Temperature dependence of corrosion behavior of a dual-phase Fe50Mn30Co10Cr10 high entropy alloy in supercritical water at 380–650 °C
Source abstract
Abstract
Corrosion behavior of a dual-phase Fe 50Mn 30Co 10Cr 10 HEA subjected to supercritical water at different temperatures was investigated. Both weight gain and oxide film thickness increased with increasing temperatures. An outer layer with polyhedral MnFe 2O 4 particles and an inner layer containing a mixture of CrMn 1.5O 4 and Fe 3O 4 were formed at 380 °C. Mn 2O 3 outer and CrMn 1.5O 4 inner layers developed at 550 and 650 °C, but the loose granular Mn 2O 3 particles at 550 °C transformed into a compact oxide film at 650 °C. Besides, Cr 2O 3 oxide particles were observed along the grain boundaries. The corrosion mechanism at different temperatures was also discussed.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · High-Temperature Coating Behaviors · Subcritical and Supercritical Water Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (95)
Show source-provided references
1. Design concepts of supercritical water-cooled reactor (SCWR) and nuclear marine vessel: a review10.1016/j.pnucene.2020.103320 ↗
2. European supercritical water cooled reactor10.1016/j.nucengdes.2010.09.039 ↗
3. A review of existing supercritical water reactor concepts, safety analysis codes and safety characteristics10.1016/j.pnucene.2022.104409 ↗
4. Chemistry in supercritical water10.1002/(SICI)1521-3773(19991018)38:20<2998::AID-ANIE2998>3.0.CO;2-L ↗
5. Corrosion resistance of candidate cladding materials for supercritical water reactor10.1016/j.anucene.2018.12.007 ↗
6. Nanostructured high-entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
7. High-entropy alloys: a critical review10.1080/21663831.2014.912690 ↗
8. Microstructural evolution after thermomechanical processing in an equiatomic, single-phase CoCrFeMnNi high-entropy alloy with special focus on twin boundaries10.1016/j.intermet.2014.05.014 ↗
9. Microstructure and compressive properties of AlCrFeCoNi high entropy alloy10.1016/j.msea.2008.01.064 ↗
10. Development and exploration of refractory high entropy alloys—a review10.1557/jmr.2018.153 ↗
11. Non-equiatomic high entropy alloys: approach towards rapid alloy screening and property-oriented design10.1016/j.msea.2015.09.010 ↗
12. A novel, single phase, non-equiatomic FeMnNiCoCr high-entropy alloy with exceptional phase stability and tensile ductility10.1016/j.scriptamat.2013.09.030 ↗
13. Design of a twinning-induced plasticity high entropy alloy10.1016/j.actamat.2015.04.014 ↗
14. Metastable high-entropy dual-phase alloys overcome the strength–ductility trade-off10.1038/nature17981 ↗
15. Microstructure investigations of Fe50Mn30Co10Cr10 dual–phase high–entropy alloy under Fe ions irradiation10.1016/j.jnucmat.2021.153006 ↗
16. Comparative corrosion behavior of Fe50Mn30Co10Cr10 dual-phase high-entropy alloy and CoCrFeMnNi high-entropy alloy in 3.5 wt% NaCl solution10.1016/j.jallcom.2020.155824 ↗
17. Corrosion behavior and passive film characterization of Fe50Mn30Co10Cr10 dual-phase high-entropy alloy in sulfuric acid solution10.1149/1945-7111/ab8de4 ↗
18. Influence of temperature on the oxidation behaviour of a ferritic-martensitic steel in supercritical water10.1016/j.corsci.2016.10.020 ↗
19. Effect of exposure temperature on the corrosion behaviors of TP347H austenitic stainless steel in supercritical water10.1016/j.corsci.2019.108188 ↗
20. Effects of exposure temperature and time on corrosion behavior of a ferritic–martensitic steel P92 in aerated supercritical water10.1016/j.corsci.2014.10.022 ↗
21. Effect of exposure temperature on oxidation of austenitic steel HR3C in supercritical water10.1007/s11085-018-9879-9 ↗
22. Oxidation of ferritic–martensitic alloys T91, HCM12A and HT-9 in supercritical water10.1016/j.jnucmat.2007.05.023 ↗
23. Corrosion behavior of ferritic/martensitic steel P92 in supercritical water10.1016/j.supflu.2009.06.019 ↗
24. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
25. The corrosion and stress corrosion cracking behavior of a novel alumina-forming austenitic stainless steel in supercritical water10.1016/j.jnucmat.2016.10.039 ↗
26. Oxidation behavior of grain boundary engineered alloy 690 in supercritical water environment10.1016/j.jnucmat.2011.12.022 ↗
27. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
28. Oxidation of alloy 600 and alloy 690: experimentally accelerated study in hydrogenated supercritical water10.1007/s11661-016-3897-5 ↗
29. Corrosion of alumina-forming austenitic steel Fe–20Ni–14Cr–3Al–0.6Nb–0.1Ti in supercritical water10.1016/j.jnucmat.2010.01.025 ↗
30. Effect of Al and Ti addition on performance of stainless steel 310 in supercritical water10.1179/1743278214Y.0000000225 ↗
31. Oxidation of 316 stainless steel in supercritical water10.1016/j.corsci.2009.03.008 ↗
32. Corrosion characteristics and mechanisms of typical Ni-based corrosion-resistant alloys in sub- and supercritical water10.1016/j.supflu.2020.105138 ↗
33. Corrosion and stress corrosion cracking susceptibility of type 347H stainless steel in supercritical water10.5006/2459 ↗
34. Corrosion behavior of alloys 625 and 718 in supercritical water10.5006/1.3278410 ↗
35. Effect of dissolved oxygen content on the oxide structure of Alloy 625 in supercritical water environments at 700°C10.1016/j.corsci.2013.11.034 ↗
36. Corrosion behavior of Ni-base alloys for advanced high temperature water-cooled nuclear plants10.1016/j.corsci.2008.08.024 ↗
37. Influence of the dissolved oxygen content on corrosion of the ferritic–martensitic steel P92 in supercritical water10.1016/j.corsci.2011.11.013 ↗
38. Effect of grain refinement on corrosion of ferritic-martensitic steels in supercritical water environment10.1002/maco.200905446 ↗
39. Effects of Si, Mn on the corrosion behavior of ferritic–martensitic steels in supercritical water (SCW) environments10.1016/j.corsci.2020.108432 ↗
40. Oxidation of ferritic and ferritic–martensitic steels in flowing and static supercritical water10.1016/j.corsci.2015.10.017 ↗
41. Corrosion Behavior of Ferritic/Martensitic Steels CNS-I and Modified CNS-II in Supercritical Water10.1016/S1006-706X(12)60102-2 ↗
42. Corrosion of ferritic–martensitic steels in steam and supercritical water10.1016/j.jnucmat.2012.09.037 ↗
43. Corrosion of ferritic–martensitic steel HT9 in supercritical water10.1016/j.jnucmat.2006.07.010 ↗
44. Corrosion behavior of ferritic–martensitic steel T91 in supercritical water10.1016/j.corsci.2005.08.021 ↗
45. Effect of long-term pre-oxidation on the corrosion rate of 316l stainless steel in a high-temperature water environment10.1007/s11665-022-06878-2 ↗
46. Uniform corrosion behavior of FeCrAl alloys in borated and lithiated high temperature water10.1016/j.jmst.2020.07.026 ↗
47. Oxidation of austenitic and ferritic/martensitic alloys in supercritical water10.1016/j.supflu.2013.03.014 ↗
48. Corrosion behavior of 9–12% Cr ferritic–martensitic steels in supercritical water10.1016/j.corsci.2009.12.032 ↗
49. Oxidation behavior of the CrMnFeCoNi high-entropy alloy10.1007/s11085-016-9616-1 ↗
50. Cycle chemistry and its effect on materials in a supercritical water-cooled reactor: a synthesis of current understanding10.1016/j.corsci.2012.08.006 ↗
51. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
52. Point defect model for the corrosion of steels in supercritical water: part i, film growth kinetics10.1016/j.corsci.2019.108280 ↗
53. Corrosion of carbon steels in high-temperature water studied by electrochemical techniques10.1016/j.corsci.2004.01.021 ↗
54. On the pH control at supercritical water-cooled reactor operating conditions10.1016/j.nucengdes.2012.03.038 ↗
55. Determination of corrosion mechanisms and estimation of electrochemical kinetics of metal corrosion in high subcritical and supercritical aqueous systems10.5006/1.3319143 ↗
56. Stress corrosion crack growth behavior of type 310s stainless steel in supercritical water10.5006/2775 ↗
57. The mechanism of high temperature aqueous corrosion of steel10.1016/0010-938X(89)90120-0 ↗
58. Early corrosion characterization of 316 stainless steel (Passivated in Supercritical Water with Na3PO4) in subcritical water containing oxygen and NaCl10.1007/s11665-020-04701-4 ↗
59. Corrosion and corrosion fatigue behaviors of 9cr steel in a supercritical water condition10.1016/j.msea.2006.05.035 ↗
60. High temperature oxidation of austenitic stainless steel in low oxygen pressure10.1016/0010-938X(77)90011-7 ↗
61. A chemical diffusion model for partitioning of transition elements in oxide scales on alloys10.1080/14786437208226960 ↗
62. Characterization of oxide films grown on 316L stainless steel exposed to H2O2-containing supercritical water10.1016/j.supflu.2006.12.020 ↗
63. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
64. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
65. Effects of sulfides on the corrosion behavior of inconel 600 and incoloy 825 in supercritical water10.1007/s11085-015-9567-y ↗
66. Effect of temperature and dissolved oxygen on stress corrosion cracking behavior of P92 ferritic-martensitic steel in supercritical water environment10.1016/j.jnucmat.2017.10.024 ↗
67. Microstructural investigation of the nodular corrosion of 304NG stainless steel in supercritical water10.1016/j.corsci.2020.108652 ↗
68. A study on the corrosion behaviour of stainless steel 08Cr18Ni10Ti in supercritical water10.1016/j.corsci.2022.110853 ↗
69. A. Roine. Outokumpu H.S.C. Chemistry for windows, version 9.; Outokumpu Research Oy: Pori, Finland, 2018.
70. Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions10.1016/j.supflu.2013.05.002 ↗
71. Effect of oxygen concentrations on the corrosion behavior of a duplex-phase FeNiCrCuAl high entropy alloy in supercritical water10.1016/j.jnucmat.2022.154046 ↗
72. Effect of Al addition on the corrosion behavior of AlxCoCrFeNi high entropy alloys in supercritical water10.1016/j.corsci.2023.111089 ↗
73. Effect of alloying elements (Mn, Ti, and Mo) on the corrosion behavior of FeCoNiCr-based high entropy alloy in supercritical water10.1016/j.corsci.2023.111291 ↗
74. Oxidation behavior of Al0.2CoCrFeNi high-entropy alloy film in supercritical water environment10.1007/s12598-021-01859-1 ↗
75. Oxidation behavior of high-entropy alloys AlxCoCrFeNi (x=0.15, 0.4) in supercritical water and comparison with HR3C steel10.1016/S1003-6326(15)63733-5 ↗
76. Corrosion in high-temperature and supercritical water and aqueous solutions: a review10.1016/S0896-8446(03)00031-7 ↗
77. Volume of activation for the corrosion of type 304 stainless steel in high subcritical and supercritical aqueous systems10.5006/1.3319147 ↗
78. Microstructures and properties of high-entropy alloys10.1016/j.pmatsci.2013.10.001 ↗
79. Concerning the evaluation of corrosion reactions by superposition of electrochemical partial reactions and concerning the potential formation on mixed electrodes
80. The point defect model for the passive state10.1149/1.2069096 ↗
81. Mechanism of corrosion of carbon and low alloy ferritic steels by high temperature water10.5006/1.3577543 ↗
82. Influence of Mn on the corrosion behaviour of medium manganese steels in a simulated seawater environment10.20964/2016.11.51 ↗
83. Atmospheric corrosion resistance of MnCuP weathering steel in simulated environments10.1016/j.corsci.2011.08.028 ↗
84. Probing the chemical and electrochemical properties of SCWO systems10.1016/S0013-4686(01)00758-7 ↗
85. Potential-pH diagrams considering complex oxide solution phases for understanding aqueous corrosion of multi-principal element alloys10.1038/s41529-020-00141-6 ↗
86. Corrosion behavior of Alloy 625 in supercritical water environments10.1016/j.pnucene.2011.12.015 ↗
87. A comparative study of oxide scales grown on stainless steel and nickel-based superalloys in ultra-high temperature supercritical water at 800 °C10.1016/j.corsci.2016.02.004 ↗
88. Corrosion behaviour of 16%Cr–4%Al and 16%Cr ODS ferritic steels under different metallurgical conditions in a supercritical water environment10.1016/j.corsci.2010.05.043 ↗
89. Corrosion properties of candidate materials in supercritical water oxidation process
90. On-line monitoring of oxide formation and dissolution on alloy 800H in supercritical water10.1016/j.corsci.2016.05.042 ↗
91. Oxidation of Fe-(5.3-29.8)%Mn-(1.1-1.9)%Al-0.45%C alloys at 550–650 oC
92. Diffusion of chromium, manganese, and iron in MnCr2O4 spinel10.1007/s11669-005-0051-2 ↗
93. Thermal-hydraulic and neutron-physical characteristics of a new SCWR fuel assembly10.1016/j.anucene.2008.11.001 ↗
94. Core and sub-channel analysis of SCWR with mixed spectrum core10.1016/j.anucene.2010.07.014 ↗
95. S. Constantin, Analyses of oxide films grown on AISI 304L stainless steel and Incoloy 800HT exposed to supercritical water environment10.1016/j.jnucmat.2011.05.007 ↗