Abstract

The role of solidification cell structure in hydrogen embrittlement (HE) in laser-powder bed fusion fabricated CoCrFeNi medium-entropy alloy is investigated by comparing as-built and annealed conditions. Annealing at 1100 °C dissolves the cell structure and induces partial recrystallization. This slightly reduced the strength but significantly improves HE resistance by suppressing hydrogen-assisted intergranular cracking. The results are discussed in terms of the changes in hydrogen trapping/diffusion behavior and deformation behavior upon removal of cell structure, as investigated through thermal desorption spectroscopy, Ag decoration, and digital image correlation technique.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. 3D ink-extrusion additive manufacturing of CoCrFeNi high-entropy alloy micro-lattices10.1038/s41467-019-08763-4 ↗
2. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
3. Additive manufacturing of advanced multi-component alloys: Bulk metallic glasses and high entropy alloys10.1002/adem.201700874 ↗
4. Recent advances on high-entropy alloys for 3D printing10.1002/adma.201903855 ↗
5. Improving the hydrogen embrittlement resistance of a selective laser melted high-entropy alloy via modifying the cellular structures10.1016/j.corsci.2021.109695 ↗
6. Corrosion resistance enhancement of CoCrFeMnNi high-entropy alloy fabricated by additive manufacturing10.1016/j.corsci.2020.108954 ↗
7. Additively manufactured hierarchical stainless steels with high strength and ductility10.1038/nmat5021 ↗
8. New insights on cellular structures strengthening mechanisms and thermal stability of an austenitic stainless steel fabricated by laser powder-bed-fusion10.1016/j.actamat.2020.11.018 ↗
9. About metastable cellular structure in additively manufactured austenitic stainless steels
10. Mesoscopic chemical heterogeneities in laser powder bed fused CoCrMo and Ni mixed powders and their effect on the mechanical properties10.1016/j.msea.2023.145795 ↗
11. Enhanced strengthening and hardening via self-stabilized dislocation network in additively manufactured metals10.1016/j.mattod.2021.06.002 ↗
12. Dislocation network in additive manufactured steel breaks strength–ductility trade-off10.1016/j.mattod.2017.11.004 ↗
13. Distinct effects of in-situ and ex-situ hydrogen charging methods on the mechanical behavior of CoCrFeNi high-entropy alloy fabricated by laser-powder bed fusion10.1016/j.jallcom.2023.168858 ↗
14. Fostering strengths against hydrogen embrittlement: insights from nanotwin-ability and post-treatment effects in additively manufactured CoCrFeMnNi10.1080/21663831.2024.2371521 ↗
15. Effect of annealing and hot isostatic pressing on the structure and hydrogen embrittlement resistance of powder-bed fusion-printed CoCrFeNiMn high-entropy alloys10.3390/met13030630 ↗
16. Effect of cell wall on hydrogen response in CoCrFeMnNi high-entropy alloy additively manufactured by selective laser melting10.1016/j.jallcom.2022.166735 ↗
17. Effect of deformation on hydrogen trapping and effusion in TRIP-assisted steel10.1016/j.actamat.2012.04.010 ↗
18. Hydrogen trapping and micromechanical behavior in additively manufactured CoCrFeNi high-entropy alloy in as-built and pre-strained conditions10.1016/j.actamat.2024.119886 ↗
19. Hydrogen delayed fracture properties and internal hydrogen behavior of a Fe–18Mn–1.5 Al–0.6C TWIP Steel10.2355/isijinternational.49.1952 ↗
20. Post-processing of additively manufactured high-entropy alloys: a review10.1016/j.jmrt.2022.11.027 ↗
21. Heat treatment for metal additive manufacturing10.1016/j.pmatsci.2022.101051 ↗
22. Hydrogen embrittlement in compositionally complex FeNiCoCrMn FCC solid solution alloy10.1016/j.cossms.2017.11.002 ↗
23. Effects of Mn content and grain size on hydrogen embrittlement susceptibility of face-centered cubic high-entropy alloys10.1007/s11661-020-05966-z ↗
24. Exploring the hydrogen absorption and strengthening behavior in nanocrystalline face-centered cubic high-entropy alloys10.1016/j.scriptamat.2021.114069 ↗
25. Effects of annealing on the structure and mechanical properties of FeCoCrNi high-entropy alloy fabricated via selective laser melting
26. Effect of homogenization and solution treatments time on the elevated-temperature mechanical behavior of Inconel 718 fabricated by laser powder bed fusion10.1038/s41598-021-81618-5 ↗
27. High-cycle fatigue induced twinning in CoCrFeNi high-entropy alloy processed by laser powder bed fusion additive manufacturing
28. The role of hydrogen in hardening/softening steel: influence of the charging process10.1016/j.scriptamat.2015.05.017 ↗
29. Hydrogen-induced nanohardness variations in a CoCrFeMnNi high-entropy alloy10.1016/j.ijhydene.2017.02.061 ↗
30. The trapping and transport phenomena of hydrogen in nickel10.1007/BF02643893 ↗
31. Hydrogen effects in equiatomic CrFeNiMn alloy fabricated by laser powder bed fusion10.3390/met11060872 ↗
32. Permeability, solubility and diffusivity of hydrogen isotopes in stainless steels at high gas pressures10.1016/j.ijhydene.2006.05.008 ↗
33. Grain refinement effect on hydrogen embrittlement resistance of an equiatomic CoCrFeMnNi high-entropy alloy10.1016/j.ijhydene.2019.04.280 ↗
34. Comparative study of hydrogen embrittlement resistance between additively and conventionally manufactured 304L austenitic stainless steels10.1016/j.msea.2020.140499 ↗
35. Hydrogen uptake and its influence in selective laser melted austenitic stainless steel: a nanoindentation study10.1016/j.scriptamat.2020.113718 ↗
36. Hydrogen trapping in laser powder bed fusion 316L stainless steel
37. A novel methodology to estimate hydrogen diffusivity and its applications in revealing hydrogen effects in CoCrNi medium-entropy alloy versus 316L stainless steel10.1016/j.ijplas.2023.103737 ↗
38. Hydrogen transport by dislocations10.1007/BF02644079 ↗
39. Hydrogen transport by mobile dislocations in nickel base superalloy single crystals10.1016/S1359-6462(98)00451-5 ↗
40. Modeling hydrogen transport by dislocations10.1016/j.jmps.2015.03.002 ↗
41. A micropillar compression investigation into the plastic flow properties of additively manufactured alloys10.1016/j.actamat.2022.118290 ↗
42. Hydrogen-enhanced localization of plasticity in an austenitic stainless steel10.1007/BF02669644 ↗
43. Strain hardening by dynamic slip band refinement in a high-Mn lightweight steel10.1016/j.actamat.2016.06.037 ↗
44. ω phase acts as a switch between dislocation channeling and joint twinning- and transformation-induced plasticity in a metastable β titanium alloy10.1016/j.actamat.2018.03.053 ↗
45. In-situ study of initiation and extension of nano-thick defect-free channels in irradiated nickel10.1016/j.jmst.2020.03.057 ↗
46. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
47. Hydrogen-assisted decohesion and localized plasticity in dual-phase steel10.1016/j.actamat.2014.01.048 ↗
48. The effect of nitrogen alloying on hydrogen-assisted plastic deformation and fracture in FeMnNiCoCr high-entropy alloys10.1016/j.scriptamat.2020.113642 ↗
49. Hydrogen-induced intergranular fracture of steels10.1016/S0013-7944(00)00124-7 ↗
50. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
51. The role of hydrogen and other interstitials in the mechanical behavior of metals10.1007/s13632-016-0319-4 ↗
52. Effect of tensile and compressive elastic stress on equilibrium hydrogen solubility in a solid10.1016/0001-6160(70)90039-8 ↗
53. The kinetics of hydrogen embrittlement: a quantitative diffusion model10.1016/0013-7944(74)90053-8 ↗
54. Hydrogen permeation behavior and hydrogen-induced defects in 316L stainless steels manufactured by additive manufacturing10.1016/j.matchemphys.2020.123038 ↗