Creep deformation and fracture of Ni-based alloy GH3535 in molten FLiNaK and Ar environment

Xiaoli Li, Litao Chang, Wenjun Liang, Chengpeng Liu, Zhijun Li, Yumiao Wang, Bin Leng

Corrosion Science· Volume 250
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Temperature Alloys and Creep · Metallurgical Processes and Thermodynamics · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Recommendations for a restart of molten salt reactor development10.1016/j.enconman.2007.07.047 ↗
2. A road map for the realization of global-scale thorium breeding fuel cycle by single molten-fluoride flow10.1016/j.enconman.2007.09.027 ↗
3. C.W. Forsberg, Developments in molten salt and liquid-salt-cooled reactors, in: Proceedings of the ICAPP ’06 Reno, NV USA, 2006, Paper 6292.
4. S.R. Greene, D.E. Holcomb, J.C. Gehin, SMAHTR–a concept for a small, modular advanced high temperature reactor, in: Proceedings of the HTR 2010, Prague, Czech Republic, 2010, Paper 205.
5. Hastelloy N Alloy, 2002, by Haynes International, Inc.
6. H.E. McCoy, Jr. Status of Materials Development for Molten Salt Reactors, ORNL-5920, 1978.10.2172/5195742 ↗
7. M. Wang, Q.L. Nai, J. Qiu, B.S. Wang, C. Yang, C. Su, J.P. Liang, Development of GH3535 alloy for thorium molten salt reactor, in: Proceedings of the Chinese Materials Conference 2017, ISSN 2352-2540, p137.10.1007/978-981-13-0158-2_16 ↗
8. Future advanced nuclear fission energy-TMSR nuclear energy system
9. Molten salt corrosion (FLiNaK) of a Ni-Mo-Cr alloy and its welds for application in energy-generation and energy-storage systems10.1016/j.corsci.2019.108306 ↗
10. Long-term corrosion behaviors of Hastelloy-N and Hastelloy-B3 in moisture-containing molten FLiNaK salt environments10.1016/j.jnucmat.2013.11.045 ↗
11. Effect of moisture on corrosion of Ni-based alloys in molten alkali fluoride FLiNaK salt environments10.1016/j.jnucmat.2013.02.021 ↗
12. Effect of yttrium content on the corrosion behavior of nickel-based UNS N10003 alloy in high-temperature molten LiF-NaF-KF salt10.1016/j.corsci.2021.109940 ↗
13. Corrosion in the molten fluoride and chloride salts and materials development for nuclear applications10.1016/j.pmatsci.2018.05.003 ↗
14. R.W. Swindeman, The mechanical properties of INOR-8, Oak Ridge National Laboratory, ORNL-2780, 1961.
15. S.J. Chen, D.K.L. Tsang, L. Jiang, K. Yu, C.W. Li, Microstructure and local strains in GH3535 alloy heat affected zone and their influence on the mechanical properties, vol. 699, 2017, pp. 48–54.10.1016/j.msea.2017.05.072 ↗
16. McCoy · 1967
17. J.R. Keiser, Status of Tellurium-Hastelloy N studies in molten fluoride salts, 1977. 〈http://dx.doi.org/10.2172/7295251〉.10.2172/7295251 ↗
18. The effect of He bubbles on the swelling and hardening of UNS N10003 alloy10.1016/j.jallcom.2018.02.291 ↗
19. Corrosion and Te embrittlement behaviors of Ni-Mo-Cr-Nb alloy in Te-containing molten salts10.1016/j.jnucmat.2024.155450 ↗
20. Effect of yttrium on intergranular embrittlement behavior of GH3535 alloy induced by tellurium10.1016/j.corsci.2023.111091 ↗
21. Voltammetric measurements on the [U(IV)]/[U(III)] couple and embrittlement of high nickel alloys in fuel LiF-BeF2-UF4 salt with tellurium addition in application to molten salt reactor10.1016/j.corsci.2019.108164 ↗
22. H.E. McCoy, B. McNabb, Intergranular cracking of INOR-8 in the MSRE, ORNL-4829, 1972, 165. 〈http://dx.doi.org/10.2172/4581899〉.10.2172/4581899 ↗
23. Creep crack growth of GH3535 alloy at elevated temperatures10.1016/j.matchar.2021.111412 ↗
24. Effects and mechanisms of constraint on creep crack growth behavior of GH3535 alloy10.1016/j.engfracmech.2022.109011 ↗
25. Creep resistance and material degradation of a candidate Ni–Mo–Cr corrosion resistant alloy10.1016/j.msea.2016.07.032 ↗
26. Stress-assisted corrosion behaviour of Hastelloy N in FLiNaK molten salt environment10.1038/s41529-022-00300-x ↗
27. Impact of dislocations and dislocation substructures on molten salt corrosion of alloys under plasticity-imparting conditions10.1016/j.corsci.2020.108915 ↗
28. Influence of lanthanum element on tellurium induced embrittlement of Ni-16Mo-7Cr alloy10.1016/j.corsci.2022.110360 ↗
29. Effect of yttrium on intergranular embrittlement behavior of GH3535 alloy induced by tellurium
30. Effect of yttrium content on the corrosion behavior of nickel-based UNS N10003 alloy in high-temperature molten LiF-NaF-KF salt10.1016/j.corsci.2021.109940 ↗
31. High-temperature corrosion behavior of Ni-16Mo-7Cr-4Fe superalloy containing yttrium in molten LiF–NaF–KF salt10.1016/j.jnucmat.2015.05.007 ↗
32. The critical role of Si doping in enhancing the stability of M6C carbides10.1016/j.jallcom.2017.09.042 ↗
33. M2C and M6C carbide precipitation in Ni-Mo-Cr based superalloys containing silicon10.1016/j.matdes.2016.09.075 ↗
34. Complex twin interface in M6C carbides10.1016/j.matlet.2019.05.020 ↗
35. Williams · 2006
36. Creep resistance and material degradation of a candidate Ni-Mo-Cr corrosion resistant alloy10.1016/j.msea.2016.07.032 ↗
37. Ashby · 2005
38. The effect of silicon on precipitation and decomposition behaviors of M6C carbide in a Ni-Mo-Cr superalloy10.1016/j.jallcom.2014.09.112 ↗
39. Effect of long-term thermal exposure on the hot ductility behavior of GH3535 alloy10.1016/j.msea.2016.07.034 ↗
40. Effect of long-term thermal exposure on microstructure and stress rupture properties of GH3535 superalloy10.1016/j.jmst.2014.07.021 ↗
41. J.S. Pan, et al. Fundamentals of Material Science, Tsinghua Universith Press, ISBN 978-7-302-24761-6, 2011, 012263, page 172.
42. Corrosion and creep behavior of a Ni-base alloy in supercritical-carbon dioxide environment at 650 °C10.1016/j.corsci.2020.108843 ↗
43. An investigation of oxidation/hot corrosion-creep interaction at 800 °C in a Ni-base superally coated with salt mixture deposits of Na2SO4-NaCl-NaVO310.1016/j.corsci.2018.11.029 ↗
44. Long-term corrosion behaviors of Hastelloy-N and Hastelloy-B3 in moisture-containing molten FLiNaK salt environments10.1016/j.jnucmat.2013.11.045 ↗
45. Effect of Te on the corrosion behavior of GH3535 alloy in molten LiF-NaF-KF salt10.1016/j.corsci.2023.111761 ↗
46. High-temperature corrosion behavior of Ni-16Mo-7Cr-4Fe superalloy containing yttrium in molten LiF–NaF–KF salt10.1016/j.jnucmat.2015.05.007 ↗
47. Corrosion mechanisms in molten salt thermal energy storage for concentrating solar power10.1016/j.rser.2019.109328 ↗
48. Corrosion behavior of GH3535 alloy in molten LiF-BeF2 salt10.1016/j.corsci.2022.110168 ↗