Valence-dependent TiO2 inhibition for enhancing oxidation resistance in Ti2AlC via Zr/Nb solid solution

Yuxi Xu, Guanshui Ma, Zhongchang Li, Yan Zhang, Anfeng Zhang, Zhenyu Wang, Aiying Wang

Corrosion Science· Volume 257
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: MXene and MAX Phase Materials · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Multi-stage phase transformation pathways in MAX phases10.1038/s41467-025-56921-8 ↗
2. MAX phases – past, present, and future10.1016/j.mattod.2023.11.010 ↗
3. Large-scale conformal synthesis of one-dimensional MAX phases10.1038/s41467-024-53137-0 ↗
4. MAX phase coatings: synthesis, protective performance, and functional characteristics10.1039/D4MH01001A ↗
5. Development of the phase composition and the properties of Ti2AlC and Ti3AlC2 MAX-phase thin films – a multilayer approach towards high phase purity10.1016/j.apsusc.2020.147864 ↗
6. Ultrahigh strength-ductility of nanocrystalline Cr2AlC coating under micropillar compression10.1016/j.scriptamat.2023.115594 ↗
7. Tribological and mechanical properties of Ti2AlC coating at room temperature and 800 °C10.1016/j.ceramint.2017.10.045 ↗
8. Corrosion performance of Ti3SiC2, Ti3AlC2, Ti2AlC and Cr2AlC MAX phases in simulated primary water conditions10.1016/j.corsci.2018.04.034 ↗
9. High temperature oxidation behavior of quaternary ordered (Cr2/3Ti1/3)3AlC2-based MAX ceramic10.1016/j.corsci.2021.109317 ↗
10. Highly dense passivation enhanced corrosion resistance of Ti2AlC MAX phase coating in 3.5 wt% NaCl solution10.1016/j.corsci.2024.111820 ↗
11. Chemical scissor–mediated structural editing of layered transition metal carbides10.1126/science.add5901 ↗
12. 25th anniversary article: MXenes: a new family of Two-Dimensional materials10.1002/adma.201304138 ↗
13. Oxidation and hot corrosion behaviors of MAX-phase Ti3SiC2, Ti2AlC, Cr2AlC10.1016/j.ceramint.2022.05.356 ↗
14. Multiple crack healing of a Ti2AlC ceramic10.1016/j.jeurceramsoc.2012.01.017 ↗
15. Towards developing Ti2AlC coatings with improved oxidation resistance via nb solid solution10.1016/j.jallcom.2024.175524 ↗
16. High temperature oxidation behaviour of Ti2AlC ceramic at 1200 °C10.3184/096034012X13348496462140 ↗
17. Alumina forming high temperature silicides and carbides10.1016/j.ceramint.2003.12.046 ↗
18. A critical review of the oxidation of Ti2AlC, Ti3AlC2 and Cr2AlC in air10.1080/21663831.2013.806364 ↗
19. Oxidation of Tin+1AlXn (n = 1­3 and X = C, N): I. Model10.1149/1.1380255 ↗
20. Oxidation of Tin+1AlXn (n=1­3 and X = C, N): II. Experimental results10.1149/1.1380256 ↗
21. Understanding the growth mechanisms of TiO2/Al2O3 mixed scales formed on Al-depleted Ti2AlC at 1000–1200 °C10.1016/j.corsci.2022.110393 ↗
22. Deposition, characterization and high-temperature steam oxidation behavior of single-phase Ti2AlC-coated Zircaloy-410.1016/j.corsci.2018.02.035 ↗
23. TEM study of the initial oxide scales of Ti2AlC10.1016/j.actamat.2011.04.058 ↗
24. Kinetic aspects of Ti2AlC MAX phase oxidation10.1007/s11085-015-9526-7 ↗
25. Influences of al concentration and nb addition on oxidation behavior of Ti2AlC ceramics at high temperatures
26. Mitigation of metal whisker growth from MAX phases by A-site alloying strategy10.1016/j.apsusc.2023.157486 ↗
27. Deposition of MAX phase-containing thin films from a (Ti, Zr)2AlC compound target10.1016/j.apsusc.2021.149370 ↗
28. Reducing the self-healing temperature of Ti2AlC MAX phase coating by substituting al with sn10.1016/j.jeurceramsoc.2019.09.009 ↗
29. Enhancing corrosion resistance of Ti2AlC MAX phase through sn solid solution in harsh acidic environments10.1016/j.corsci.2025.113073 ↗
30. Atomic scale insight into the oxidation mechanism of Nb/Ta-Doped Ti3SiC2/Al2O3 ceramics10.1002/adem.202301319 ↗
31. Investigation on the effect of nb doping on the oxidation mechanism of Ti3SiC210.1016/j.corsci.2018.05.028 ↗
32. Improving the High-Temperature oxidation resistance of Ti3(SiAl)C2 by Nb-Doping10.1111/j.1551-2916.2011.04586.x ↗
33. Effect of nb on the bonding characteristics of TiAl intermetallic compounds: a first-principle study
34. Studying the oxidation of Ti2AlC MAX phase in atmosphere: a review10.1016/j.ijrmhm.2016.07.006 ↗
35. High temperature oxidation behavior of disordered (Ti0.5Zr0.5)2AlC MAX phase via a machine Learning-Augmented DFT approach
36. Effect of nb dopant on the oxidation behavior of Zr2[Al(Si)]4C5 at 1000–1300 °C10.1111/j.1551-2916.2011.04564.x ↗
37. Tailoring microstructure and improving oxidation resistance of an additively manufactured high nb containing TiAl alloy via heat treatment10.1016/j.corsci.2023.111287 ↗
38. First-principles simulation: ideas, illustrations and the CASTEP code10.1088/0953-8984/14/11/301 ↗
39. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
40. A generalized synchronous transit method for transition state location10.1016/S0927-0256(03)00111-3 ↗
41. HiPIMS induced high-purity Ti3AlC2 MAX phase coating at low-temperature of 700 °C10.1016/j.jeurceramsoc.2023.03.059 ↗
42. Chalcogenide MAX phases Zr2Se(B1-xSex) (x=0–0.97) and their conduction behaviors10.1016/j.actamat.2022.118183 ↗
43. The oxidation behaviour of niobium containing γ-TiAl based intermetallics in air and argon/oxygen10.1007/BF01244851 ↗
44. Effect of Al2O3 content on the high-temperature oxidation behaviour of CoCrAlYTa coatings produced by laser-induction hybrid cladding10.1016/j.corsci.2022.110739 ↗
45. Oxidation and hot corrosion behavior of Al2O3/YSZ coatings prepared by cathode plasma electrolytic deposition10.1016/j.corsci.2016.03.017 ↗
46. Effect of nb doping on high temperature oxidation resistance of Ti-Al alloyed coatings
47. Alloying effects on properties of Al2O3 and TiO2 in connection with oxidation resistance of TiAl10.1016/j.intermet.2015.09.005 ↗
48. Experimental and thermodynamic modeling of Al2O3 corundum and TiO2 rutile structures forming on Ti-6Al-4V powder during oxidation10.1016/j.actamat.2023.119037 ↗
49. Oxidation of nickel-based single-crystal superalloys for industrial gas turbine applications10.1016/j.actamat.2010.09.027 ↗
50. Effect of zr on microstructure and oxidation behavior of α and α + α2Ti-Al-Nb alloys10.2320/matertrans.MAW201603 ↗
51. Electronic structure and reactivity of Ce- and Zr-Doped TiO2: assessing the reliability of density functional theory approaches10.1021/jp203112p ↗