/2631-7990/ad16bb ↗
6. Solid-state additive manufacturing of aluminum and copper using additive friction stir deposition: Process-microstructure linkages10.1016/j.mtla.2020.100967 ↗
7. Additive friction stir deposition of metallic materials: Process, structure and properties10.1016/j.matdes.2023.112356 ↗
8. Experimental and numerical analysis of friction stir additive manufacturing of 2024 aluminium alloy
9. In situ investigation into temperature evolution and heat generation during additive friction stir deposition: A comparative study of Cu and Al-Mg-Si
10. Friction stir welding of high-strength aerospace aluminum alloy and application in rocket tank manufacturing10.1016/j.jmst.2017.11.041 ↗
11. Effect of pulsed current welding on mechanical properties of high strength aluminum alloy10.1007/s00170-006-0848-0 ↗
12. Microstructure and mechanical properties of 600 MPa grade ultra-high strength aluminum alloy fabricated by wire-arc additive manufacturing10.1016/j.jmst.2022.12.007 ↗
13. Review of high-strength aluminium alloys for additive manufacturing by laser powder bed fusion10.1016/j.matdes.2022.110779 ↗
14. Microstructure and corrosion of AA202410.1515/corrrev-2014-0039 ↗
15. A closer look at constituent induced localised corrosion in Al-Cu-Mg alloys10.1016/j.corsci.2016.10.018 ↗
16. Sheet AA2024-T3: a new investigation of microstructure and composition10.1002/sia.3163 ↗
17. High Strength Al-Alloys: Microstructure, Corrosion and Principles of Protection
18. Corrosion of AA2024-T3 Part I: Localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
19. Stable pit formation on AA2024-T3 in a NaCl environment10.1016/j.corsci.2009.08.043 ↗
20. Morphological and microstructural investigation of the non-planar interface formed in solid-state metal additive manufacturing by additive friction stir deposition
21. Additive friction stir deposition of an Al-Cu-Mg alloy: Microstructure evolution and mechanical properties10.1016/j.matchar.2024.114562 ↗
22. A comparative study of machine learning in predicting the mechanical properties of the deposited AA6061 alloys via additive friction stir deposition
23. Time–frequency methods for trend removal in electrochemical noise data10.1016/j.electacta.2012.03.062 ↗
24. Technical Note: Localization Index Obtained from Electrochemical Noise Analysis10.5006/1.3283926 ↗
25. Electrochemical noise analysis (ENA) for active and passive systems in chloride media10.1016/S0013-4686(01)00643-0 ↗
26. Electrochemical noise: a review of experimental setup, instrumentation and DC removal10.1134/S1023193515070071 ↗
27. Detection of corrosion degradation using electrochemical noise (EN): review of signal processing methods for identifying corrosion forms
28. Application of transient analysis using Hilbert spectra of electrochemical noise to the identification of corrosion inhibition10.1016/j.electacta.2013.11.084 ↗
29. An integrated approach in the time, frequency and time-frequency domain for the identification of corrosion using electrochemical noise10.1016/j.electacta.2016.11.018 ↗
30. Evaluation of the formation and protectiveness of a lithium-based conversion layer using electrochemical noise10.1016/j.electacta.2022.140733 ↗
31. A Review of Wavelet Analysis and Its Applications: Challenges and Opportunities10.1109/ACCESS.2022.3179517 ↗
32. The Effect of Ambient Ageing on the Corrosion Protective Properties of a Lithium-Based Conversion Layer
33. A critical review of electrochemical noise measurement as a tool for evaluation of organic coatings
34. EN, EIS and polarization studies to evaluate the inhibition effect of 3H-phenothiazin-3-one, 7-dimethylamin on mild steel corrosion in 1M HCl solution10.1016/j.corsci.2008.09.022 ↗
35. Interpretation of Electrochemical Noise Data10.5006/1.3290350 ↗
36. How complex is the microstructure of AA2024-T3?10.1016/j.corsci.2009.05.001 ↗
37. Comparison of Constituent Intermetallic Particles in Different Aluminium Alloys10.1007/s13632-025-01170-w ↗
38. Computer simulations of realistic microstructures of coarse constituent particles in a hot-rolled aluminum alloy10.1016/j.commatsci.2005.11.011 ↗
39. Microconstituent-Induced Pitting Corrosion in Aluminum Alloy 2024-T310.5006/1.3292099 ↗
40. Nano-scale dissolution phenomena in Al–Cu–Mg alloys, Electrochemistry Communications 10 (2008) 32–37. https://doi.org/10.1016/j.elecom.2007.10.032.10.1016/j.elecom.2007.10.032 ↗
41. Size-dependent role of S phase in pitting initiation of 2024Al alloy10.1016/j.corsci.2016.01.016 ↗
42. A machine learning strategy to achieve dual-synchronous property improvement of aviation Al-Cu-Mg alloy10.1016/j.jmst.2025.04.036 ↗
43. Observations of intergranular corrosion in AA2024-T351: The influence of grain stored energy10.1016/j.corsci.2012.04.005 ↗
44. Microstructure and localized corrosion properties of 2219 aluminum alloy manufactured by additive friction stir deposition10.1016/j.corsci.2024.112508 ↗
45. Effect of joining material direction on material flow, microstructure and mechanical properties of dissimilar AA2024/7075 joints fabricated by friction stir welding, Journal of Materials Research and Technology 35 (2025) 3679–3692. https://doi.org/10.1016/j.jmrt.2025.02.007.10.1016/j.jmrt.2025.02.007 ↗
46. In-situ nanoscopic observations of dealloying-driven local corrosion from surface initiation to in-depth propagation10.1016/j.corsci.2020.108912 ↗
47. Simulating corrosion of Al2CuMg phase by measuring ionic currents, chloride concentration and pH10.1016/j.corsci.2014.07.021 ↗
48. When all intermetallics dealloy in AA2024-T3: Quantifying early stage intermetallic corrosion kinetics under immersion10.1016/j.corsci.2021.109836 ↗
49. Dealloying-driven local corrosion by intermetallic constituent particles and dispersoids in aerospace aluminium alloys10.1016/j.corsci.2020.108947 ↗
50. The Study of AA2024 De-Alloying Using Luminol Electrogenerated Chemiluminescence Imaging10.1149/2.0481911jes ↗
51. Corrosion of AA2024-T3 Part II: Co-operative corrosion10.1016/j.corsci.2010.09.030 ↗
52. Corrosion of AA2024-T3 Part III: Propagation10.1016/j.corsci.2010.09.035 ↗
53. Galvanic coupling between AA7075-T6 and AA2024-T3 intensifies local corrosion10.1016/j.electacta.2025.147335 ↗
54. An integral non-intrusive electrochemical and in-situ optical technique for the study of the effectiveness of corrosion inhibition10.1016/j.electacta.2021.139619 ↗
55. Electrochemical Characteristics of Intermetallic Phases in Aluminum Alloys: An Experimental Survey and Discussion10.1149/1.1869984 ↗
56. On the corrosion of additively manufactured aluminium alloy AA2024 prepared by selective laser melting, Corrosion Science 143 (2018) 93–106. https://doi.org/10.1016/j.corsci.2018.08.019.10.1016/j.corsci.2018.08.019 ↗
57. Corrosion behavior of 650 MPa high strength low alloy steel in industrial polluted environments containing different concentrations of Cl−10.1007/s12613-025-3135-5 ↗
58. Improving forming quality and corrosion resistance of CMT-P additive manufactured 2024 aluminum alloy using assisted laser10.1016/j.jmapro.2024.06.071 ↗
59. The corrosion behavior and mechanical properties of 5083 Al-Mg alloy manufactured by additive friction stir deposition10.1016/j.corsci.2023.110972 ↗