Studying the formation of nodules in a Ni-Fe-Cr based superalloy used in fireside corrosion under the impact of creep stress
Source abstract
Abstract
Creep rupture tests on a Ni-Fe-Cr based superalloy were conducted in a custom-built rig at 750 °C under simulated fireside corrosion environment. The impact of creep stress on corrosion was investigated by controlling load level (without loading, loads of 120–195 MPa). The phase composition, microstructure, and morphology of surface corrosion products and corrosion-affected area were studied. The mechanism responsible for the production of surface nodules and the observed uniform oxide scale during fireside corrosion are discussed. Results show that the presence of creep stress promotes the development of surface nodules and increases the corrosion-affected area.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Material Properties and Failure Mechanisms · Coal Combustion and Slurry Processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Fireside corrosion of superheaters: effects of air and oxy-firing of coal and biomass10.1016/j.fuel.2011.03.010 ↗
2. Fireside issues in advanced power generation systems10.1179/1743284712Y.0000000133 ↗
3. High efficiency electric power generation: the environmental role10.1016/j.pecs.2006.08.002 ↗
4. Overview of the efficient tehnologies for power generation based on coal
5. Materials for boilers operating under supercritical steam conditions10.1533/9780857097514.1.81 ↗
6. Fireside corrosion in pc-fired boilers10.1016/0360-1285(90)90048-8 ↗
7. Application of coatings to alleviate fireside corrosion on heat transfer tubes during the combustion of low-grade solid fuels: a review10.1021/acs.energyfuels.0c02145 ↗
8. The multiple value characteristics of fly ash from Indian coal thermal power plants: a review10.1007/s10661-022-10473-2 ↗
9. Fundamental challenges and engineering opportunities in flue gas desulfurization wastewater treatment at coal fired power plants
10. Failure of 2.25Cr–1Mo steel superheater tubes in a fluidized bed combustor due to fireside corrosion10.1016/j.matchar.2010.10.012 ↗
11. Trends in fireside corrosion damage to superheaters in air and oxy-firing of coal/biomass10.1016/j.fuel.2013.04.005 ↗
12. Impact of fireside corrosion on the creep rupture life and oxide scale structure of a super304H boiler tube10.5006/4277 ↗
13. Creep rupture of a Ni-Fe based model alloy under simulated fireside corrosion in coal-fired boilers10.1016/j.corsci.2023.111536 ↗
14. An investigation of oxidation/hot corrosion-creep interaction at 800 °C in a Ni-base superalloy coated with salt mixture deposits of Na2SO4-NaCl-NaVO310.1016/j.corsci.2018.11.029 ↗
15. A newly developed Wrought Ni-Fe-Cr-based superalloy for advanced ultra-supercritical power plant applications beyond 700 degrees C10.1007/s40195-015-0298-5 ↗
16. Effect of the application of a mechanical load on the oxide-layer microstructure and on the oxidation mechanism of Ni-20Cr foils10.1023/A:1004553623556 ↗
17. Fatigue–oxidation–creep damage model under axial-torsional thermo-mechanical loading10.1177/1056789519887217 ↗
18. Influence of stress and secondary orientation on the oxidation-induced dynamic recrystallization behavior of a Ni-based single crystal superalloy10.1016/j.jallcom.2017.02.251 ↗
19. Subsurface microstructural degeneration of Super304H boiler tube under the synergy of fireside corrosion and creep stress10.1016/j.corsci.2022.110250 ↗
20. Static and dynamic aspects of coupling between creep behavior and oxidation on MC2 single crystal superalloy at 1150 °C10.1016/j.actamat.2005.05.018 ↗
21. Effects of imposed stresses on high temperature corrosion behaviour of T9110.1016/j.corsci.2021.109595 ↗
22. Temperature dependence of deformation mechanisms and tensile strength of a new Ni-Fe-base superalloy10.1016/j.matchar.2018.05.032 ↗
23. Surface oxidation studies of Al-2 wt% Li thin films10.1007/BF02744516 ↗
24. Study of thin oxidation films on iron-alloys by Raman-spectroscopy10.1016/0040-6090(89)90878-X ↗
25. Raman spectra of titanium dioxide (anatase, rutile) with identified oxygen isotopes (16, 17, 18)10.1039/c2cp42763j ↗
26. Effects of corrosion in supercritical CO2 on the microstructural evolution in 800H alloy10.1007/s11085-018-9852-7 ↗
27. Multi-scale analyses of phase transformation mechanisms and hardness in linear friction welded Ti17(α + β)/Ti17(β) dissimilar titanium alloy joint10.1016/j.cja.2023.08.018 ↗
28. Fuel ash corrosion of boiler and superheater tubes10.1023/A:1018585129341 ↗
29. Investigation of fireside corrosion of austenitic heat-resistant steel 10Cr18Ni9Cu3NbN in ultra-supercritical power plants10.1016/j.engfailanal.2019.02.048 ↗
30. Short-term corrosion behavior of polycrystalline Ni3Al-based superalloy in sulfur-containing atmosphere10.1016/j.intermet.2021.107446 ↗
31. Oxidation behavior of K4750 alloy at temperatures between 750 °C and 1000 °C10.1007/s40195-021-01235-z ↗
32. Effect of temperature on coal ash hot corrosion resistance of Inconel 740 superalloy10.1016/j.corsci.2014.01.020 ↗
33. Determination of the initiation and propagation mechanism of fireside corrosion10.1007/s11085-015-9559-y ↗
34. A review on molten sulfate salts induced hot corrosion10.1016/j.jmst.2021.03.013 ↗
35. Effect of nickel base superalloy composition on oxidation resistance in SO2 containing, high pO2 environments10.1002/maco.201307299 ↗
36. Localized oxidation of Zr-2.5Nb alloy in high temperature carbon dioxide environment containing hydrochloric acid10.1016/j.corsci.2019.108236 ↗
37. Nodular corrosion of zirconium alloys in gaseous environment containing different contaminants10.1016/j.jnucmat.2020.152640 ↗
38. Growth of nodular corrosion products on Fe–Al alloys in various high-temperature gaseous environments10.1023/A:1004658530596 ↗
39. Mechanism of zircaloy nodular corrosion10.1016/0022-3115(83)90199-X ↗
40. Delayed hydride cracking of Zr-2.5 %Nb pressure tube material due to partially constrained precipitates10.1016/j.jnucmat.2018.10.040 ↗
41. Effect of surface finishing on the oxidation characteristics of a Fe-21Cr-32Ni alloy in supercritical carbon dioxide10.1016/j.corsci.2021.110019 ↗
42. High-temperature oxidation behavior of a directionally solidified superalloy repaired by directed energy deposition10.1016/j.corsci.2021.109918 ↗
43. Low cycle fatigue of a single crystal CoNi-base superalloy10.1016/j.msea.2021.142007 ↗
44. Gradient-corrected density functional calculation of structural and magnetic properties of BCC, FCC and HCPCr10.1016/S0304-8853(99)00654-X ↗
45. Effect of alloying chemistry on fireside corrosion behavior of Ni–Fe-based superalloy for ultra-supercritical boiler applications10.1007/s11085-017-9804-7 ↗
46. Mechanical properties of oxide scales10.1007/BF01046722 ↗
47. Effects of external stress on high-temperature corrosion behavior of T92 ferrite steel with Na2SO4-K2SO4 molten salts