Synergistic effects of Al2O3 and Y2O3 on enhancing the wet-oxidation resistance of SiC ceramics
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Magnesium Oxide Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. Phase-field simulation of microscale crack propagation/deflection in SiCf/SiC composites with weak interphase10.1111/jace.19117 ↗
2. The influence of grinding process on the mechanical behavior of SiC/SiC composite tubes under uniaxial tension10.1016/j.jeurceramsoc.2023.07.067 ↗
3. Fibre-reinforced multifunctional SiC matrix composite materials10.1080/09506608.2016.1213939 ↗
4. Recent advances in interphase engineering for improved behavior of SiCf/SiC composites10.1016/j.jeurceramsoc.2024.04.068 ↗
5. Insight into crack propagation induced by fiber orientations during single grain scratching of SiCf/SiC composites using FEM10.1016/j.compositesa.2023.107928 ↗
6. High-temperature oxidation resistance of SiCf/SiC composites annealed and cladded with LaMgAl11O19/Yb2Si2O7 thermal/environmental barrier coatings10.1016/j.corsci.2024.111962 ↗
7. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
8. Environmental degradation of high-temperature protective coatings for ceramic-matrix composites in gas-turbine engines10.1038/s41529-019-0075-4 ↗
9. Ceramic matrix composites taking flight at GE Aviation
10. Degradation of silicon carbide in combustion gas flow at high temperature and high speed10.1299/jsmea.44.520 ↗
11. Stressed oxidation behaviors of SiC matrix composites in combustion environments10.1016/j.matlet.2007.01.038 ↗
12. Oxidation behavior of 3D Hi-Nicalon/SiC composite exposed in wet and simulated air environments10.1016/j.corsci.2012.09.008 ↗
13. The tensile damage behavior of SiCf/SiC composites after oxidation in wet atmosphere
14. Oxidation of SiC/BN/SiC ceramic matrix composites in dry and wet oxygen at intermediate temperatures10.1016/j.jeurceramsoc.2022.04.003 ↗
15. Tension–tension fatigue damage characteristics of a 3D SiC/SiC composite in H2O–O2–Ar environment at 1300° C10.1016/j.msea.2006.07.041 ↗
16. Challenging ceramic matrix composites for applications in severe environments10.1163/156855195X00104 ↗
17. Oxidation resistance of SiC ceramics prepared by different proceessing routes10.1016/j.jeurceramsoc.2016.03.016 ↗
18. Improved wet-oxidation resistance of SiCf/SiC composites modified with Y2O310.5006/4150 ↗
19. Enhanced wet-oxidation resistance of Y2O3 modified SiC ceramics by the formation of Y2Si2O7 protective layer10.1016/j.jeurceramsoc.2023.04.039 ↗
20. Fabrication of SiCf/SiC composites by alternating current electrophoreticdeposition (AC-EPD) and hot pressing10.1016/j.jeurceramsoc.2014.09.011 ↗
21. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
22. Single- and multilayered interphases in SiC/SiC composites exposed to severe environmental conditions: an overview10.1111/j.1744-7402.2009.02424.x ↗
23. Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
24. Creep behavior in interlaminar shear of a SiC/SiC ceramic composite with a self-healing matrix10.1007/s10443-013-9366-z ↗
25. Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si-B-C/SiC coatings under wet oxygen atmosphere10.1016/j.apsusc.2015.06.153 ↗
26. Wet oxidation behavior of C/SiC–SiHf(B)CN composites at high temperature10.1007/s42114-020-00172-2 ↗
27. Oxidation behaviour of a boron carbide based material in dry and wet oxygen10.1023/A:1010133703284 ↗
28. Fatigue behavior of a Hi-Nicalon/SiC–B4C composite at 1200°C in air and in steam10.1016/j.msea.2011.11.049 ↗
29. Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
30. Effect of Al/Si ratio on the crystallization properties and structure of mold flux10.1016/j.conbuildmat.2019.04.261 ↗
31. Effect of Al2O3 on the densification and oxidation behavior of SiC coating for carbon/carbon composites10.1016/j.ceramint.2018.04.072 ↗
32. More effective crack self-healing capability of SiCf/SiC-B4C with Al2O3 modified under wet environment10.1111/jace.17371 ↗
33. The oxidation behavior and corrosion mechanism of SiC matrix ceramics in a high temperature wet air environment10.1016/j.jeurceramsoc.2024.116729 ↗
34. Wet oxidation behavior of Al-Y synergistic modified liquid phase sintered SiC
35. High temperature oxidation behaviors of bulk SiC with low partial pressures of air and water vapor in argon10.1016/j.corsci.2020.108795 ↗
36. Fabrication of SiC fiber reinforced titanium matrix composites processed with sprayed preforms10.2320/jinstmet1952.65.10_946 ↗
37. Variation of the oxidation rate of silicon carbide with water-vapor pressure10.1111/j.1151-2916.1999.tb01810.x ↗
38. Oxidation/corrosion of polymer-derived SiAlCN ceramics in water vapor10.1111/j.1551-2916.2005.00791.x ↗
39. Paralinear oxidation of Cr-Si-C coated C/SiC at 1300ºC in wet and dry air environments10.1007/s11837-019-03841-w ↗
40. Viscosity of liquid silica, silicates and alumino-silicates10.1016/0016-7037(82)90059-X ↗