Uncovering the influence of Mo and N on the hot-corrosion resistance of super austenitic stainless steels in a chloride-containing oxidizing environment
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Microstructure and chemical composition of the oxide scale formed on the Sanicro25 steel tubes after fireside corrosion10.1016/j.corsci.2015.10.030 ↗
2. Corrosion behavior of three iron-based model alloys in reducing atmospheres containing HCl and H2S at 600 °C10.1016/j.corsci.2006.06.014 ↗
3. Microstructure and oxidation behavior of C-HRA-5 austenitic heat-resistant steel in air at the temperature range of 650-750 °C10.1002/adem.202301622 ↗
4. Long term creep properties and microstructure of SUPER304H, TP347HFG and HR3C for A-USC boilers10.1179/174892408X382860 ↗
5. A sequential dual-passivation strategy for designing stainless steel used above water oxidation10.1016/j.mattod.2023.07.022 ↗
6. Alloy design employing high Cr concentrations for Mo-free stainless steels with enhanced corrosion resistance10.1016/j.corsci.2018.06.021 ↗
7. The contribution of Cr and Mo to the passivation of Ni22Cr and Ni22Cr10Mo alloys in sulfuric acid10.1016/j.corsci.2020.109015 ↗
8. On some fundamental factors in the effect of alloying elements on passivation of alloys10.1016/0010-938X(94)90013-2 ↗
9. Design for improving corrosion resistance of duplex stainless steels by wrapping inclusions with niobium armour10.1038/s41467-023-43752-8 ↗
10. Effects of alloying elements, Cr, Mo and N on re-passivation characteristics of stainless steels using the abrading electrode technique10.1016/j.matchemphys.2005.10.016 ↗
11. Oxidation behavior and high-temperature tensile properties of Fe-9Cr- (Mo, Mo/Ni) alloys10.1016/j.corsci.2021.109243 ↗
12. Effect of Mo on the high-temperature oxidation behavior of Cr-Ni-Mo hot-work die steels10.1016/j.corsci.2023.111487 ↗
13. Chloridation and oxidation of iron, chromium, nickel and their alloys in chloridizing and oxidizing atmospheres at 400-700 °C10.1016/S0010-938X(99)00142-0 ↗
14. Chloride- and sulphate-induced hot corrosion mechanism of super austenitic stainless steel S31254 under dry gas environment10.1016/j.corsci.2019.108295 ↗
15. A new insight into high-temperature oxidation mechanism of super-austenitic stainless steel S32654 in air10.1016/j.jallcom.2016.06.023 ↗
16. Catastrophic oxidation mechanism of hyper duplex stainless steel S32707 at high temperature in air10.1016/j.matchar.2018.08.041 ↗
17. Role of Mo and W during sensitization of super-austenitic stainless steel-crystallography and composition of precipitates10.1007/s11661-000-0217-9 ↗
18. Localized corrosion of a high nitrogen stainless steel N-Mo synergism
19. Nitrogen strengthening of a stable austenitic stainless steel10.1016/0001-6160(87)90131-3 ↗
20. Evaluation of high temperature corrosion in simulated waste incinerator environments10.1007/s11085-016-9615-2 ↗
21. Review on fate of chlorine during thermal processing of solid wastes10.1016/j.jes.2018.09.003 ↗
22. Corrosion of superheater materials in a waste-to-energy plant10.1016/j.fuproc.2011.06.017 ↗
23. Investigation into high-temperature corrosion in a large-scale municipal waste-to-energy plant10.1016/j.corsci.2010.07.032 ↗
24. Ash deposit characterisation in a large-scale municipal waste-to-energy incineration plant10.1016/j.jhazmat.2010.10.095 ↗
25. Precipitation behavior of sigma phase and its influence on mechanical properties of a Ni-Fe based alloy10.1016/j.jallcom.2019.01.048 ↗
26. Influence of N on precipitation behavior associated corrosion and mechanical properties of super austenitic stainless steel S3265410.1016/j.jmst.2019.10.011 ↗
27. Effects of Cr and Mo on precipitation behavior and associated intergranular corrosion susceptibility of super-austenitic stainless steel S3265410.1016/j.matchar.2019.04.010 ↗
28. Unveiling the role of cerium in enhancing the hot ductility of super austenitic stainless steel S32654 at different temperatures10.1016/j.jmst.2024.09.027 ↗
29. Molecular dynamics simulation of Cr-N clusters formation in high nitrogen austenitic stainless steel10.1016/j.scriptamat.2023.115309 ↗
30. High-temperature corrosion of austenitic alloys in HCl and H2S containing atmospheres under reducing conditions10.1016/j.corsci.2022.110214 ↗
31. Behavior of S31400 and S32205 steels in HCl- and H2S-containing gas atmospheres under a low oxygen partial pressure between 480 and 680 °C10.1002/maco.201709992 ↗
32. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
33. Effect of titanium element on high temperature chlorine corrosion properties of 904L alloy10.1016/j.corsci.2022.110915 ↗
34. Competition between thermodynamics, kinetics and growth mode in the early-stage oxidation of an equimolar CoCrFeNi alloy10.1016/j.actamat.2020.06.056 ↗
35. Nanoscale characterization of grain boundary oxidation in cold-worked stainless steels10.1016/j.corsci.2012.06.030 ↗
36. Clarifying the irradiation effect on the general oxidation of 316L stainless steel in high temperature hydrogenated water after 1000h immersion10.1016/j.actamat.2023.119100 ↗
37. Precipitation of σ-phase in high-nitrogen austenitic 18Cr-18Mn-2Mo-0.9N stainless steel during isothermal aging10.1016/j.scriptamat.2004.02.013 ↗
38. Chlorine-induced high-temperature corrosion characteristics of Ni-Cr alloy cladding layer and Ni-Cr-Mo alloy cladding layer10.1016/j.corsci.2023.111102 ↗
39. Effect of Mo on intergranular corrosion behavior in super-austenitic stainless steel10.1016/j.corsci.2024.111986 ↗
40. Unveiling the mechanism of yttrium significantly improving high-temperature oxidation resistance of super-austenitic stainless steel S3265410.1016/j.jmst.2022.01.001 ↗
41. Oxidation and hot corrosion behaviors of Mo-doped NiMoAlY alloys at 750 °C10.1016/j.corsci.2022.110262 ↗
42. Transient oxidation of Mo-Si-B alloys: effect of the microstructure size scale10.1016/j.actamat.2009.06.036 ↗
43. Formation of multilayered scale during the oxidation of NiAl-Mo alloy10.1016/j.apsusc.2014.01.148 ↗
44. Chlorine-induced high-temperature corrosion of the Pt-modified aluminide coating in simulated marine environment10.1016/j.corsci.2023.111493 ↗
45. High temperature corrosion of superalloys in an environment containing both oxygen and chlorine10.1007/BF02661276 ↗
46. The effects of chlorides, hydrogen chloride, and sulfur dioxide in the oxidation of steels below deposits10.1016/0010-938X(95)00011-8 ↗
47. Chlorine-induced high temperature corrosion of Inconel 625 sprayed coatings deposited with different thermal spray techniques10.1016/j.surfcoat.2016.12.086 ↗
48. Multi-scale computational study of high-temperature corrosion and the design of corrosion-resistant alloys10.5772/intechopen.1004978 ↗
49. High-temperature corrosion behavior of C276 alloy, 1.4529 steel and laser-cladding 1.4529 coating under the synergistic action of deposited chloride salt and HCl-containing atmosphere10.1016/j.corsci.2023.111413 ↗