This research scrutinizes the intricate effects of hydrogen charging on crystal defects and passive film properties in high-defect-density 443 ultrapure ferritic stainless steel. It discerns that with non-saturated hydrogen at hydrogen traps, escalated hydrogen charging current density results in increased hydrogen capture . These trapped atoms fill the defects, thus mitigating the stress level and fostering the growth of chromium oxides within the passive film. Consequently, the alloy’s resistance to intergranular corrosion is enhanced.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (73)
Show source-provided references
1. Improved corrosion performance of selective laser melted stainless steel 316L in the deep-sea environment10.1016/j.corcom.2021.09.002 ↗
2. A short review on the role of alloying elements in duplex stainless steels
3. Roles of different components of complex inclusion in pitting of 321 stainless steel: Induction effect of CaS and inhibition effect of TiN10.1016/j.corsci.2022.110692 ↗
4. Intergranular corrosion of low Cr ferritic stainless steel 429 evaluated by the optimized double loop electrochemical potentiokinetic reactivation test
5. Investigation on ultra-pure ferritic stainless steel 436L susceptibility to intergranular corrosion using optimised double loop electrochemical potentiokinetic reactivation method10.1080/1478422X.2018.1512222 ↗
6. Enhancement in intergranular corrosion resistance of the stabilised ultra-pure 430LX ferritic stainless steel by tin addition10.1080/1478422X.2020.1721807 ↗
7. Effect of Ti addition on forming limit diagrams of Nb-bearing ferritic stainless steel10.1016/j.jmatprotec.2011.08.004 ↗
8. A comparative study on the critical pitting criteria of a super ferritic stainless steel at different temperatures in chloride or bromide solution10.1016/j.corsci.2021.109311 ↗
9. New findings on intergranular corrosion mechanism of 445J2 ultra-pure ferritic stainless steel10.5006/4065 ↗
10. Effects of grain boundary characteristics changing with cold rolling deformation on intergranular corrosion resistance of 443 ultra-pure ferritic stainless steel10.1016/j.corcom.2022.07.002 ↗
11. Hydrogen embrittlement behavior of 430 and 445NF ferritic stainless steels10.1007/s11661-012-1265-7 ↗
12. Effect of hydrogen charging conditions on hydrogen blisters and pitting susceptibility of 445J1M ferritic stainless steel10.1149/2.0711816jes ↗
13. Synergistic effect of cold work and hydrogen charging on the pitting susceptibility of 2205 duplex stainless steel10.1016/j.electacta.2019.135081 ↗
14. The role of stress in hydrogen induced delayed failure
15. An example of the effect of hydrogen trapping on hydrogen embrittlement10.1007/BF02648348 ↗
16. Effects of hydrogen on the crevice corrosion behaviors of duplex stainless steel 220510.1016/j.jmrt.2022.05.026 ↗
17. A different type of intergranular corrosion facilitated by hydrogen in austenitic stainless steel10.1016/j.corsci.2023.111258 ↗
18. Trapping of hydrogen by substitutional and interstitial impurities in α-iron10.1016/0036-9748(83)90439-8 ↗
19. Trapping of hydrogen by oxygen and nitrogen impurities in niobium, vanadium and tantalum10.1016/0001-6160(83)90193-1 ↗
20. The role of hydrogen in the corrosion and cracking of steels a review10.1016/j.corcom.2021.10.005 ↗
21. On partial molal volume of hydrogen in alpha iron
22. The thermodynamics of stressed solids10.1524/zpch.1966.49.3_5.271 ↗
23. Hydrogen, crack initiation, and delayed failure in steel
24. New model for hydrogen-assisted cracking10.1007/BF02642048 ↗
25. Effect of hydrogen on the intergranular stress corrosion cracking of alloy 600 in high temperature aqueous environments10.5006/1.3583894 ↗
26. Hydrogen trapping in ferritic steel weld metal10.1179/095066002225006548 ↗
27. Corrosion behavior of a nickel-free high-nitrogen stainless steel with hydrogen charging10.1007/s11837-021-04569-2 ↗
28. The mechanism of hydrogen-induced pitting corrosion in duplex stainless steel studied by SKPFM10.1016/j.corsci.2012.04.010 ↗
29. Influence of carbide precipitation and rolling direction on intergranular stress corrosion cracking of austenitic stainless steels in hydrogenated high-temperature water10.5006/1.3280670 ↗
30. Investigation of hydrogen concentration and hydrogen damage on API X80 steel surface under cathodic overprotection10.1016/j.ijhydene.2017.10.116 ↗
31. Corrosion fatigue crack initiation and initial propagation mechanism of E690 steel in simulated seawater10.1016/j.msea.2017.09.078 ↗
32. Influence of rare earth metals on mechanisms of localised corrosion induced by inclusions in Zr-Ti deoxidised low alloy steel10.1016/j.corsci.2020.108463 ↗
33. Residual stress analysis of diamond-coated WC–Co cutting tools: separation of film and substrate information by grazing X-ray diffraction10.1107/S0021889813020451 ↗
34. Exceptionally high CO 2 capture in an amorphous polymer with ultramicropores studied by positron annihilation10.1021/acsami.9b07015 ↗
35. Inhibition effect and mechanism of tin on the active dissolution of tin-containing 430LX ferritic stainless steel10.1016/j.corsci.2021.109818 ↗
36. Formation of hydrogen-induced vacancies during growth of the Fe layer studied by slow positron beam10.1016/S0039-6028(02)01644-8 ↗
37. Correlation between Cu precipitates and irradiation defects in Fe–Cu model alloys investigated by positron annihilation spectroscopy10.1016/j.actamat.2015.10.051 ↗
38. Binding of solute atoms to dislocations
39. Stress fields around inclusions and their relation to mechanical properties
40. Hydrogen embrittlement in Fe-Mn-B steels
41. Hydrogen degradation of spheroidized AISI 1090 steel10.1007/BF02658674 ↗
42. The mechanism of brittle fracture in a microalloyed steel: Part II. Mechanistic modeling10.1007/s11661-000-0008-3 ↗
43. Interstitial solute trapping by edge dislocations10.1016/0001-6160(85)90123-3 ↗
44. Embrittlement of ferritic stainless steels10.1007/BF02670694 ↗
45. Effect of stabilising elements on formation of σ phase in experimental ferritic stainless steels containing 39%Cr10.1179/mst.1992.8.5.437 ↗
46. Effect of chromium content on intergranular corrosion and precipitation of Ti-stabilized ferritic stainless steels10.1016/j.corsci.2010.01.037 ↗
47. Theoretical, numerical and experimental approaches for structural studies of grain boundaries: Methods, remarkable results and perspectives10.4028/www.scientific.net/SSP.59-60.1 ↗
48. “Dislocation–interface” interaction — stress accommodation processes at interfaces10.1016/S0921-5093(00)01696-8 ↗
49. G. Totten, M. Howes, T. Inoue, Handbook of residual stress and deformation of steel, ASM. International Materials Park, Ohio, 2002.
50. The recovery of gas-vacancy-complexes in Fe irradiated with high energy H or He ions10.2320/matertrans.45.9 ↗
51. Effect of electrochemical hydrogen charging on defect structure in titanium10.1016/j.jallcom.2021.160909 ↗
52. Brandt · 1983
53. Hautojarvi · 1979
54. Titanium defect structure change after gas-phase hydrogenation at different temperatures and cooling rates
55. Positron lifetime computations of defects in nickel containing hydrogen or helium10.1016/S0022-3115(02)01227-8 ↗
56. Positron simulations of defects in tungsten containing hydrogen and helium10.1016/j.nimb.2008.11.045 ↗
57. Passivity breakdown on 436 ferritic stainless steel in solutions containing chloride10.1016/j.jmst.2018.10.030 ↗
58. Strategies to enhance corrosion resistance of Zn electrodes for next generation batteries10.3389/fmats.2020.00096 ↗
59. Understanding the pitting mechanism of super ferritic stainless steel in bromide solutions: the role of Ti/Nb–Mo precipitates with a core–shell structure10.1016/j.corsci.2022.110176 ↗
60. The chemical composition of the passive film on Fe-24Cr and Fe-24Cr-11Mo studied by AES, XPS and SIMS10.1016/0010-938X(91)90013-F ↗
61. Chemical composition and electronic structure of the oxide films formed on 316L stainless steel and nickel based alloys in high temperature aqueous environments
62. Comparative study of structural and semiconducting properties of passive films and thermally grown oxides on AISI 304 stainless steel10.1016/j.corsci.2011.05.012 ↗
63. On the relation between growth instabilities and internal stress evolution during galvanostatic Ti thin film anodization10.1149/1.2958306 ↗
64. Stress-induced breakdown during galvanostatic anodising of zirconium10.1016/j.electacta.2010.03.042 ↗
65. Passive film of 18-8 stainless steel structure and its function10.1016/0010-938X(73)90031-0 ↗
66. Semiconductor properties of passive films formed on sputter-deposited Fe–18Cr alloy thin films with various additive elements10.1016/j.stam.2003.10.014 ↗
67. On the determination of the flat-band potential of a semiconductor in contact with a metal or an electrolyte from the Mott-Schottky plot10.1088/0022-3727/11/4/003 ↗
68. Chemical composition and semiconducting behaviour of stainless steel passive films in contact with artificial seawater10.1016/S0010-938X(98)00016-X ↗
69. The electronic properties of sputtered chromium and iron oxide films10.1016/j.corsci.2003.09.022 ↗
70. Corrosion resistance of stainless steel layer prepared by twin-wire indirect arc surfacing welding10.1016/j.vacuum.2020.109348 ↗
71. Theory of steady‐state passive films10.1149/1.2086949 ↗
72. Chemical composition and electronic structure of the oxide films formed on 316L stainless steel and nickel based alloys in high temperature aqueous environments
73. A study of the passive films on chromium by capacitance measurement10.1016/S0010-938X(02)00148-8 ↗