Improved mechanical properties and hydrogen environment assisted cracking resistance of a secondary hardening ultra-high strength steel via double aging treatment

Lijin Dong, Maozhang Wu, Dong Ling, Hongli Wang, Huaibei Zheng, Cheng Ma, Li Liu, Qinying Wang

Corrosion Science· Volume 246
Publisher page

Abstract

Mechanical properties and hydrogen environment assisted cracking (HEAC) resistance of AerMet 100 steel after single and double aging treatments were investigated. The fracture toughness increased by 10 –25 % after double aging treatment due to the higher faction of reversed austenite. Stronger hydrogen traps formed after double aging treatment decreased hydrogen diffusion rates. The double aging treatment increased the K TH by 20–60 % while lowered the d a/d t II by 25–70 %. The improvement of HEAC resistance was related to the suppressed hydrogen diffusion and partitioning to the crack tip by carbides and reversed austenite, along with the enhanced austenite stability by Ni enrichment.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (71)

Show source-provided references
1. Microstructure characterization and mechanical behaviour of laser additive manufactured ultrahigh-strength M54 steel
2. Revealing the evolution behavior of multiple carbides precipitation and mechanical response in M54 secondary hardening steel
3. E. Lee, M. stanley, B. Pregger, C. Lei, E. Lipnickas. Ferrium M54 Steel, Report No: NAWCADPAX/TIM-2014/292, Defense Technical Information Center, 2015.
4. J. Quan. Ausforming and tempering of a computationally designed ultra-high strength steel, University of Virginia, Ph. D. thesis, 2018. 〈https://www.proquest.com/dissertations-theses/ausforming-tempering-computationally-designed/docview/2139678073/se-2?accountid= 132643〉.
5. Materials considerations for aerospace applications
6. Understanding the correlation of aging treatments and stress corrosion crack growth of a secondary hardening ultra-high strength steel
7. Insights into the stress corrosion cracking of M54 ultra-high-strength steel in the marine environments at varying temperatures by comparison of slow strain rate tensile and crack growth tests
8. Internal hydrogen embrittlement of ultrahigh-strength AERMET 100 steel
9. G. Pioszak, Hydrogen assisted cracking of ultra-high strength steels, University of Virginia, Ph. D. thesis, 2015.
10. Measurement and modeling of hydrogen environment–assisted cracking of ultra-high-strength steel10.1007/s11661-006-9051-z ↗
11. Garrison · Ultrah. -Strength Steels Aerosp. Appl. · 1990 · 42 · 20
12. Effects of microstructures on the fatigue crack growth behavior of laser additive manufactured ultrahigh-strength AerMet100 steel10.1016/j.msea.2018.02.088 ↗
13. Sun · Eval. Microstruct. Fatigue Prop. Laser cladding Repair Ultrah. Strength AerMet® 100 Steel · 2015 · 27
14. Lourenço · Fatigue Fract. Behav. Laser clad Repair AerMet® 100 Ultra-High. Strength Steel · 2016 · 85 · 18
15. Wang · Evol. a Microstruct. tempering its Influ. Mech. Prop. AerMet 100 Steel, Mater. · 2023 · 16 · 6907
16. On the characteristics of M2C carbides in the peak hardening regime of AerMet 100 steel10.1007/s11661-998-0280-1 ↗
17. Influence of cooling rate during cryogenic treatment on the hierarchical microstructure and mechanical properties of M54 secondary hardening steel10.1016/j.msea.2022.143659 ↗
18. Improvement of toughness of ultrahigh strength steel AerMet 100
19. Effect of solid-solution temperature on the microstructure and properties of ultra-high-strength ferrium S53® steel10.1016/j.msea.2018.05.099 ↗
20. Controlling the MC and M2C carbide precipitation in Ferrium® M54® steel to achieve optimum ultimate tensile strength/fracture toughness balance10.1016/j.matchar.2018.03.041 ↗
21. Austenite and precipitation in secondary-hardening ultra-high-strength stainless steel10.1016/j.matchar.2018.07.038 ↗
22. Experimental verification of segregation of carbon and precipitation of carbides due to deep cryogenic treatment for tool steel by internal friction method10.1016/j.msea.2013.03.070 ↗
23. Warm tempforming effect on the hydrogen embrittlement of 1.8-GPa-class ultra-high-strength low-alloy steel10.1016/j.msea.2017.07.091 ↗
24. A review of hydrogen embrittlement of martensitic advanced high-strength steels10.1515/corrrev-2016-0006 ↗
25. Hydrogen trapping and hydrogen embrittlement in 15-5PH stainless steel10.1016/j.corsci.2022.110416 ↗
26. Hydrogen trap states in ultrahigh-strength AERMET 100 steel10.1007/s11661-004-0011-1 ↗
27. Hydrogen diffusion and trapping in laser additively manufactured ultra-high strength AerMet100 steel10.5006/3812 ↗
28. Hydrogen environment assisted cracking of modern ultra-high strength martensitic steels10.1007/s11661-017-4156-0 ↗
29. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
30. Microstructural effects on the toughness of a high Co–Ni steel10.1002/adem.201600633 ↗
31. Meta-equilibrium transition microstructure for maximum austenite stability and minimum hardness in a Ti-stabilized supermartensitic stainless steel10.1016/j.matdes.2018.07.018 ↗
32. Double-step inter-critical tempering of a supermartensitic stainless steel: evolution of hardness, microstructure and elemental partitioning10.1016/j.matchar.2019.109994 ↗
33. Influence of deep cryogenic treatment and secondary tempering on microstructure and mechanical properties of medium-carbon low-alloy steels10.1007/s11665-019-04532-y ↗
34. The morphology and crystallography of lath martensite in Fe-C alloys10.1016/S1359-6454(02)00577-3 ↗
35. M. Tanaka, C.S. Choi. The effects of carbon contents and Ms temperatures on the hardness of martensitic Fe-Ni-C Alloys, Trans. Iron Steel Inst. Japan, 12 (972) 16-25. https://doi.org/10.2355/isijinternational1966.12.16.10.2355/isijinternational1966.12.16 ↗
36. Effect of two steps annealing on the microstructure and dynamic strain aging behavior of Al-6Mg alloy10.1016/j.msea.2020.140097 ↗
37. X-ray diffraction study on cooling-rate-induced γ fcc → ε hcp martensitic transformation in cast-homogenized Fe-26Mn-0.14C austenitic steel10.1007/s11661-007-9240-4 ↗
38. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
39. Evaluation of the dislocation density and dislocation character in cold rolled Type 304 steel determined by profile analysis of X-ray diffraction10.1016/j.actamat.2011.03.055 ↗
40. On the relative efficacy of electropermeation and isothermal desorption approaches for measuring hydrogen diffusivity10.1016/j.ijhydene.2022.10.025 ↗
41. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
42. Environmentally assisted cracking in the fusion boundary region of a SA508-Alloy 52M dissimilar weld joint in simulated primary pressurized water reactor environments10.1016/j.corsci.2021.109668 ↗
43. Stress corrosion cracking in the heat affected zone of a stainless steel 308L-316L weld joint in primary water10.1016/j.corsci.2016.02.030 ↗
44. Environmentally assisted crack growth in 308L stainless steel weld metal in simulated primary water10.1016/j.corsci.2016.12.011 ↗
45. High-pressure corrosion fatigue experiments employing diverse methodologies for assessing rates of crack propagation10.1016/j.jmrt.2024.07.058 ↗
46. Experimental comparison of gaseous and electrochemical hydrogen charging in X65 pipeline steel using the permeation technique10.1016/j.corsci.2023.111025 ↗
47. A novel heat treatment for improving the hydrogen embrittlement resistance of a precipitation-hardened martensitic stainless steel10.1016/j.corsci.2022.110530 ↗
48. Investigation of the mechanical stability of reversed austenite in 13%Cr-4%Ni martensitic stainless steel during the uniaxial tensile test10.1016/j.msea.2013.08.028 ↗
49. Structures of M2C carbides and its influence on strengthening in AerMet100 steel at the typical tempering temperature 482 °C10.1016/j.vacuum.2023.112209 ↗
50. Transmission electron microscopy examination of hardening and toughening phenomena in Aermet 10010.1007/BF02666329 ↗
51. Microstructural effects on the toughness of a high Co-Ni Steel10.1002/adem.201600633 ↗
52. Formation and growth kinetics of reverted austenite during tempering of a high Co-Ni steel10.1007/s11661-016-3760-8 ↗
53. Effect of intercritical annealing on the microstructure and mechanical properties of a PH 13-8 Mo maraging steel10.1016/j.msea.2024.146220 ↗
54. Reverted austenite in PH 13-8 Mo maraging steels10.1016/j.matchemphys.2010.02.058 ↗
55. Microstructure analysis and yield strength simulation in high Co-Ni secondary hardening steel10.1016/j.msea.2016.05.069 ↗
56. Study on the microstructure and mechanical properties of Aermet 100 steel at the tempering temperature around 482 °C10.1016/j.jallcom.2016.04.087 ↗
57. Size effects on martensitic phase transformations in nanocrystalline NiTi shape memory alloys10.1179/174328408X302620 ↗
58. Stability and TRIP effect of retained austenite of medium manganese Q&P steel
59. Hydrogen degradation of steels and its related parameters, a review10.1080/01411594.2011.561774 ↗
60. Comparative study on the crack growth behaviours of E690 steel and heat-affected zone microstructures under cathodic potential in artificial seawater based on mechano-electrochemical effect at crack tip10.1016/j.corsci.2022.110103 ↗
61. The effect of crack tip environment on crack growth behaviour of a low alloy steel at cathodic potentials in artificial seawater10.1016/j.jmst.2020.04.034 ↗
62. Factors distinguishing hydrogen-assisted intergranular and intergranular-like fractures in a tempered lath martensitic steel10.1007/s11661-022-06608-2 ↗
63. Hierarchical characteristics of hydrogen-assisted crack growth and microstructural strain evolution in tempered martensitic steels: case of quasi-cleavage fracture10.1007/s11661-021-06423-1 ↗
64. Martensite boundary characteristics on cycle-and time-dependent fatigue crack growth paths of tempered lath martensitic steels in a 90 MPa gaseous hydrogen atmosphere10.1007/s11661-023-07041-9 ↗
65. Characteristics and mechanisms of hydrogen-induced quasi-cleavage fracture of lath martensitic steel10.1016/j.actamat.2021.116635 ↗
66. Hydrogen transport and embrittlement in 300 M and AerMet100 ultra high strength steels10.1016/j.corsci.2010.01.001 ↗
67. Probabilistic fracture mechanics simulation of stress corrosion cracking using accelerated laboratory testing and multi-scale modeling10.5006/1920 ↗
68. The influence of cohesive forces on the equilibrium concentration of hydrogen atoms ahead of a crack tip in single crystal iron10.1016/0956-716X(92)90152-5 ↗
69. The equilibrium concentration of hydrogen atoms ahead of a mixed mode I-mode III crack tip in single crystal iron10.1007/s11661-999-0203-9 ↗
70. Fracture in mechanism-based strain gradient plasticity10.1016/S0022-5096(00)00070-3 ↗
71. Correlation between the microstructure and hydrogen embrittlement resistance in a precipitation-hardened martensitic stainless steel10.1016/j.corsci.2021.109260 ↗