An inclusion modification approach to improve hydrogen embrittlement resistance: Trace Mg addition facilitating MnS dispersion for enhanced deep hydrogen trapping
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (78)
Show source-provided references
1. Enhancing hydrogen embrittlement resistance through chemical heterogeneity in austenite of medium Mn steel10.1016/j.corsci.2025.112857 ↗
2. Evolution and mechanism of hydrogen gas embrittlement susceptibility for X80 pipeline steel within the service temperature range10.1016/j.corsci.2025.112928 ↗
3. Investigating the correlation of microstructure with stress corrosion cracking of the high-temperature heat treated 2205 duplex stainless steel10.1016/j.jmrt.2025.02.212 ↗
4. An extended engineering critical assessment for corrosion fatigue of subsea pipeline steels10.1016/j.engfailanal.2017.11.012 ↗
5. A novel approach for estimating hydrogen uptake and diffusion coefficient10.1016/j.ijhydene.2025.02.400 ↗
6. A comparative study on the passive film and SCC behavior of Ti-6Al-3Nb-2Zr-1Mo alloy at various test temperatures in simulated seawater10.1016/j.corsci.2024.112066 ↗
7. A novel understanding of dislocation density effect on the corrosion resistance of 316L stainless steel with passive film nucleation growth kinetic calculation10.1016/j.corsci.2025.112810 ↗
8. Unveiling the environmentally assisted cracking behavior of rails in industrial railway applications and the strategies for improvement via vanadium-microalloying10.1016/j.conbuildmat.2025.140334 ↗
9. Probing into the fundamental effect of Cr on the failure mechanisms of rebars within carbonation and stress environments
10. Hydrogen embrittlement in different materials: a review10.1016/j.ijhydene.2018.09.201 ↗
11. Effect of non-metallic inclusions on hydrogen-induced cracking of API5L X100 steel10.1016/j.ijhydene.2010.05.089 ↗
12. Effect of submicron-scale MnS inclusions on hydrogen trapping and HIC susceptibility of X70 pipeline steels10.1002/srin.201700566 ↗
13. New insights into the mechanism of localised corrosion induced by TiN-containing inclusions in high strength low alloy steel10.1016/j.jmst.2021.12.075 ↗
14. Finite element modeling of HIC propagation in pipeline steel with regard to experimental observations10.1016/j.ijhydene.2020.06.054 ↗
15. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
16. Influence of electrochemical hydrogenation parameters on microstructures prone to hydrogen-induced cracking10.1016/j.jngse.2022.104533 ↗
17. The effects of inclusions and second phase particles on hydrogen-induced blistering in iron10.1016/j.matchemphys.2007.07.004 ↗
18. Effects of manganese and chromium on sulfide stress cracking in 125 ksi grade high-strength low-alloyed steel for oil country tubular goods10.1016/j.corsci.2025.112718 ↗
19. Sequential kinetic analysis of the influences of non-metallic inclusions on hydrogen diffusion and trapping in high-strength pipeline steel with Al-Ti deoxidisation and Mg treatment10.1016/j.corsci.2021.110006 ↗
20. Corrosion behavior of 650 MPa high strength low alloy steel in industrial polluted environment containing different concentration of Cl
21. Prevention of hydrogen embrittlement in steels10.2355/isijinternational.ISIJINT-2015-430 ↗
22. Role of Te-RE alloying on the passive film and pitting corrosion behavior of 316L stainless steel10.1016/j.corsci.2024.112457 ↗
23. A strategy to overcome the negative effect of Mg treatment on localized corrosion and enhance the performance of high-nitrogen martensitic stainless steel by Mg&Ce composite treatment10.1016/j.corsci.2025.112852 ↗
24. Improving hydrogen induced cracking resistance of high strength acid-resistant submarine pipeline steels via trace-Mg treatment10.1016/j.ijhydene.2022.12.322 ↗
25. Evolution of Al2O3 inclusions by magnesium treatment in H13 hot work die steel10.1080/03019233.2016.1165498 ↗
26. Effect of Ca-Mg microalloying on corrosion behavior and corrosion resistance of low alloy steel in the marine atmospheric environment10.1016/j.corsci.2024.112134 ↗
27. Morphology study on inclusion modifications using Mg–Ca treatment in resulfurized special steel10.3390/ma12020197 ↗
28. Comparative study of non-metallic inclusions on the critical size for HIC initiation and its influence on hydrogen trapping10.1016/j.ijhydene.2020.02.131 ↗
29. Numerical study on hydrogen permeation of ferritic steel evaluated under constant load10.1080/02670836.2016.1162001 ↗
30. Role of texture and inclusions on the failure of an API X70 pipeline steel at different service environments10.1016/j.matchar.2020.110330 ↗
31. Direct observation of hydrogen evolution in the electron microscope scale10.1016/0036-9748(82)90377-5 ↗
32. Improvement of the hydrogen microprint technique on AHSS steels10.1007/s13632-012-0015-y ↗
33. Mechano-electrochemical interaction of high-strength pipeline steels with Al-Ti deoxidization and Mg-Ca compound treatment10.1016/j.corsci.2023.111534 ↗
34. High-resolution Kelvin probe microscopy in corrosion science: scanning Kelvin probe force microscopy (SKPFM) versus classical scanning Kelvin probe (SKP)10.1016/j.electacta.2007.03.016 ↗
35. Kelvin probe force microscopy and its application10.1016/j.surfrep.2010.10.001 ↗
36. Scanning Kelvin probe as a highly sensitive tool for detecting hydrogen permeation with high local resolution10.1016/j.elecom.2011.10.014 ↗
37. Understanding the non-steady electrochemical mechanism on SCC of 304 SS under applied polarization potentials10.1016/j.corsci.2023.111686 ↗
38. Uncoupling chloride and acidification attack on the naturally formed corrosion scales10.1016/j.corsci.2022.110207 ↗
39. First-principles investigation of hydrogen interaction with TiC precipitates in a-Fe10.1103/PhysRevB.93.184108 ↗
40. Effects of Mg-Al-O-Mn-S inclusion on the nucleation of acicular ferrite in magnesium-containing low-carbon steel10.1016/j.matchar.2018.05.005 ↗
41. Influences of (Al, Ca, Si, Nb, Mn)-oxy-sulfide inclusions on corrosion degradation for newly designed 17–4 martensitic PH steel in simulated geothermal environments10.1016/j.corsci.2024.112279 ↗
42. Solidification of iron and steel on single-crystal oxide10.2355/isijinternational.47.847 ↗
43. Hydrogen permeation behavior at different positions in the normal direction of X42 and X52 pipeline steels10.1016/j.ijhydene.2024.05.479 ↗
44. Scanning probe microscopy of thermal conductivity and subsurface properties10.1063/1.108207 ↗
45. Hydrogen detection in metals: a review and introduction of a Kelvin probe approach10.1088/1468-6996/14/1/014201 ↗
46. The finding of hydrogen trapping at phase boundary in austenitic stainless steel by scanning Kelvin probe force microscopy10.1016/j.scriptamat.2018.11.020 ↗
47. In-Situ synchrotron investigation of elastic and tensile properties of oxide dispersion strengthened EUROFER97 steel for advanced fusion reactors10.1016/j.actamat.2024.119876 ↗
48. Crystallographic analysis of isothermally transformed bainite in 0.2C–2.0Mn–1.5Si–0.6Cr steel using EBSD10.1016/j.jmst.2013.01.015 ↗
49. On the role of crystallographic texture in mitigating hydrogen-induced cracking in pipeline steels10.1016/j.corsci.2011.08.031 ↗
50. Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing10.1016/j.corsci.2016.05.003 ↗
51. A review of strain analysis using electron backscatter diffraction10.1017/S1431927611000055 ↗
52. Investigate on dissimilar welding of high-entropy alloy and 310S with various fillers10.1016/j.matdes.2024.113454 ↗
53. Influence of different heat-affected zone microstructures on the stress corrosion behavior and mechanism of high-strength low-alloy steel in a sulfurated marine atmosphere10.1016/j.msea.2019.05.024 ↗
54. Improving the resistance of high-strength steel to SCC in a SO2-polluted marine atmosphere through Nb and Sb microalloying10.1016/j.corsci.2020.108693 ↗
55. Transverse crack micromechanisms in high-strength steel weld metal with microstructure heterogeneity under hydrogen-containing environment10.1016/j.msea.2024.147132 ↗
56. Effect of HAGBs for ultra-high strength stainless steel on pitting/microcrack initiation with synergy between strain and corrosion environment10.1016/j.jmst.2024.12.077 ↗
57. Enhancing sulfide stress cracking resistance of a Cu-bearing high strength low alloyed steel through decreasing austenitizing temperature10.1016/j.jmrt.2025.01.219 ↗
58. First-principles determination of the effect of boron on aluminum grain boundary cohesion
59. Hydrogen diffusion and trapping process around MnS precipitates in α-Fe examined by tritium autoradiography10.1016/j.jallcom.2007.02.005 ↗
60. A first-principles study on the hydrogen trap characteristics of coherent nano-precipitates in α-Fe10.1016/j.ijhydene.2020.07.123 ↗
61. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
62. Combined thermal desorption spectroscopy, differential scanning calorimetry, scanning electron microscopy and X-ray diffraction study of hydrogen trapping in cold deformed TRIP steel10.1016/j.actamat.2012.01.026 ↗
63. Behavior of alumina-magnesia complex inclusions and magnesia inclusions on the surface of molten low-carbon steels10.1007/s11663-001-0010-1 ↗
64. Effect of manganese content and microstructure on the susceptibility of X70 pipeline steel to hydrogen cracking10.1016/j.msea.2012.04.076 ↗
65. DFT study on the mechanism of inclusion-induced initial pitting corrosion of Al-Ti-Ca complex deoxidized steel with Ce treatment10.1016/j.physb.2019.01.027 ↗
66. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
67. Towards a better understanding of localised corrosion induced by typical non-metallic inclusions in low-alloy steels10.1016/j.corsci.2020.109150 ↗
68. Numerical study of the effect of inclusions on the residual stress distribution in high-strength martensitic steels during cooling10.3390/app9030455 ↗
69. P.J.Z. Juvonen, Effects of non-metallic inclusions on fatigue properties of calcium treated steels, 2004.
70. Optical and electrical properties of thin films of MnS/metal/MnS for photocatalysis and gas sensing applications10.1016/j.ijleo.2023.171549 ↗
71. A review of recent advance on hydrogen embrittlement phenomenon based on multiscale mechanical experiments
72. A statistical, physical-based, micro-mechanical model of hydrogen-induced intergranular fracture in steel10.1016/j.jmps.2009.10.005 ↗
73. Adverse effects of Ni on the mechanical and corrosion-induced hydrogen embrittlement properties of ultra-strong giga steel used for automotive applications10.1016/j.matdes.2020.108877 ↗
74. An atomic simulation of the influence of hydrogen on the fracture behavior of nickel10.1557/JMR.1992.2080 ↗
75. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
76. An empirical model of the kinetics of hydrogen-induced cracking in pipeline steel, using statistical distribution models and considering microstructural characteristics and hydrogen diffusion parameters10.1016/j.corsci.2024.112556 ↗
77. A discussion of the effects of composition and heat treatment on the toughness of a medium carbon secondary hardening steel10.1016/j.msea.2019.01.079 ↗
78. Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys10.1016/j.msea.2016.08.053 ↗