Sanicro 25 in advanced ultra-supercritical (AUSC) steam: Oxidation behaviour of a high strength, heat-resistant austenitic stainless steel for high-efficiency coal-fired power plants

C. Sundaresan, Bhagwat Ghule, Kamanio Chattopadhyay, V.S. Raja

Corrosion Science· Volume 250

Abstract

The oxidation behaviour of Sanicro 25 was investigated in advanced ultra-supercritical (AUSC) steam at 650–710 ℃, 31 MPa for 600 h. The alloy recorded low weight gains and formed sub-micron-sized external oxide comprising (Mn,Fe,Ni)Cr 2 O 4 spinel over Cr 2 O 3 . Its oxidation resistance was better than other candidate heat-resistant stainless steels and on par with Ni-base superalloy 617. Fine strengthening precipitates of Cu, Cr-rich M 23 C 6 , W-rich Lave’s and Nb-rich Z phases were found to form in the substrate during oxidation and their volume fraction increased with increasing temperature. The reasons for the alloy’s superior AUSC steam oxidation behaviour and its implications are discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Heat transfer and supercritical fluids

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (98)

Show source-provided references
1. Advanced ultrasupercritical thermal power plant and associated auxiliaries
2. A.K. Bhaduri, Materials research and opportunities in thermal (coal-based) power sector including advanced ultra super critical power plants10.16943/ptinsa/2015/v81i4/48294 ↗
3. The fossil fuel power plants technology
4. Development and qualification of materials for Indian advanced ultra-supercritical coal-fired power plant10.1520/MPC20200189 ↗
5. Alloy 617 and derivatives10.1016/B978-0-08-100552-1.00016-6 ↗
7. Sanicro 25
8. Creep and LCF behaviors of newly developed advanced heat resistant austenitic stainless steel for A-USC10.1016/j.proeng.2013.03.248 ↗
9. Long term performance of newly developed austenitic heat resistant stainless steel grade UNS S31035
10. Evolution of the microstructure and mechanical properties of Sanicro 25 austenitic stainless steel after long-term ageing10.1007/s43452-023-00690-y ↗
11. Formation of laves phase in Sanicro 25 austenitic steel during creep-rupture test at 700 °C10.1007/s13632-019-00529-0 ↗
12. On the origin of extraordinary cyclic strengthening of the austenitic stainless steel Sanicro 25 during fatigue at 700 °C10.1557/jmr.2017.311 ↗
13. Atomic resolution characterization of strengthening nanoparticles in a new high-temperature-capable 43Fe-25Ni-22.5Cr austenitic stainless steel10.1016/j.msea.2018.02.004 ↗
14. Creep and fatigue interaction behavior in sanicro 25 heat resistant austenitic stainless steel10.1007/s12666-015-0806-3 ↗
15. Microstructure, chemical- and phase composition of sanicro 25 austenitic steel after oxidation in steam at 700 °C10.1007/s11085-017-9824-3 ↗
16. Microstructural studies of the scale on Sanicro 25 after 25,000 h of oxidation in steam using advanced electron microscopy techniques10.1016/j.surfcoat.2019.124901 ↗
17. Microstructural characterisation of austenitic heat resistant sanicro 25 steel after steam oxidation10.3390/ma13153382 ↗
18. Microstructural stability and oxidation behavior of Sanicro 25 during long-term steam exposure in the temperature range 600-750 °C10.1002/maco.201407901 ↗
19. Oxidation behavior of austenitic steel Sanicro25 and TP347HFG in supercritical water10.1002/maco.201810247 ↗
20. High temperature oxidation of alloy 617, 740, HR6W and Sanicro 25 in supercritical water at 650 ° C
21. Theoretical study of steam grown oxides as a function of temperature, pressure and p(O2)10.3184/096034005782750455 ↗
22. A review of the oxidation behaviour of structural alloys in steam10.1179/095066010X12646898728165 ↗
23. Steam oxidation and chromia evaporation in ultrasupercritical steam boilers and turbines10.1149/1.3155442 ↗
24. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapor10.1007/s11085-006-9030-1 ↗
25. Theoretical and experimental investigation of the thermochemistry of CrO2(OH)2(g)10.1021/jp0647380 ↗
26. Thermodynamics of gas phase chromium species: the chromium oxides, the chromium oxyhydroxides, and volatility calculations in waste incineration processes10.1016/0010-2180(93)90087-J ↗
27. Oxidation behaviour of austenitic stainless steel 304HCu in advanced ultra supercritical (AUSC) steam and the efficacy of shot-peening treatment10.1016/j.corsci.2024.112214 ↗
28. Oxidation behaviour of Ni-base superalloy 617 in simulated advanced ultra supercritical (AUSC) steam10.1016/j.corsci.2023.111503 ↗
29. The powder diffraction file: a quality materials characterization database10.1017/S0885715619000812 ↗
30. High-temperature deformation and fracture mechanisms of an advanced heat resistant Fe-Cr-Ni alloy10.1016/j.msea.2017.01.002 ↗
31. Effect of niobium on microstructure and precipitation in As-annealed Sanicro 25 steel10.1080/03019233.2018.1540524 ↗
32. The oxidation behaviour of an austenitic steel in deaerated supercritical water at 600–700 °C10.1016/j.matchar.2017.07.023 ↗
33. Oxidation kinetics of austenitic stainless steels as SCWR fuel cladding candidate materials in supercritical water
34. Influence of temperature on the oxidation behavior of an austenitic steel in deaerated supercritical water10.1002/maco.201709705 ↗
35. Diffusion in solid-state systems
36. Role of Mn doping on magnetic properties of multiferroic NiCr2O4 nanoparticles10.1016/j.ceramint.2020.12.177 ↗
37. Effect of surface preparation on the corrosion of austenitic stainless steel 304L in high temperature steam and simulated PWR primary water10.1016/j.corsci.2011.12.007 ↗
38. Stability of chromia (Cr2O3)-based scales formed during corrosion of austenitic Fe-Cr-Ni alloys in flowing oxygenated supercritical water10.5006/1982 ↗
39. Environment effects on chromia (Cr2O3) scale stability formed on type 310S stainless steel during wet oxidation10.5006/2771 ↗
40. Reducibility of oxides and sulphides in metallurgical processes
41. Alloy oxidation III: multiphase scales10.1016/B978-0-08-100101-1.00007-8 ↗
42. L. Qiu, D.A. GuzonasPrediction of metal oxide stability in supercritical water reactors - Pourbaix versus Ellingham, in: 3rd Canada-China JointWorkshop Supercrit. Water-Cooled React. CCSC-2012, Zian, China, 2012. http://inis.iaea.org/search/search.aspx?orig_q=RN:49101514..
43. Oxidation behavior of a new wrought Ni-30Fe-20Cr based alloy at 750 °C in pure steam and the effects of alloyed yttrium10.1016/j.corsci.2017.06.009 ↗
44. The effect of silicon addition on the high temperature oxidation of a Fe-Cr alloy
45. Silicon effects on the wet oxidation of type 310 stainless steel10.1016/j.corsci.2018.08.011 ↗
46. Obtaining and Indexing Parallel-Beam Diffraction Patterns
47. On the crystallography and composition of topologically close-packed phases in ATI 718Plus®10.1016/j.actamat.2017.03.038 ↗
48. Subsurface depletion and enrichment processes during oxidation of a high chromium, Laves-phase strengthened ferritic steel10.1149/1.3590258 ↗
49. High-temperature cyclic oxidation behavior and microstructure evolution of W- and Ce-containing 18Cr-Mo type ferritic stainless steel10.3390/ma17102230 ↗
50. Precipitation behavior of laves phase in the vicinity of oxide film of ferritic stainless steel: selective oxidation-induced precipitation10.1007/s11085-019-09955-5 ↗
51. On the crystal structure of Z-phase Cr(V,Nb)N10.1007/BF02586098 ↗
52. Characterization of intergranular phases in precipitation hardening Ni alloy UNS N0772510.1016/j.matchar.2020.110770 ↗
53. Atomic imaging of the interface between M23C6-type carbide and matrix in a long-term ageing polycrystalline Ni-based superalloy10.1080/09500839.2015.1039621 ↗
54. On the M23C6-carbide in 2205 duplex stainless steel: an unexpected (M23C6/Austenite)—eutectoid in the δ-ferritic matrix10.3390/met11091340 ↗
55. Computational modeling of the effect of B and W in the phase transformation of M23C6 carbides in 9 to 12 pct Cr martensitic/ferritic steels10.1088/2053-1591/ab500c ↗
56. Long-term creep behaviours and structural stabilities of austenitic heat-resistant stainless steels10.1080/09603409.2023.2263719 ↗
57. Precipitation and hot deformation behavior of austenitic heat-resistant steels: A review10.1016/j.jmst.2017.01.025 ↗
58. Refinement of the a Al2O3, Ti2O3, V2O3 and Cr2O3 structures
59. Crystallographic study of chromium spinels10.1063/1.1708502 ↗
60. U. Hålenius, Structural changes and valence states in the MgCr2O4-FeCr2O4 solid solution series10.1007/s00269-004-0420-0 ↗
61. The low-temperature tetragonal phase of NiCr2O410.1107/S0108270199011713 ↗
62. Isothermal compression of face-centered cubic iron10.2138/am.2012.3958 ↗
63. The crystal structure of Cr23C610.1107/S0567740872007526 ↗
64. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
65. Oxidation of binary FeCr alloys (Fe-2.25Cr, Fe-10Cr, Fe-18Cr and Fe-25Cr) in O2 and in O2 + H2O environment at 600 °c10.1007/s11085-010-9229-z ↗
66. Enhanced internal oxidation as trigger for breakaway oxidation of Fe-Cr alloys in gases containing water vapor10.1016/j.scriptamat.2007.06.058 ↗
67. The effect of water vapor on selective oxidation of Fe-Cr alloys10.1007/s11085-007-9090-x ↗
68. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor10.1023/A:1018875024306 ↗
69. Microstructural investigation of the breakdown of the protective oxide scale on a 304 steel in the presence of oxygen and water vapour at 600 °C10.1016/j.corsci.2005.08.012 ↗
70. oxidation behaviour of super 304H stainless steel in supercritical water10.1080/1478422X.2018.1459064 ↗
71. Early oxidation of Super304H stainless steel and its scales stability in supercritical water environments10.1016/j.ijhydene.2016.04.144 ↗
72. Investigation on oxidation behavior of super304H and HR3C steel in high temperature steam from a 1000 MW ultra-supercritical coal-fired boiler
73. The oxidation of alloys10.1088/0034-4885/39/5/001 ↗
74. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
75. The effect of manganese additions on the reactive evaporation of chromium in Ni-Cr alloys10.1016/j.scriptamat.2006.01.026 ↗
76. Chromium vaporization from high-temperature alloys10.1149/1.2434690 ↗
77. Evaluation of the oxidation and Cr evaporation properties of selected FeCr alloys used as SOFC interconnects10.1016/j.ijhydene.2013.09.044 ↗
78. Effect of water vapour partial pressure on the chromia (Cr2O3)-based scale stability10.1080/00084433.2017.1373968 ↗
79. S. Mahboubi, Wet oxidation performance of Type 310S stainless steel, McMaster University, 2018. 〈http://hdl.handle.net/11375/22887〉 (accessed August 1, 2024).
80. Oxidation behavior of Fe-25Cr-20Ni-2.8Si during isothermal oxidation at 1,286 K; life-time prediction10.1007/s11085-008-9097-y ↗
81. Revealing the oxidation mechanism of 310S stainless steel in supercritical water via high-resolution characterization10.1016/j.corsci.2022.110212 ↗
82. Oxidation behavior of UHP Fe-based model alloy and SUS310S steel in superheated steam and supercritical water conditions10.1007/s11085-017-9788-3 ↗
83. Effect of exposure temperature on oxidation of austenitic steel HR3C in supercritical water10.1007/s11085-018-9879-9 ↗
84. Internal oxidation of austenitic Fe-Ni-Cr alloys at high temperatures: deduction of oxygen permeability and the influence of carbon-bearing gases10.1016/j.corsci.2023.111465 ↗
85. Thermodynamic modelling of the Cr-Fe-Ni-O system
86. Comparison of the corrosion behavior of four Fe-Cr-Ni austenitic alloys in supercritical water10.1016/j.jnucmat.2024.155409 ↗
87. Role of nickel in the oxidation of Fe-Cr-Ni alloys in air-water vapour atmospheres10.3184/096034005782744236 ↗
88. High temperature oxidation behavior of ferritic stainless steel containing W and Ce10.1016/j.corsci.2018.07.017 ↗
89. Oxidation behavior of ferritic stainless steels in simulated automotive exhaust gas containing 5 vol% water vapor10.1016/j.matchemphys.2017.11.051 ↗
90. The role of dissolved oxygen in supercritical water in the oxidation of ferritic-martensitic steel10.1016/j.supflu.2015.10.017 ↗
91. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
92. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
93. Effect of pressure on the rate of corrosion of metals in high subcritical and supercritical aqueous systems10.1016/j.supflu.2003.09.004 ↗
94. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.msea.2007.05.035 ↗
95. The influence of manganese on the high-temperature oxidation of iron-chromium alloys10.1002/maco.19890400403 ↗
96. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
97. First study of manganese diffusion in Cr2O3 polycrystals and thin films by SIMS10.1080/14786430601120462 ↗
98. A chemical diffusion model for partitioning of transition elements in oxide scales on alloys10.1080/14786437208226960 ↗