journal article·2025-10

Insights into the role of multiple microstructural characteristics in hydrogen embrittlement of pipeline steel under high-pressure hydrogen environment

Chen Sun, Haoqian Ma, Meng Xu, Xin Li, Jing Liu, Meifeng Li, Chungen Zhou

Corrosion Science· Volume 255
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (71)

Show source-provided references
1. Hydrogen related degradation in pipeline steel: A review10.1016/j.ijhydene.2018.06.064 ↗
2. Hydrogen induced cracking of pipeline and pressure vessel steels: A review10.1016/j.engfracmech.2018.06.018 ↗
3. Hydrogen embrittlement in hydrogen-blended natural gas transportation systems: A review10.1016/j.ijhydene.2023.04.266 ↗
4. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
5. Enhanced hydrogen embrittlement of low-carbon steel to natural gas/hydrogen mixtures10.1016/j.scriptamat.2020.08.011 ↗
6. Enhanced hydrogen embrittlement of steel by the premature hydrogen dissociation with the increasing inert gas pressure in hydrogen-containing mixtures10.1016/j.actamat.2023.119279 ↗
7. The role of reversed austenite in hydrogen embrittlement fracture of S41500 martensitic stainless steel10.1016/j.actamat.2017.08.011 ↗
8. Effect of hydrogen on tensile properties and fracture behavior of PH 13-8 Mo steel10.1016/j.matdes.2016.06.110 ↗
9. Modeling hydrogen induced damage mechanisms in metals, in: Gaseous Hydrogen Embrittlement of Materials in Energy Technologies: Mechanisms
10. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
11. Mechanisms of Hydrogen Related Fracture - A Review
12. Hydrogen effects on deformation - Relation between dislocation behavior and the macroscopic stress-strain behavior10.1016/0956-716X(94)90166-X ↗
13. Microstructural and crystallographic study of hydrogen-assisted cracking in high strength PSB1080 steel
14. The advantage of grain refinement in the hydrogen embrittlement of Fe-18Mn-0.6C twinning-induced plasticity steel10.1016/j.corsci.2015.01.012 ↗
15. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
16. Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials10.1016/j.actamat.2009.05.012 ↗
17. Study on the Hydrogen Embrittlement of Aermet100 Using Hydrogen Permeation and SSRT Techniques
18. Prediction of hydrogen-assisted fracture under coexistence of hydrogen-enhanced plasticity and decohesion10.1016/j.ijhydene.2023.06.033 ↗
19. Hydrogen-enhanced-plasticity mediated decohesion for hydrogen-induced intergranular and “quasi-cleavage” fracture of lath martensitic steels10.1016/j.jmps.2017.12.016 ↗
20. Investigation of the hydrogen induced cracking behaviour of API 5L X65 pipeline steel10.1016/j.ijhydene.2020.04.211 ↗
21. Review of Hydrogen Embrittlement in Metals: Hydrogen Diffusion, Hydrogen Characterization, Hydrogen Embrittlement Mechanism and Prevention10.1007/s40195-020-01039-7 ↗
22. Hydrogen embrittlement testing procedure for the analysis of structural steels with Small Punch Tests using notched specimens10.1016/j.engfracmech.2021.107906 ↗
23. Experimental investigation on the hydrogen embrittlement characteristics and mechanism of natural gas-hydrogen transportation pipeline steels10.1088/2053-1591/ac6654 ↗
24. A comparative study of hydrogen induced cracking behavior in API 5L X60 and X70 pipeline steels10.1016/j.engfailanal.2013.04.028 ↗
25. Deformation microstructures of a low carbon steel characterized by tritium autoradiography and thermal desorption spectroscopy, Nippon Kinzoku Gakkaishi/10.2320/jinstmet1952.58.10_1141 ↗
26. Hydrogen-induced cracking in a very-high-purity high-strength steel10.1016/j.msea.2008.03.012 ↗
27. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
28. Hydrogen-induced intergranular failure of iron10.1016/j.actamat.2014.01.060 ↗
29. Effect of hydrogen environment on the separation of Fe grain boundaries10.1016/j.actamat.2016.01.067 ↗
30. Characterization of Hydrogen-Related Fracture Behavior in As-Quenched Low-Carbon Martensitic Steel and Tempered Medium-Carbon Martensitic Steel
31. Microstructural and crystallographic features of hydrogenrelated crack propagation in low carbon martensitic steel10.2355/isijinternational.52.208 ↗
32. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
33. Mitigation of hydrogen embrittlement in ultra-high strength lath martensitic steel via Ta microalloying10.1016/j.matdes.2021.110090 ↗
34. Effect of specific microstructures on hydrogen embrittlement susceptibility of a modified AISI 4130 steel10.1016/j.ijhydene.2021.08.147 ↗
35. Enhancement of the resistance to hydrogen embrittlement by tailoring grain boundary characteristics in a low carbon high strength steel10.1016/j.jmrt.2023.11.156 ↗
36. An understanding of hydrogen embrittlement in nickel grain boundaries from first principles10.1016/j.matdes.2021.110283 ↗
37. Grain size and grain-boundary effects on diffusion and trapping of hydrogen in pure nickel10.1016/j.actamat.2012.09.004 ↗
38. Effects of grain size and dislocation density on the susceptibility to high-pressure hydrogen environment embrittlement of high-strength low-alloy steels10.1016/j.ijhydene.2011.10.099 ↗
39. Critical grain size to limit the hydrogen-induced ductility drop in a metastable austenitic steel10.1016/j.ijhydene.2015.06.111 ↗
40. Effect of grain refinement on hydrogen embrittlement behaviors of high-Mn TWIP steel10.1016/j.msea.2015.11.017 ↗
41. Effect of austenite grain size on the bainitic ferrite morphology and grain refinement of a pipeline steel after continuous cooling10.1016/j.matchar.2016.11.025 ↗
42. Susceptibility of different crystal orientations and grain boundaries of polycrystalline Ni to hydrogen blister formation10.1016/j.ijhydene.2019.01.263 ↗
43. Atomistic investigation of the role of grain boundary structure on hydrogen segregation and embrittlement in α-Fe10.1007/s11661-012-1430-z ↗
44. Effects of grain boundary- and triple junction-character on intergranular fatigue crack nucleation in polycrystalline aluminum10.1007/s10853-007-2236-z ↗
45. A critical perspective on pipeline processing and failure risks in hydrogen service conditions10.1016/j.jallcom.2020.158240 ↗
46. Is Hydrogen Diffusion along Grain Boundaries Fast or Slow? Atomistic Origin and Mechanistic Modeling10.1103/PhysRevLett.122.215501 ↗
47. Application of electron backscatter diffraction (EBSD) to fracture studies of ferritic steels10.1046/j.1365-2818.2002.00998.x ↗
48. On the role of crystallographic texture in mitigating hydrogen-induced cracking in pipeline steels10.1016/j.corsci.2011.08.031 ↗
49. A new understanding of intergranular stress corrosion cracking resistance of pipeline steel through grain boundary character and crystallographic texture studies10.1016/j.corsci.2008.10.006 ↗
50. Role of lattice strain and texture in hydrogen embrittlement of 18Ni (300) maraging steel10.1016/j.ijhydene.2017.03.209 ↗
51. Texture, local misorientation, grain boundary and recrystallization fraction in pipeline steels related to hydrogen induced cracking10.1016/j.msea.2014.10.009 ↗
52. Hydrogen-assisted stress cracking of high-strength wheel bolts10.1016/S1350-6307(96)00023-4 ↗
53. On hydrogen-induced Vickers indentation cracking in high-strength steel10.1016/j.mechrescom.2010.01.001 ↗
54. Unveiling the nature of hydrogen embrittlement in bearing steels employing a new technique10.1016/j.scriptamat.2012.11.018 ↗
55. G. Kresse, J. Hafner, Ab initio molecular dynamics for open-shell transition metals, 1993.10.1103/PhysRevB.48.13115 ↗
56. Projector augmented-wave method10.1103/PhysRevB.50.17953 ↗
57. Generalized gradient approximation made simple10.1103/PhysRevLett.77.3865 ↗
58. J.P. Perdew, K. Burke, M. Ernzerhof, Generalized Gradient Approximation Made Simple, 1996.10.1103/PhysRevLett.77.3865 ↗
59. Slip planes in bcc transition metals10.1179/1743280412Y.0000000015 ↗
60. Phase transformation induced transitional twin boundary in body-centered cubic metals10.1016/j.actamat.2023.118815 ↗
61. Enhancement of fatigue resistance of additively manufactured 304L SS by unique heterogeneous microstructure10.1080/17452759.2021.1881869 ↗
62. The difference in fatigue crack growth induced by internal and external hydrogen in selective laser melted 304L stainless steel10.1016/j.ijfatigue.2022.107052 ↗
63. Thermal desorption spectroscopy evaluation of the hydrogen-trapping capacity of NbC and NbN precipitates10.1007/s11661-013-2181-1 ↗
64. Delayed Fracture Properties of 1500 MPa Bainite/Martensite Dual-phase High Strength Steel and Its Hydrogen Traps10.2355/isijinternational.42.1560 ↗
65. A classification of hydrogen traps in steel10.1007/BF02812023 ↗
66. Evaluation of hydrogen trapping in high strength steels by thermal desorption spectroscopy10.1016/j.msea.2012.04.078 ↗
67. Suppressing hydrogen embrittlement of a CrCoNi medium-entropy alloy by triggering co-segregation of carbon, boron, and Cr10.1016/j.corsci.2024.112232 ↗
68. Role of crystallographic texture on the improvement of hydrogen-induced crack resistance in API 5L X70 pipeline steel10.1016/j.ijhydene.2016.10.124 ↗
69. Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing10.1016/j.corsci.2016.05.003 ↗
70. On the synergy of diffusible hydrogen content and hydrogen diffusivity in the mechanical degradation of laboratory cast Fe-C alloys10.1016/j.msea.2016.03.107 ↗
71. Hydrogen embrittlement mechanisms in advanced high strength steel10.1016/j.actamat.2021.117488 ↗