journal article·2025-11

Corrosion behavior of extra-high-purity type 316 austenitic stainless steel in a liquid lead–bismuth eutectic with oxygen saturation or low oxygen concentrations

Eriko Irisawa, Chiaki Kato

Corrosion Science· Volume 256
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Nuclear reactor physics and engineering · Nuclear Materials and Properties · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. C.F. Smith, L. Cinotti, Lead-cooled fast reactor, in: I.L. Pioro (Ed.) Handbook of Generation Iv Nuclear Reactors, 2016, pp. 119-155.10.1016/B978-0-08-100149-3.00006-9 ↗
2. Structural materials for Gen-IV nuclear reactors: challenges and opportunities10.1016/j.jnucmat.2008.08.044 ↗
3. Nuclear Energy Agency · 2015
4. A review of steel corrosion by liquid lead and lead-bismuth10.1016/j.corsci.2009.03.013 ↗
5. Corrosion of stainless steels in lead-bismuth eutectic up to 600 °C10.1016/j.jnucmat.2004.07.012 ↗
6. Liquid metal corrosion of T91 and A316L materials in Pb-Bi eutectic at temperatures 400-600 °C10.1016/j.corsci.2005.04.001 ↗
7. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb-Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
8. Corrosion behavior of austenitic steels in liquid lead bismuth containing 10−6 wt% and 10−8 wt% oxygen at 400-500 °C10.1016/j.jnucmat.2014.01.046 ↗
9. Corrosion of metallic materials in flowing liquid lead-bismuth
10. Corrosion behaviour of steels and refractory metals and tensile features of steels exposed to flowing PbBi in the LECOR loop10.1016/S0022-3115(03)00009-6 ↗
11. Behavior of steels in flowing liquid PbBi eutectic alloy at 420-600 °C after 4000–7200 h10.1016/j.jnucmat.2004.07.010 ↗
12. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
13. Modeling of oxidation of structural materials in LBE systems10.1016/j.jnucmat.2007.07.022 ↗
14. Models of liquid metal corrosion10.1016/j.jnucmat.2010.05.024 ↗
15. Dissolution mechanism of 316L in lead-bismuth eutectic at 500 °C10.1016/j.corsci.2011.05.031 ↗
16. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 520 °C10.1016/j.jnucmat.2015.11.005 ↗
17. Nuclear Energy Agency · 2015
18. Nickel solubility limit in liquid lead-bismuth eutectic10.1016/j.jnucmat.2010.03.008 ↗
19. Thermodynamic assessment of solubility and activity of iron, chromium, and nickel in lead bismuth eutectic10.1016/j.jnucmat.2014.03.011 ↗
20. Dissolution corrosion of 316L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LSE) at 500 °C10.1016/j.jnucmat.2017.04.004 ↗
21. Orientation relationship of the austenite-to-ferrite transformation in austenitic stainless steels due to dissolution corrosion in contact with liquid Pb-Bi eutectic10.1016/j.scriptamat.2019.03.035 ↗
22. Influence of plastic deformation on dissolution corrosion of type 316L austenitic stainless steel in static, oxygen-poor liquid lead-bismuth eutectic at 500°C10.5006/2400 ↗
23. Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500 °C10.1016/j.matchar.2021.111234 ↗
24. Characterization of oxide layers grown on D9 austenitic stainless steel in lead bismuth eutectic10.1016/j.jnucmat.2007.12.005 ↗
25. Transmission electron electron microscopy study of complex oxide scales on DIN 1.4970 steel exposed to liquid Pb-Bi eutectic10.1016/j.corsci.2018.10.018 ↗
26. AFM and MFM characterization of oxide layers grown on stainless steels in lead bismuth eutectic10.1016/j.jnucmat.2008.02.013 ↗
27. Structural, electrical and magnetic measurements on oxide layers grown on 316L exposed to liquid lead-bismuth eutectic10.1016/j.jnucmat.2011.11.042 ↗
28. Transmission electron microscopy (TEM) on oxide layers formed on D9 stainless steel in lead bismuth eutectic (LBE)10.1016/j.corsci.2012.09.019 ↗
29. Intergranular corrosion for extra high purity austenitic stainless steel in boiling nitric acid with Cr(VI)10.1299/jpes.3.31 ↗
30. Extra high purity alloy EHP for next generation nuclear systems
31. The effect of sulfur and phosphorus on the intergranular corrosion of 304 stainless steel10.5006/0010-9312-36.9.497 ↗
32. Effects of impurities on environmentally assisted crack growth of solution-annealed austenitic steels in primary water at 325°C10.5006/1.3280550 ↗
33. Environmentally assisted cracking of types 304L/316L/316NG stainless steel in 288°C water10.5006/1.3582044 ↗
34. Effect of dissolved oxygen concentration on the corrosion behavior of stainless steel in liquid lead-bismuth alloy
35. Electrochemical oxygen sensors for on-line monitoring in lead-bismuth alloys: status of development10.1016/j.jnucmat.2004.07.020 ↗
36. Diffusivity, activity and solubility of oxygen in liquid lead and lead-bismuth eutectic alloy by electrochemical methods10.1016/j.jnucmat.2005.10.006 ↗
37. Nuclear Energy Agency, Handbook on Lead-bismuth Eutectic Alloy and Lead Properties, Materials Compatibility, Thermal-hydraulics and Technologies – 2015 Edition, Thermodynamic relationships and heavy liquid metal interaction with other coolants (Chapter 3), OECD Publishing, Paris (2015).
38. The distribution of cations in metal oxide and metal sulphide solid solutions formed during the oxidation of alloys10.1016/S0010-938X(69)80046-6 ↗
39. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
40. Oxidation mechanism of an Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy at 470 °C (Part II)10.1016/j.corsci.2008.06.051 ↗
41. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part III)10.1016/j.corsci.2008.06.049 ↗
42. Internal external transition for the oxidation of fe-Cr-Ni austenitic stainless-steels in steam10.1007/BF00665267 ↗
43. SCALING OF AUSTENITIC STAINLESS-STEELS AND NICKEL-BASE ALLOYS IN HIGH-TEMPERATURE STEAM AT 973-K10.5006/1.3585251 ↗
44. Influence of dislocations on diffusion kinetics in solids with particular reference to alkali halides10.1039/tf9615701191 ↗
45. On the role of dislocations in bulk diffusion10.1016/0001-6160(57)90127-X ↗
46. Low temperature grain boundary diffusion of chromium in SUS316 and 316L stainless steels10.2320/matertrans.45.2945 ↗
47. Comparison of the corrosion behavior of austenitic and ferritic/martensitic steels exposed to static liquid Pb-Bi at 450 and 550 °C10.1016/j.jnucmat.2004.07.064 ↗
48. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead-bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
49. Effect of silicon on the oxidation resistance of 9 wt% Cr heat resistance steels in 550 °C lead-bismuth eutectic10.1016/j.corsci.2016.04.020 ↗
50. Effect of silicon on dynamic/static corrosion resistance of T91 in lead-bismuth eutectic at 550 °C
51. Effect of silicon on the oxidation resistance of 9% Cr steels10.1016/S0169-4332(02)01505-2 ↗
52. Silicon effects on the wet oxidation of type 310 stainless steel10.1016/j.corsci.2018.08.011 ↗
53. Modelling Cr depletion under a growing Cr2O3 layer on austenitic stainless steel: the influence of grain boundary diffusion10.1088/0965-0393/17/3/035009 ↗
54. Hot Corrosion of Metals by Molten Salts
55. Hot corrosion of materials: a fluxing mechanism10.1016/S0010-938X(01)00057-9 ↗