Oxidation kinetics and mechanisms of aluminum modified ultra-pure low chromium ferritic stainless steels
Source abstract
Abstract
Abstract The oxidation behavior of ultra-pure low chromium ferritic stainless steels with aluminum contents of 0, 0.16, and 1.51 wt.% has been investigated at 800 and 1000 °C in air for up to 100 h. Aluminum promotes the appearance of parabolic nature of oxidation, and the parabolic rate constant significantly decreases to about 1.1 × 10−7 mg2 mm−4 h−1 at 1000 °C and 1.4 × 10−3 μg2 mm−4 h−1 at 800 °C for the steel with 1.51 wt.% Al. The TiO2 + Al2O3 oxide scale at 1000 °C and Al2O3 + Cr2O3 oxide scale at 800 °C significantly improve oxidation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Breakaway oxidation behavior of ferritic stainless steels at 1150 °C in humid air10.1016/j.corsci.2016.02.042 ↗
2. Thermally grown oxide films and corrosion performance of ferritic stainless steels under simulated exhaust gas condensate conditions10.1016/j.corsci.2014.06.041 ↗
3. High temperature oxidation behavior of ferritic stainless steel containing W and Ce10.1016/j.corsci.2018.07.017 ↗
4. Oxidation of AISI 304 and AISI 439 stainless steels10.1016/j.msea.2006.10.022 ↗
5. Effects of alloyed La, Cu and B on the oxidation of Fe-22Cr ferritic stainless steels under simulated cathode side atmosphere of solid oxide fuel cell interconnects10.1016/j.corsci.2018.01.025 ↗
6. High temperature oxidation of Co-W electroplated type 430 stainless steel for the interconnect of solid oxide fuel cells10.1016/j.corsci.2018.02.026 ↗
7. Microstructure and mechanical properties of friction stir welded 18Cr-2Mo ferritic stainless steel thick plate10.1016/j.matdes.2014.05.070 ↗
8. The metallurgical evolution of stainless steels
9. Effect of copper and aluminium addition on mechanical properties and corrosion behaviour of AISI 430 ferritic stainless steel gas tungsten arc welds10.1016/j.jmrt.2013.02.009 ↗
10. The effect of alloy composition and welding conditions on columnar-equiaxed transitions in ferritic stainless steel gas-tungsten arc welds10.1007/BF02647249 ↗
11. Ion diffusion study in the oxide layers due to oxidation of AISI 439 ferritic stainless steel10.1007/s11085-013-9451-6 ↗
12. The effects of the minor alloying elements Al, Si and Mn on the cyclic oxidation of Ni-Cr-W-Mo alloys10.1016/j.corsci.2014.02.015 ↗
13. Development of alumina-forming duplex stainless steels as accident-tolerant fuel cladding materials for light water reactors10.1016/j.jnucmat.2018.04.027 ↗
14. Distinct oxidation behaviour attributed to phase constitution transformation at different hot processing temperatures in Fe-10Mn-5.5Al-0.25C steel10.1016/j.corsci.2019.01.045 ↗
15. Corrosion behavior of alumina-forming and oxide dispersion strengthened austenitic 316 stainless steel in supercritical water10.1016/j.corsci.2018.04.026 ↗
16. Identification by photoelectrochemistry of oxide phases grown during the initial stages of thermal oxidation of AISI 441 ferritic stainless steel in air or in water vapour10.1016/j.corsci.2008.12.002 ↗
17. Cyclic oxidation resistance of ferritic stainless steels used in mufflers of automobiles10.1016/j.engfailanal.2017.04.013 ↗
18. Oxidation behavior of ferritic stainless steels in simulated automotive exhaust gas containing 5 vol.% water vapor10.1016/j.matchemphys.2017.11.051 ↗
19. The role of (FeCrSi)2(MoNb)-type Laves phase on the formation of Mn-rich protective oxide scale on ferritic stainless steel10.1016/j.corsci.2017.12.026 ↗
20. The role of thin functional layers in solid oxide fuel cells10.1016/j.electacta.2016.04.075 ↗
21. Pre-treatment and oxidation behavior of sol-gel Co coating on 430 steel in 750 °C air with thermal cycling10.1016/j.surfcoat.2012.02.023 ↗
22. Fabrication of reactive element oxide coatings on porous ferritic stainless steel for use in metal-supported solid oxide fuel cells10.1016/j.surfcoat.2015.03.041 ↗
23. Cyclic oxidation of Mn-Co spinel coated SUS 430 alloy in the cathodic atmosphere of solid oxide fuel cells10.1016/j.jpowsour.2008.06.055 ↗
24. High temperature oxidation behavior of a high Al-containing ferritic heat-resistant stainless steel10.1016/j.matchar.2017.11.038 ↗
25. High temperature oxidation behaviour of ferritic stainless steel SUS 430 in humid air10.1007/s12540-015-4168-5 ↗
26. The single-crystal Raman spectra of nearly opaque materials. Iron (III) oxide and chromium (III) oxide10.1039/j19700000980 ↗
27. Temperature-dependent light-scattering studies of the Verwey transition and electronic disorder in magnetite10.1103/PhysRevB.9.5236 ↗
28. Composition, structure and properties of the oxide films formed on the stainless steel 316L in a primary type PWR environment10.1016/S0010-938X(97)00158-3 ↗
29. The air oxidation of an austenitic Fe-Mn-Cr stainless steel for fusion-reactor applications10.1007/BF00655899 ↗
30. Raman microspectroscopy of some iron oxides and oxyhydroxides10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO;2-B ↗
31. Raman spectra of possible corrosion products of iron10.1366/000370278774330739 ↗
32. High temperature corrosion, chapter 1
33. Effects of oxide thickness on scale and interface stresses under isothermal cooling and micro-indentation for ferritic stainless steel interconnect10.1149/1.2729017 ↗
34. Kinetics of Fe-30%Ni-12.5%Co invar alloy during high temperature oxidation10.1007/BF03186109 ↗
35. The importance of temperature in assessing iron pipe corrosion in water distribution systems10.1023/A:1016021815596 ↗
36. Product/metal ratio (PMR): a novel criterion for the evaluation of electrolytes on micro-arc oxidation (MAO) of Mg and its alloys10.1007/s11431-011-4502-1 ↗
37. The development of alumina-forming austenitic stainless steels for high-temperature structural use10.1007/s11837-008-0083-2 ↗
38. Corrosion behavior of an alumina forming austenitic steel exposed to supercritical carbon dioxide10.1016/j.corsci.2013.12.023 ↗
39. Effect of W and Ti addition on oxidation behavior and area-specific resistance of Fe-22Cr-0.5Mn ferritic stainless steel for SOFCs interconnect10.1016/j.ijhydene.2013.11.100 ↗
40. Severe dual atmosphere effect at 600 °C for stainless steel 44110.1016/j.jpowsour.2015.10.001 ↗
41. Oxidation behavior of Cu-doped MnCo2O4 spinel coating on ferritic stainless steels for solid oxide fuel cell interconnects10.1016/j.ijhydene.2016.03.051 ↗
42. Thermal degradation mechanism of ferritic alloy (Crofer 22 APU)10.1016/j.corsci.2018.01.022 ↗
43. Oxidation of ferritic stainless steel interconnects: thermodynamic and kinetic assessment10.1016/j.jpowsour.2010.09.099 ↗
44. A review of recent progress in coatings, surface modifications and alloy developments for solid oxide fuel cell ferritic stainless steel interconnects10.1016/j.jpowsour.2009.09.069 ↗
45. Effect of pre-oxidation on the oxidation resistance of Crofer 22 APU10.1016/j.corsci.2018.04.016 ↗
46. Oxidation kinetics and phase evolution of a Fe-16Cr alloy in simulated SOFC cathode atmosphere10.1016/j.jpowsour.2005.09.056 ↗
47. A fundamental study of chromium deposition on solid oxide fuel cell cathode materials10.1016/j.jpowsour.2006.02.017 ↗
48. Electrical contacts between cathodes and metallic interconnects in solid oxide fuel cells10.1016/j.jpowsour.2005.05.010 ↗
49. High temperature cyclic oxidation behavior of ferritic stainless steel with addition of alloying elements Nb and Ti for use in SOFCs interconnect10.1016/j.ijhydene.2016.01.090 ↗