journal article·2022-08

Erosion-corrosion behavior of Ni-20Cr-4Fe and Ni-20Cr-4Fe-7Mo under fluidized-bed biomass boiler conditions

Suzue Yoneda, Shigenari Hayashi, Yasuki Miyakoshi, Takashi Kogin, Eiji Ishikawa, Manabu Noguchi

Corrosion Science· Volume 205
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Erosion and Abrasive Machining · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Industrial waste combustion boiler installed at paper mill, Japan10.2524/jtappij.57.645 ↗
2. Link · Oxid. Met. · 1998 · 49 · 21310.1023/A:1018886509459 ↗
3. High temperature degradation by erosion-corrosion in bubbling fluidized bed combustors10.1590/S1516-14392004000100011 ↗
4. M. Manabu, H. Yakuwa, M. Miyasaka, H. Sakamoto, S. Kosugi, T. Narita, High temperature erosion-corrosion behavior of boiler tube materials in fluidized-bed waste incinerator conditions, High-temperature corrosion and protection (2000) 573–578.
5. Erosion-corrosion behavior of nickel and iron based superalloys in boiler environment10.1007/s11085-014-9509-0 ↗
6. Erosion-corrosion of preoxidised Incoloy 800H in fluidized bed environments: effect of temperature, velocity, and exposure time10.1179/mst.1991.7.12.1128 ↗
7. Erosion and corrosion of cooled 1018 steel10.1016/0043-1648(93)90451-Q ↗
8. Erosion-corrosion of mild steel in a temperature gradient10.1016/0043-1648(95)07185-7 ↗
9. A new method for the experimental evaluation of high-temperature erosion-corrosion in fluidized bed waste Incineration condition
10. High temperature erosion-oxidation behavior of nickel- based alloys containing Mo in fluidized bed waste incineration
11. Mechanism in the simultaneous erosion-oxidation attack of nickel and cobalt at high temperature10.1007/BF02646210 ↗
12. Some principal mechanisms in the simultaneous erosion and corrosion attack of metals at high temperatures10.1016/0921-5093(91)90739-A ↗
13. High temperature erosion-corrosion mechanisms, maps and models10.1016/j.wear.2003.04.003 ↗
14. The effect of oxide volatilization on the oxidation kinetics of Cr and Fe-Cr alloys10.1149/1.2424115 ↗
15. Paralinear oxidation of chromium in O2 + H2O environment at 600-700°C10.1007/s11085-008-9114-1 ↗
16. Paralinear oxidation of CVD SiC in water vapor
17. Birksm · 2006
18. Effect of Mo on corrosion behavior of Ni20Cr-xMo alloys in air with NaCl-KCl-CaCl2 vapor at 570oC10.1002/maco.201911469 ↗